Response of ferrite, bainite, martensite, and retained austenite to a fire cycle in a fire-resistant steel

被引:15
|
作者
Escobar, J. D. [1 ]
Delfino, P. M. [1 ]
Ariza-Echeverri, E. A. [1 ,2 ]
Carvalho, F. M. [3 ]
Schell, N. [4 ]
Stark, A. [4 ]
Rodrigues, T. A. [5 ]
Oliveira, J. P. [5 ]
Avila, J. A. [6 ]
Goldenstein, H. [1 ]
Tschiptschin, A. P. [1 ]
机构
[1] Univ Sao Paulo, Met & Mat Engn Dept, Av Prof Mello Moraes 2463, Sao Paulo, Brazil
[2] Univ Tecnolag Pereira, Escuela Tecnol Mecan, Carrera 27 10-02 Alamos, Pereira, Colombia
[3] Inst Technol Res, Met Proc Lab, Av Prof Almeida Prado 532, Sao Paulo, Brazil
[4] Helmholtz Zentrum Hereon, Inst Mat Phys, Max Planck Str 1, D-21502 Geesthacht, Germany
[5] Univ NOVA Lisboa, NOVA Sch Sci & Technol, Dept Mech & Ind Engn, UNIDEMI, P-2829516 Caparica, Portugal
[6] Sao Paulo State Univ, UNESP, Campus Sao Joao da Boa Vista, Sao Joao Da Boa Vista, SP, Brazil
基金
巴西圣保罗研究基金会; 欧盟地平线“2020”;
关键词
Synchrotron X-ray diffraction; Fire-resistant steel; Secondary cementite; Retained austenite; MECHANICAL-PROPERTIES; CARBON-STEEL; BEHAVIOR; MICROSTRUCTURE; PRECIPITATION; STRENGTH; DECOMPOSITION;
D O I
10.1016/j.matchar.2021.111567
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Understanding the kinetics of microstructural degradation during the event of a fire is of major relevance to future optimization of fire-resistant steels (FRS). In this work, we use in situ synchrotron X-ray diffraction to assess the rapid thermally-assisted degradation of different starting microstructures, such as (i) ferrite + pearlite; (ii) bainite + retained austenite, and (iii) martensite + retained austenite, during the simulation of a fire cycle in a Fe-0.13C-0.11Cr-0.38Mo-0.04V FRS. Our results show that retained austenite is the most unstable phase, especially when generated by faster cooling rates, decomposing at temperatures as low as 180 degrees C during fire simulations. Bainite and martensite are both unstable and undergo recovery and carbon desaturation via secondary precipitation of cementite. However, bainite is comparatively more stable than martensite since its decomposition starts at 400 degrees C, while for martensite it occurs at 320 degrees C. We also present a methodology to deconvolute the effect of temperature on the increased background and signal intensities of the X-ray spectra, allowing the direct observation of the kinetics of secondary cementite precipitation.
引用
收藏
页数:13
相关论文
共 50 条
  • [41] Performance-based fire-resistant design of steel structure
    Li, Guoqiang
    Gongcheng Lixue/Engineering Mechanics, 2004, 21 (SUPPL.): : 105 - 115
  • [42] HIGH-TEMPERATURE PROPERTIES OF FIRE-RESISTANT STEEL FOR BUILDINGS
    SAKUMOTO, Y
    YAMAGUCHI, T
    OHASHI, M
    SAITO, H
    JOURNAL OF STRUCTURAL ENGINEERING-ASCE, 1992, 118 (02): : 392 - 407
  • [43] Technology for the commercial production of fire-resistant steel for building structures
    A. N. Muratov
    Yu. D. Morozov
    O. N. Chevskaya
    G. A. Filippov
    Metallurgist, 2007, 51 : 446 - 453
  • [44] Effects of heating temperature on microstructure and precipitate of a fire-resistant steel
    Wang, Ya-Nan
    He, Cheng-Xu
    Ying, Zheng-Yan
    Liu, Xuan
    Liu, Ming
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2012, 33 (12): : 94 - 99
  • [45] Effect of Mo on the microstructures and mechanical properties of fire-resistant steel
    Chen Jie
    Pan Fusheng
    Zuo Rulin
    Li Cong
    Dang Ying
    Proceedings of the First Australia-China-Japan Symposium on Iron and Steelmaking, 2006, : 304 - 308
  • [46] Technology for the commercial production of fire-resistant steel for building structures
    Muratov, A. N.
    Morozov, Yu. D.
    Chevskaya, O. N.
    Filippov, G. A.
    METALLURGIST, 2007, 51 (7-8) : 446 - 453
  • [47] Performance Studies and Application of Fire-resistant Coatings for Steel Structures
    Ou, Manli
    Cao, Weijun
    Jiang, Longmin
    Cao, Hui
    SUSTAINABLE DEVELOPMENT OF NATURAL RESOURCES, PTS 1-3, 2013, 616-618 : 1801 - 1807
  • [48] Experiments on fire-resistance performance of fire-resistant steel-concrete composite beams
    Jiang X.
    Tong G.-S.
    Zhang L.
    Zhejiang Daxue Xuebao (Gongxue Ban)/Journal of Zhejiang University (Engineering Science), 2016, 50 (08): : 1463 - 1470
  • [49] EXPERIMENTAL STUDY ON POST-FIRE MECHANICAL PROPERTIES OF HIGH STRENGTH FIRE-RESISTANT STEEL
    Lou G.-B.
    Fei C.-N.
    Wang Y.-B.
    Chen L.-H.
    Gongcheng Lixue/Engineering Mechanics, 2022, 39 (09): : 153 - 159
  • [50] Effect of Fire-Resistant Systems on Fire Hazard in Plasticized Polyvinylchloride
    Konstantinova, N., I
    Zubkova, N. S.
    FIBRE CHEMISTRY, 2020, 51 (06) : 459 - 463