Investigation of the γ′ Precipitates Dissolution in a Ni-Based Superalloy During Stress-Free Short-Term Annealing at High Homologous Temperatures

被引:10
|
作者
Rakoczy, Lukasz [1 ]
Grudzien-Rakoczy, Malgorzata [2 ]
Hanning, Fabian [3 ]
Cempura, Grzegorz [1 ]
Cygan, Rafal [4 ]
Andersson, Joel [3 ]
Zielinska-Lipiec, Anna [1 ]
机构
[1] AGH Univ Sci & Technol, Fac Met Engn & Ind Comp Sci, Mickiewicza 30, PL-30059 Krakow, Poland
[2] Lukasiewicz Res Network Krakow Inst Technol, Zakopianska 73, PL-30418 Krakow, Poland
[3] Univ West, Dept Engn Sci, Gustava Melins Gata 2, S-46132 Trollhattan, Sweden
[4] Consolidated Precision Prod Corp, Invest Casting Div, Hetman ska 120, PL-35078 Rzeszow, Poland
关键词
SINGLE-CRYSTAL SUPERALLOY; NICKEL-BASED SUPERALLOY; WELD CRACKING; MICROSTRUCTURE; MORPHOLOGY; BEHAVIOR; DIFFUSION; PHASE; DECOMPOSITION; EVOLUTION;
D O I
10.1007/s11661-021-06420-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The equiaxed Ni-based superalloy Rene 108 was subjected to short-term annealing at five temperatures between 900 degrees C and 1100 degrees C. The phase composition, phase lattice parameters, microstructure, stereological parameters, and chemical composition of gamma ' precipitates were investigated by thermodynamic simulations, X-ray diffraction, scanning and transmission electron microscopy, and energy-dispersive X-ray spectroscopy. Analysis of the gamma and gamma ' lattice parameters using the Nelson-Riley extrapolation function showed that the misfit parameter for temperatures 900 degrees C to 1050 degrees C is positive (decreasing from 0.32 to 0.11 pct). At 1100 degrees C, the parameter becomes negative, delta = - 0.18 pct. During the short-term annealing, gamma ' precipitates dissolution occurred progressing more rapidly with increasing temperatures. The surface fraction of gamma ' precipitates decreased with increasing temperature from 0.52 to 0.34. The dissolution of gamma ' precipitates did not only proceed through uninterrupted thinning of each individual precipitate, but also included more complex mechanisms, including splitting. Based on transmission electron microscopy, it was shown that after gamma ' precipitates dissolution, the matrix close to the gamma/gamma ' interface is strongly enriched in Co and Cr and depleted in Al.
引用
收藏
页码:4767 / 4784
页数:18
相关论文
共 24 条
  • [21] Effects of Cr content on the microstructure and stress rupture property of a directionally solidified Ni-based superalloy during long-term thermal exposure
    Zhang, H. W.
    Qin, X. Z.
    Wu, Y. S.
    Zhou, L. Z.
    Li, X. W.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 718 : 449 - 460
  • [22] Stress-induced influence on the evolution of γ′ phase in dendritic area during long-term stress aging at 900 °C in Ni-based superalloy K444
    Cai, Hang
    Hou, Jieshan
    Xing, Jing
    Yang, Fenqi
    Liu, Zitong
    Zhou, Lan-Zhang
    MATERIALS CHARACTERIZATION, 2024, 207
  • [23] Investigation on the influence of Ta on the microstructure evolution of Ni-based superalloy DZ411 during directional solidification, heat treatment, and long-term aging
    Peng, Peng
    Lu, Li
    Liu, Zijie
    Pei, Xing
    Gan, Lu
    Xu, Yuanli
    Zhang, Xudong
    Ma, Zhikun
    Guo, Min
    Liu, Lin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 920
  • [24] Investigation on the influence of Ta on the microstructure evolution of Ni-based superalloy DZ411 during directional solidification, heat treatment, and long-term aging
    Peng, Peng
    Lu, Li
    Liu, Zijie
    Pei, Xing
    Gan, Lu
    Xu, Yuanli
    Zhang, Xudong
    Ma, Zhikun
    Guo, Min
    Liu, Lin
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 920