摘要
Ceramic coatings were prepared on Ti-6Al-4V alloy using ac micro-arc oxidation (MAO) in silicate-hypophosphate solution. Growth regularity and formation mechanism of ceramic coatings were discussed. It was found that during the first stage the growth rate of coatings toward the external surface was larger than that toward substrate and then the coating began to grow mainly towards Ti alloy. When the total coating thickness reaches a certain value, it would no longer increase. In addition, the variations of the composition and microstructure of ceramic coatings according to the depositing time were also investigated with X-ray diffraction (XRD) and scanning electron microscope (SEM). The amount of rutile TiO2 gradually increased, whereas the amounts of the anatase TiO2 and amorphous phases first increased and then decreased slightly.
引用
收藏
页码:281 / 284
页数:4
相关论文
共 50 条
  • [41] Modification of Microstructure and Surface Properties of Ti-6Al-4V Alloy by Molybdenum Disilicide Particles Using Micro-Arc Oxidation Process
    Kadhim, Nawar Fahem
    Haleem, Ali Hubi
    Awad, Samir Hamid
    ADVANCES IN SCIENCE AND TECHNOLOGY-RESEARCH JOURNAL, 2024, 18 (02) : 374 - 384
  • [42] Novel artificial hip joint: A layer of alumina on Ti-6Al-4V alloy formed by Micro-arc oxidation
    Khanna, Rohit
    Kokubo, Tadashi
    Matsushita, Tomiharu
    Nomura, Yuuji
    Nose, Norihiro
    Oomori, Yoshiyuki
    Yoshida, Takuya
    Wakita, Koichi
    Takadama, Hiroaki
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2015, 55 : 393 - 400
  • [43] Preparation of bioceramic films containing hydroxyapatites on Ti-6Al-4V alloy surfaces by the micro-arc oxidation technique
    Yang, Xizhen
    Yu, Sirong
    Li, Wen
    MATERIALS RESEARCH BULLETIN, 2009, 44 (04) : 947 - 949
  • [44] Effect of Ag concentration on structure and wear behaviour of coatings formed by micro-arc oxidation on Ti6Al4 V Alloy
    Demirbas, Cagatay
    Ayday, Aysun
    SURFACE ENGINEERING, 2021, 37 (01) : 24 - 31
  • [45] Effect of auxiliary laser irradiation on characteristics and properties of micro-arc oxidation coating on Ti6Al4V alloy
    Wang, Ye
    Peng, Qiandi
    Wu, Guolong
    Yao, Jianhua
    Yin, Yanyi
    Li, Lin
    Zheng, Yafeng
    Wen, Chen
    CERAMICS INTERNATIONAL, 2024, 50 (11) : 19412 - 19423
  • [46] The effect of Micro-arc Oxidation treatment on the microstructure and properties of open cell Ti6Al4V alloy foams
    Korkmaz, Kemal
    SURFACE & COATINGS TECHNOLOGY, 2015, 272 : 72 - 78
  • [47] Structure and mechanical properties of ceramic coatings fabricated by micro-arc oxidation
    Li, H. X.
    Song, R. G.
    Zhao, J.
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES, PTS 1 AND 2, 2008, 47-50 : 554 - 557
  • [48] Preperation of Ceramic Coatings on Ti Alloy by Surface Nanocrystallization/Micro-arc Oxidation
    Zhang, Jinxue
    Hao, Guodong
    ADVANCES IN SUPERALLOYS, PTS 1 AND 2, 2011, 146-147 : 1821 - 1824
  • [49] Compound Ceramic Coatings on Ti-6Al-4V by Micro-Plasma Oxidation in NaAlO2 Solution
    YAO Zheng-ping
    材料热处理学报, 2004, (05) : 1060 - 1063
  • [50] Compound ceramic coatings on Ti-6Al-4V by micro-plasma oxidation in NaAlO2 solution
    Yao, ZP
    Jiang, ZH
    Xin, SG
    Sun, XT
    Wu, ZD
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 1060 - 1063