Laser-assisted micro-milling of austenitic stainless steel X5CrNi18-10

被引:12
|
作者
Kadivar, Mohammadali [1 ]
Azrhoushang, Bahman [1 ]
Zahedi, Ali [1 ]
Mueller, Claas [2 ]
机构
[1] Furtwangen Univ Appl Sci, Inst Precis Machining KSF, Jakob Kienzle Str 17, D-78056 Villingen Schwenningen, Germany
[2] Univ Freiburg, Lab Proc Technol, Dept Microsyst Engn, IMTEK, Georges Kohler Allee 103, D-79110 Freiburg, Germany
关键词
Laser-assisted micro-milling; Micro-milling; Laser structuring; Ultra-short pulsed laser; Austenitic stainless steel; SILICON-NITRIDE; TOOL WEAR; MACHINING PERFORMANCE; BURR FORMATION; FRICTION; FLOW; CBN;
D O I
10.1016/j.jmapro.2019.11.002
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper presents a novel Laser-Assisted Micro-Milling (LAMM) process of austenitic stainless steel X5CrNi18-10. The LAMM process is compared with the conventional micro-milling process. Ultra-short pulsed laser radiation is utilized for the structuring of the workpiece surface prior to the micro-milling process. Different laser structures are produced on the workpiece surface at a constant laser scanning speed with various laser powers and laser line spans. The high performance of the developed process is shown by experimental investigations. The effect of laser structuring on the micro-milling forces and temperature indicated the superior performance of the new LAMM process. Cutting forces and temperature could be reduced by up to 70% and 50%, respectively. The results of conventional micro-milling showed that increasing the cutting speed, at a constant undeformed chip thickness, reduced the micro-milling forces. Increasing the cutting speed from 50 to 250 m/min halved both the trust and normal forces, while it slightly improved the surface roughness. On the other hand, increasing the feed per tooth degraded the surface roughness and increased the cutting forces. Furthermore, in conventional milling the workpiece was subjected to high plastic deformation during the cutting process, while side flow, smeared material, metal debris, and cavities were observed on the workpiece surface.
引用
收藏
页码:174 / 184
页数:11
相关论文
共 50 条
  • [41] THE MICROSTRUCTURE OF METASTABLE AUSTENITE IN X5CrNi18-10 STEEL AFTER ITS STRAIN-INDUCED MARTENSITIC TRANSFORMATION
    Kurc-Lisiecka, Agnieszka
    Ozgowicz, Wojciech
    Kalinowska-Ozgowicz, Elzbieta
    Maziarz, Wojciech
    MATERIALI IN TEHNOLOGIJE, 2016, 50 (06): : 837 - 843
  • [42] Methodology of Increasing Safety of Welding Joints in Pressure Vessels X5CrNi18-10
    Vacková M.
    Va¾ko M.
    Pavlenko S.
    Ha¾ko J.
    Ha½ko, Jozef (jozef.halko@tuke.sk), 2017, Jan-Evangelista-Purkyne-University (17): : 61
  • [43] THERMOGRAPHIC METHOD BASED ACCELERATED FATIGUE LIMIT CALCULATION FOR STEEL X5CRNI18-10 SUBJECTED TO ROTATING BENDING
    Lipski, Adam
    POLISH MARITIME RESEARCH, 2015, 22 (04) : 64 - 69
  • [44] Pulsed Laser Processing of Dissimilar Ti-6Al-4V and X5CrNi18-10 Joints
    Mitelea, Ion
    Groza, Cosmin
    Craciunescu, Corneliu Marius
    MATERIALS AND MANUFACTURING PROCESSES, 2014, 29 (08) : 975 - 979
  • [45] Micro-milling of 65 vol% SiCp/Al composites with a novel laser-assisted hybrid process
    Zhao, Guolong
    Mao, Pengcheng
    Li, Liang
    Iqbal, Asif
    He, Ning
    CERAMICS INTERNATIONAL, 2020, 46 (16) : 26121 - 26128
  • [46] Thermal and mechanical modeling analysis of laser-assisted micro-milling of difficult-to-machine alloys
    Ding, Hongtao
    Shen, Ninggang
    Shin, Yung C.
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2012, 212 (03) : 601 - 613
  • [47] MELTED ZONE MORPHOLOGY BY LASER WELDING OF TI-6AL-4V WITH X5CRNI18-10
    Groza, Cosmin
    Mitelea, Ion
    Utu, Ion-Dragos
    Craciunescu, Corneliu Marius
    21ST INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS (METAL 2012), 2012, : 690 - 696
  • [48] Investigations on remote laser beam welding of dissimilar joints of austenitic chromium-nickel steel (X5CrNi18-10) and aluminum alloy (AA6082-T6) for battery housings
    Seffer, Oliver
    Springer, Andre
    Kaierle, Stefan
    JOURNAL OF LASER APPLICATIONS, 2018, 30 (03)
  • [49] X5CrNi18-10奥氏体不锈钢焊接工艺研究
    粟世富
    惠铭钰
    化工管理, 2020, (08) : 194 - 195
  • [50] Modeling and optimization in dry face milling of X2CrNi18-9 austenitic stainless steel using RMS and desirability approach
    Selaimia, Abdel-Ali
    Yallese, Mohamed Athmane
    Bensouilah, Hamza
    Meddour, IKhlas
    Khattabi, Riad
    Mabrouki, Tarek
    MEASUREMENT, 2017, 107 : 53 - 67