Correlating the microstructure of the die-chill skin and the corrosion properties for a hot-chamber die-cast AZ91D magnesium alloy

被引:29
|
作者
Yu, BL [1 ]
Uan, JY [1 ]
机构
[1] Natl Chung Hsing Univ, Dept Mat Engn, Taichung 402, Taiwan
关键词
D O I
10.1007/s11661-005-0343-5
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The corrosion of a hot-chamber die-cast AZ91D thin plate (1.4 mm in thickness) was investigated in terms of its microstructure, to elucidate the role of die-chill skin in corrosion. The die-chill skin was composed of a thin layer of chill zone and a thick layer of an interdendritic Al-rich alpha-Mg/Al12Mg17 beta-phase particle/alpha-Mg grain composite microstructures. The chill zone (4 +/- 1 mu m in thickness) had fine columnar and equiaxed grains and contained a distribution of submicron Mg-Al-Zn intermetallic particles. Beneath the chill zone, Al12Mg17 beta particles were irregularly shaped but did not have an interdendritic network morphology. Furthermore, Al-rich alpha phase (also known as eutectic alpha) was in the interdendritic network, which occupied a higher volume fraction than the beta phase in the die-skin layer. Corrosion characteristics were studied via constant-immersion and electrochemical tests. Although previous studies have ascribed the fine microstructure to good corrosion resistance for the AZ91D alloy, the present study showed severe corrosion of the sample with a die skin in chloride solution. Moreover, the sample without the die skin on the surface corroded more slowly. The inferior corrosion performance of the die skin was considered to be related to the high volume fraction of the interdendritic network of Al-rich alpha phase contained in the die skin, owing to the high cooling rate during solidification. The Al-rich alpha phase does not increase the corrosion resistance of the AZ91D alloy.
引用
收藏
页码:2245 / 2252
页数:8
相关论文
共 50 条
  • [21] Barium phosphate conversion coating on die-cast AZ91D magnesium alloy
    刘锋
    单大勇
    韩恩厚
    刘常升
    Transactions of Nonferrous Metals Society of China, 2008, 18(S1) (S1) : 344 - 348
  • [22] Fatigue crack growth behaviour of a die-cast magnesium alloy AZ91D
    Venkateswaran, P
    Raman, SGS
    Pathak, SD
    Miyashita, Y
    Mutoh, Y
    MATERIALS LETTERS, 2004, 58 (20) : 2525 - 2529
  • [23] Effects of combined addition of Ca and Y on the corrosion behaviours of die-cast AZ91D magnesium alloy
    Woo, Sang Kyu
    Blawert, Carsten
    Yasakau, K. A.
    Yi, Sangbong
    Scharnagl, Nico
    Suh, Byeong-Chan
    Kim, Young Min
    You, Bong Sun
    Yim, Chang Dong
    CORROSION SCIENCE, 2020, 166
  • [24] Effect of cyclic loading on mechanical properties and microstructure of die cast magnesium alloy AZ91D
    Li, Jiquan
    Chen, Long
    Wang, Fenghua
    Jiang, Shaofei
    Gan, Huiqi
    Zhou, Jun
    Hao, Weina
    MATERIALS TESTING, 2023, 65 (02) : 153 - 161
  • [25] Microstructural refinement of AZ91D die-cast alloy by intensive shearing
    Tzamtzis, S.
    Zhang, H.
    Babu, N. Hari
    Fan, Z.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (12): : 2929 - 2934
  • [26] High cycle fatigue properties of AZ91D die cast magnesium alloy
    Yang, You
    Liu, Yongbing
    Yang, Xiaohong
    Tezhong Zhuzao Ji Youse Hejin/Special Casting and Nonferrous Alloys, 2006, 26 (02): : 105 - 107
  • [28] Galvanic corrosion behavior of die cast AZ91D magnesium alloy in chloride solution
    Tong, ZS
    Zhang, W
    Li, JQ
    Gao, J
    He, JQ
    Zhou, J
    JOURNAL OF UNIVERSITY OF SCIENCE AND TECHNOLOGY BEIJING, 2004, 11 (02): : 127 - 132
  • [29] Structure and formation mechanism of phosphate conversion coating on die-cast AZ91D magnesium alloy
    Zhou, Wanqiu
    Shan, Dayong
    Han, En-Hou
    Ke, Wei
    CORROSION SCIENCE, 2008, 50 (02) : 329 - 337
  • [30] Microstructural Evolution of Vacuum Die-Cast AZ91D Magnesium Alloy during Solution Treatment
    Wang, Qingliang
    Han, Yi
    Xiong, Shoumei
    MATERIALS TRANSACTIONS, 2019, 60 (10) : 2125 - 2131