摘要
The corrosion process of the alloy AA5083 in an aerated solution of NaCl at 3.5% has been studied. The results obtained indicate that the main process that this alloy undergoes, under the conditions of exposure studied, is related to localized corrosion that takes place as a consequence of the process of alkalinization around the cathodic precipitates existing in the alloy. The pitting formed presents a hemispherical morphology that is clearly different from crystallographic pitting. The formation of crystallographic pitting has not been observed, even in samples submitted to tests of very long duration. In order to obtain the formation of crystallographic pitting, it is necessary to polarize the alloy at the nucleation potential of pitting and. in addition, the density of the current must be above a critical value. Only when the layer of oxide is eliminated does the formation of crystallographic pitting take place by simple exposure in an aerated solution of NaCl at 3.5%. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1657 / 1674
页数:18
相关论文
共 50 条
  • [2] The research of electrochemical behavior of alloy AA5083 in 3.5% NaCl solution
    Chen, Shan
    Li, Guoming
    Chang, Wanshun
    Chen, Xuequn
    ADVANCED RESEARCH ON MATERIAL ENGINEERING AND ELECTRICAL ENGINEERING, 2013, 676 : 80 - 84
  • [3] Role of intermetallic phases in localized corrosion of AA5083
    Yasakau, Kiryl A.
    Zheludkevich, Mikhail L.
    Lamaka, Sviatlana V.
    Ferreira, Mario G. S.
    ELECTROCHIMICA ACTA, 2007, 52 (27) : 7651 - 7659
  • [4] Study of the localized corrosion resistance of AA5083 aluminium alloy subjected to severe plastic deformation
    Vicere, A.
    Cabibbo, M.
    Forcellese, P.
    Giuliani, G.
    Bellezze, T.
    METALLURGIA ITALIANA, 2022, 114 (02): : 28 - 33
  • [5] Localized corrosion of a 2219 aluminium alloy exposed to a 3.5% NaCl solution
    Grilli, Rossana
    Baker, Mark A.
    Castle, James E.
    Dunn, Barrie
    Watts, John F.
    CORROSION SCIENCE, 2010, 52 (09) : 2855 - 2866
  • [6] Effect of Fluid parameters on Erosion-corrosion behavior of Al-2%Zn coatings on AA5083 Aluminium Alloy in 3.5% NaCl
    Xia, Yanming
    Zhou, Dejing
    Gao, Zhiming
    Hu, Wenbin
    INTERNATIONAL JOURNAL OF ELECTROCHEMICAL SCIENCE, 2022, 17 (04):
  • [7] Effect of Hg2+ on the corrosion behavior of Al-2%Zn coatings on AA5083 in 3.5 Wt.% NaCl solution
    Xia, Yanming
    Zhou, Dejing
    Gao, Zhiming
    Hu, Wenbin
    ANTI-CORROSION METHODS AND MATERIALS, 2022, 69 (03) : 261 - 268
  • [8] The Positive impact of biomineralization for marine corrosion protection of AA5083 alloy
    Marques, M. J. F.
    Jaume, J.
    Mercier, D.
    Seyeux, A.
    Zanna, S.
    Basseguy, R.
    Marcus, P.
    CORROSION SCIENCE, 2024, 233
  • [9] Corrosion study on AA5083 aluminum alloy - boron carbide composite
    Vasudevan, N.
    Bhaskar, G. B.
    Prasad, Rajendra A.
    Suresh, S. M.
    MATERIALS TODAY-PROCEEDINGS, 2019, 16 : 1124 - 1129
  • [10] Using EIS to study the electrochemical response of alloy AA5083 in solutions of NaCl
    Aballe, A
    Bethencourt, M
    Botana, FJ
    Marcos, M
    Osuna, R
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2001, 52 (03): : 185 - 192