Role of intermetallic phases in localized corrosion of AA5083

被引:303
|
作者
Yasakau, Kiryl A.
Zheludkevich, Mikhail L. [1 ]
Lamaka, Sviatlana V.
Ferreira, Mario G. S.
机构
[1] Univ Aveiro, CICECO, Dept Ceram & Glass Engn, P-3810 Aveiro, Portugal
[2] Inst Super Tecn, ICEMS, Dept Chem Engn, P-1049 Lisbon, Portugal
关键词
AA5083; corrosion; pitting; scanning Kelvin probe force microscopy; intermetallic phases;
D O I
10.1016/j.electacta.2006.12.072
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The presence of intermetallic inclusions very often plays a crucial role for the susceptibility of different aluminium alloys to localized corrosion attack. The intimate details of localized corrosion of 5083 aluminium alloy have been studied in the present work. Local techniques such as scanning Kelvin probe force microscopy, in situ atomic force microscopy, scanning electron microscopy coupled with energy dispersive spectroscopy were used to investigate the mechanisms and the kinetics of localized corrosion attack. The importance of iron-rich and Mg2Si intermetallic phases in the initiation of corrosion processes is demonstrated in the paper. The Mg2Si phase has a potential lower relatively to the matrix. Moreover, the high reactivity of magnesium leads to the dissolution and consequently to the fast dealloying of these intermetallics. However, hydroxide (Mg(OH)(2) and SiO2 center dot nH(2)O) deposits formed during corrosion act as an additional diffusion barrier hindering the deep propagation of pits. The iron containing intermetallics have the potential higher with respect to the aluminum matrix playing the role of effective cathodic centers for oxygen reduction causing anodic polarization and pitting in the surrounding alloy matrix. Dealloying of such intermetallics with subsequent iron enrichment was also revealed. Pitting initiation seems to be statistical and independent of the composition of Fe-rich intermetallics. However, the active growth of the pits prevents initiation of localized corrosion attack in nearby sites. A new pit can start to grow only when a neighbor one becomes passivated. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:7651 / 7659
页数:9
相关论文
共 50 条
  • [1] Localized alkaline corrosion of alloy AA5083 in neutral 3.5% NaCl solution
    Aballe, A
    Bethencourt, M
    Botana, FJ
    Cano, MJ
    Marcos, M
    CORROSION SCIENCE, 2001, 43 (09) : 1657 - 1674
  • [2] Effect of thermomechanical treatment on the corrosion of AA5083
    Tan, L.
    Allen, T. R.
    CORROSION SCIENCE, 2010, 52 (02) : 548 - 554
  • [3] Corrosion Inhibition of Sensitized and Solutionized AA5083
    Seong, Jinwook
    Frankel, G. S.
    Sridhar, N.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (09) : C449 - C456
  • [4] Influence of the Altered Surface Layer on the Corrosion of AA5083
    Seong, Jinwook
    Yang, Fan
    Scheltens, Frank
    Frankel, G. S.
    Sridhar, N.
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2015, 162 (06) : C209 - C218
  • [5] Inhibition of Stress Corrosion Cracking of Sensitized AA5083
    Seong, Jinwook
    Frankel, G. S.
    Sridhar, N.
    CORROSION, 2016, 72 (02) : 284 - 296
  • [6] Study of the localized corrosion resistance of AA5083 aluminium alloy subjected to severe plastic deformation
    Vicere, A.
    Cabibbo, M.
    Forcellese, P.
    Giuliani, G.
    Bellezze, T.
    METALLURGIA ITALIANA, 2022, 114 (02): : 28 - 33
  • [7] On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface-Part 1: Corrosion initiation mechanism
    Xia, Da-Hai
    Ji, Yuanyuan
    Zhang, Ruifeng
    Mao, Yingchang
    Behnamian, Yashar
    Hu, Wenbin
    Birbilis, Nick
    CORROSION SCIENCE, 2023, 213
  • [8] Enhancement of the Stress Corrosion Sensitivity of AA5083 by Heat Treatment
    Gao, Jie
    Quesnel, David J.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (02): : 356 - 364
  • [9] Enhancement of the Stress Corrosion Sensitivity of AA5083 by Heat Treatment
    Jie Gao
    David J. Quesnel
    Metallurgical and Materials Transactions A, 2011, 42 : 356 - 364
  • [10] The effect of temperature on corrosion behavior of AA5083 in brackish water and seawater
    Lokas, Lea
    Alar, Vesna
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2019, 70 (10): : 1817 - 1825