Effect of common water contaminants on the corrosion of aluminium alloys in ethylene glycol-water solution

被引:67
|
作者
Abiola, Olusegun K. [1 ]
Otaigbe, J. O. E. [2 ]
机构
[1] Univ Lagos, Dept Chem, Lagos, Nigeria
[2] Univ Port Harcourt, Dept Pure & Ind Chem, Port Harcourt, Nigeria
关键词
aluminium; corrosion; kinetics;
D O I
10.1016/j.corsci.2007.06.013
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of common water contaminants of chloride (Cl-), cupric (Cu2+) and ferric (Fe3+) ions, in four different mixture combination of Fe3++Cu2+, Cl-+Fe3+, Cl- + Cu2+ and Cl- + Fe3+ + Cu2+, were examined on the corrosion behaviour of aluminium alloys in ethylene glycol-water solution, using mass loss technique. The highest material losses were recorded for the two alloys in ethylene glycol solution containing the combination of the chloride and the two heavy metal ions. The corrosivity of the solution in the presence of the combination of ions was in the order of Cl- + Fe3+ + Cu2+ > Cl- + Cu2+ > Cl- + Fe3+ > Fe3+ + Cu2+. The results gave first-order kinetics with respect to aluminium in ethylene glycol solution-ion systems. Alloy 3SR exhibits maximum corrosion in all the solutions. It is concluded that the two commercial alloys in the solution polluted with all the three ions would not be able to survive for reasonable period of time without corrosion inhibitor. (c) 2007 Elsevier Ltd. All rights reserved.
引用
收藏
页码:242 / 247
页数:6