Enhancement of the Coercive Force of Sm2Fe17N3 Powders via Surfactant Added Mechanical Milling

被引:2
|
作者
Kolodkin, D. A. [1 ]
Popov, A. G. [1 ,2 ]
Gaviko, V. S. [1 ,2 ]
机构
[1] Russian Acad Sci, Mikheev Inst Met Phys, Ural Branch, Ekaterinburg 620108, Russia
[2] Yeltsin Ural Fed Univ, Inst Nat Sci & Math, Ekaterinburg 620002, Russia
来源
PHYSICS OF METALS AND METALLOGRAPHY | 2021年 / 122卷 / 06期
关键词
Sm2Fe17N3; powder; mechanical milling; surfactant; hysteresis properties; N BULK MAGNETS; FINE POWDER; MICROSTRUCTURE; REDUCTION; DEFORMATION; IMPROVEMENT; PARTICLES;
D O I
10.1134/S0031918X21060053
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The effect of the mechanical milling of Sm2Fe17N3 nitride in a vibratory mill, in particular, the effect of the powder-to-ball mass ratio (m), milling time (t(mill)), milling medium, and concentration of added surfactants, has been systematically studied in order to determine optimum parameters for the high level of hysteresis properties of the magnetically anisotropic powder. It is shown that, as m increases from 15 to 50, the increase in the coercivity H-c of the powder at the beginning milling stages (t(mill) <= 4 h) is substantially accelerated; in this case, about 80% particles are less than 1 mu m in size. As the milling time increases (t(mill) > 4 h), the coercivity continues to increase. However, the specific residual magnetization sigma(r) and maximum energy product (BH)(max) begin to decrease because of the developed process of particle agglomeration, which results in a deterioration of the powder allignment. The addition of a surfactant to the protective medium markedly intensifies the milling process and accelerates the kinetics of the increase of H-c at the beginning milling stages at m = 15. The best complex of magnetic hysteresis properties, sigma(r) >= 135 emu/g, H-c, >= 8 kOe, and (BH)(max) >= 18 MG Oe, is observed for powders milled in 5% solution of oleic acid in acetone, 5% solution of capronic acid in toluene, and 1% solution of methyl caproate in toluene.
引用
收藏
页码:547 / 558
页数:12
相关论文
共 50 条
  • [21] Magnetization reversal in Sm2Fe17N3 particles
    Cent Natl de la Recherche, Scientifique, Grenoble, France
    J Magn Magn Mater, (97-98):
  • [22] Magnetisation reversal in Sm2Fe17N3 particles
    Kobayashi, K
    Givord, D
    Coey, JMD
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1996, 157 : 97 - 98
  • [23] A20 DETERMINATION FOR SM2FE17N3
    LI, HS
    COEY, JMD
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1992, 115 (2-3) : 152 - 154
  • [24] Exchange coupling between soft magnetic ferrite and hard ferromagnetic Sm2Fe17N3 in ferrite/Sm2Fe17N3 composites
    Imaoka, N.
    Kakimoto, E.
    Takagi, K.
    Ozaki, K.
    Tada, M.
    Nakagawa, T.
    Abe, M.
    AIP ADVANCES, 2016, 6 (05):
  • [25] Production of Sm2Fe17N3 Bulk Magnets
    Saito, Tetsuji
    INORGANICS, 2024, 12 (04)
  • [26] Electrochemical Passivation for Sm2Fe17N3 Magnetic Powders in Non-Aqueous Solvents
    Kadowaki, Mariko
    Muto, Izumi
    Sugawara, Yu
    Ishikawa, Takashi
    Yoneyama, Yukinobu
    Hara, Nobuyoshi
    ELECTROCHIMICA ACTA, 2017, 224 : 386 - 396
  • [27] Improvement of the magnetic properties of HDDR Sm2Fe17N3
    IFW Dresden e.V., Dresden, Germany
    J Magn Magn Mater, (99-100):
  • [28] Improvement of the magnetic properties of HDDR Sm2Fe17N3
    Dempsey, NM
    Wendhausen, PAP
    Gebel, B
    Muller, KH
    Coey, JMD
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 1996, 157 : 99 - 100
  • [29] HIP sintering and magnetic properties of Sm2Fe17N3
    Ito, Shigeru
    Igarashi, Jun
    Fujii, Takashi
    Funtai Oyobi Fummatsu Yakin/Journal of the Japan Society of Powder and Powder Metallurgy, 2000, 47 (07): : 801 - 806
  • [30] Sm2Fe17N3各向异性磁体
    光明
    金属功能材料, 1997, (04) : 35 - 36