Study of interfacial adhesion energy of multilayered ULSI thin film structures using four-point bending test

被引:31
|
作者
Gan, ZH [1 ]
Mhaisalkar, SG
Chen, Z
Zhang, S
Chen, Z
Prasad, K
机构
[1] Nanyang Technol Univ, Sch Mat Engn, Singapore 639798, Singapore
[2] Nanyang Technol Univ, Sch Mech & Prod Engn, Singapore 639798, Singapore
[3] Nanyang Technol Univ, Sch Elect & Elect Engn, Singapore 639798, Singapore
来源
SURFACE & COATINGS TECHNOLOGY | 2005年 / 198卷 / 1-3期
关键词
four-point bending; photoelectron microscopy; silicon carbide; polyarylene ether (PAE);
D O I
10.1016/j.surfcoat.2004.10.036
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Adhesion between barrier layers and interconnect metals or dielectrics continues to be a significant concern in the microelectronic industry, with delamination occurring in between the layers leading to device failure. As the sizes of transistors are scaled down to submicron regime, new materials and multilayered thin film structures are applied, which pose a great challenge to quantify the adhesion energy of the interfaces in order to optimize the structures of the multilayered thin films. In this paper, the four-point bending technique is used to quantify the adhesion energy (G(c)) between interfaces in multilayered thin film structures for ULSI. An example is presented to demonstrate the applicability of the four-point bending technique for determining the adhesion strength of the SiC/porous polyarylene ether (PAE)/SiC interface. The G(c) value obtained is 26.2 J/m(2), higher than that of the SiN/PAE interface reported by others, indicating a good adhesion. The resulting fracture surfaces were then characterized by field emission scanning electron microscopy (FESEM) and X-ray photoelectron spectroscopy (XPS) to identify the location of the debonded path. It is found that the crack propagates alternatively between the two PAE/SiC interfaces. (c) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:85 / 89
页数:5
相关论文
共 50 条
  • [21] Modified four-point bending specimen for determining the interface fracture energy for thin, brittle layers
    Hofinger, Ines
    Oechsner, Matthias
    Bahr, Hans-Achim
    Swatn, Michael V.
    International Journal of Fracture, 1999, 92 (03): : 213 - 220
  • [22] Modeling the Ligament Breakage Mechanism in Concrete Specimens Using a Four-Point Bending Test
    Fu, J. W.
    Haeri, H.
    Sarfarazi, V
    Marji, M. F.
    STRENGTH OF MATERIALS, 2022, 54 (04) : 671 - 680
  • [23] Modified four-point bending specimen for determining the interface fracture energy for thin, brittle layers
    Hofinger, I
    Oechsner, M
    Bahr, HA
    Swain, MV
    INTERNATIONAL JOURNAL OF FRACTURE, 1998, 92 (03) : 213 - 220
  • [24] Modeling the Ligament Breakage Mechanism in Concrete Specimens Using a Four-Point Bending Test
    J. W. Fu
    H. Haeri
    V. Sarfarazi
    M. F. Marji
    Strength of Materials, 2022, 54 : 671 - 680
  • [25] Modified four-point bending specimen for determining the interface fracture energy for thin, brittle layers
    Ines Hofinger
    Matthias Oechsner
    Hans-Achim Bahr
    Michael V. Swain
    International Journal of Fracture, 1998, 92 : 213 - 220
  • [26] Adhesion evaluation of thin films to dielectrics in multilayer stacks: A comparison of four-point bending and stressed overlayer technique
    Lassnig, A.
    Putz, B.
    Hirn, S.
    Toebbens, D. M.
    Mitterer, C.
    Cordill, M. J.
    MATERIALS & DESIGN, 2021, 200
  • [27] Measurement and characterization of interfacial strain energy release rate of Si3N4/BN composites by four-point bending test
    Zou, Linhua
    Huang, Yong
    Wang, Chang'an
    Kuei Suan Jen Hsueh Pao/ Journal of the Chinese Ceramic Society, 2002, 30 (02): : 178 - 183
  • [28] Fatigue-healing performance evaluation of asphalt mixture using four-point bending test
    Xiang, Hao
    Zhang, Wenwu
    Liu, Peng
    He, Zhaoyi
    MATERIALS AND STRUCTURES, 2020, 53 (03)
  • [29] Experimental determination of thin film adhesion using 4 point bending specimen
    Kim, JH
    Lee, SB
    Earmme, YY
    ADVANCES IN ELECTRONIC MATERIALS AND PACKAGING 2001, 2001, : 376 - 381
  • [30] Loading Conditions Effects on Fatigue Life of Notched Rods Using Four-Point Bending Test
    Chouikhi, H.
    Mahdi, M.
    Saber, M.
    EXPERIMENTAL TECHNIQUES, 2024, 48 (06) : 1039 - 1052