TG/MS/FTIR study on thermal degradation process of clay mineral-polysiloxane nanocomposites

被引:11
|
作者
Wojcik-Bania, Monika [1 ]
机构
[1] AGH Univ Sci & Technol, Fac Geol Geophys & Environm Protect, Al Mickiewicza 30, PL-30059 Krakow, Poland
关键词
Polymer clay nanocomposites; Polysiloxane; TG/FTIR/MS analysis; Thermal stability; SILICON OXYCARBIDE; PRECURSORS; PYROLYSIS; MONTMORILLONITE; BEHAVIOR; GLASSES; TRANSFORMATION; DECOMPOSITION; CERAMICS; NETWORKS;
D O I
10.1016/j.polymdegradstab.2022.110200
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Clay-polymer nanocomposites (CPNs) are an important group of materials that are currently receiving increasing attention. The study of the properties of new CPNs is vital, as it facilitates a deeper understanding of their applicability. This study assessed for the first time the thermal stability of clay-polysiloxane nanocomposite as well as their degradation mechanism under an inert atmosphere with the use of the TG/MS/FTIR (simultaneous mass spectrometry and Fourier transform infrared spectroscopy of off-gases from a thermogravimetric analyzer) technique. Organo-montmorillonite (organo-Mt) nanofiller was introduced at different amounts (0, 1, 2, 4, and 8 wt% in relation to the weight of the polymer matrix) into the structure-controlled polysiloxane network. The polysiloxane matrix was obtained by cross-linking poly(methylhydrosiloxane) with poly(dimethylsiloxane) terminated by vinyldimethylsiloxy groups at both ends. This cross-linking was carried out through a hydrosilylation reaction with an equimolar ratio of Si-H and Si-CH=CH2 groups, in the presence of Karstedt's catalyst. Along with an increased amount of organo-Mt, a deterioration in nanocomposites thermal stability, with an increase in the number of thermal decomposition steps, and changes in the degradation mechanism of polysiloxane matrix were observed. The presence of organo-Mt mainly affected the redistribution of bonds at the silicon atoms during the thermolysis of the studied materials. Regardless of the amount of the mineral nanofiller added, the nanocomposites had a similar residual mass remaining after pyrolysis of the studied CPNs at 1000 degrees C, which was much lower than that of the initial polysiloxane network.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] TG-MS and TG-FTIR applied for an unambiguous thermal analysis of intumescent coatings
    Kunze, R
    Schartel, B
    Bartholmai, M
    Neubert, D
    Schriever, R
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2002, 70 (03): : 897 - 909
  • [42] Thermal and kinetic study of tyre waste pyrolysis via TG-FTIR-MS analysis
    Galvagno, S.
    Casu, S.
    Martino, M.
    Di Palma, E.
    Portofino, Sabrina
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2007, 88 (02) : 507 - 514
  • [43] Thermal and kinetic study of tyre waste pyrolysis via TG-FTIR-MS analysis
    S. Galvagno
    S. Casu
    M. Martino
    E. Di Palma
    Sabrina Portofino
    Journal of Thermal Analysis and Calorimetry, 2007, 88 : 507 - 514
  • [44] Compositional and kinetic study of thermal degradation of kerogen using TG-FTIR, NMR, and microscopic study
    Baruah, Bhargav
    Tiwari, Pankaj
    AICHE JOURNAL, 2022, 68 (01)
  • [45] Assessment of the thermal degradation characteristics of isomeric poly(styrene)s using TG, TG/MS and TG/GC/MS
    Howell, BA
    Cui, YM
    Priddy, DB
    THERMOCHIMICA ACTA, 2003, 396 (1-2) : 167 - 177
  • [46] TG-FTIR analysis of PVC thermal degradation and HCl removal
    Zhu, H. M.
    Jiang, X. G.
    Yan, J. H.
    Chi, Y.
    Cen, K. F.
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2008, 82 (01) : 1 - 9
  • [47] Thermal degradation of polyurethanes containing lignin studied by TG-FTIR
    Hirose, S
    Kobashigawa, K
    Izuta, Y
    Hatakeyama, H
    POLYMER INTERNATIONAL, 1998, 47 (03) : 247 - 256
  • [48] TG-FTIR study of the thermal degradation of polyoxymethylene (POM)/thermoplastic polyurethane (TPU) blends
    Pielichowski, K
    Leszczynska, A
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2004, 78 (02) : 631 - 637
  • [49] TG-FTIR study of the thermal degradation of polyoxymethylene (POM)/thermoplastic polyurethane (TPU) blends
    K. Pielichowski
    A. Leszczyńska
    Journal of Thermal Analysis and Calorimetry, 2004, 78 : 631 - 637
  • [50] TG-FTIR analysis of PVC thermal degradation and HCl removal
    Zhu, H.M.
    Jiang, X.G.
    Yan, J.H.
    Chi, Y.
    Cen, K.F.
    Journal of Analytical and Applied Pyrolysis, 2008, 82 (01): : 1 - 9