Effect of Isothermal Aging on the Magnetic Properties of 1Cr-0.5Mo Steel

被引:0
|
作者
Kim, Min-gi [1 ,2 ]
Ryu, K. S. [1 ]
Lee, Y. H. [1 ]
Park, J. S. [1 ]
Kim, C. G. [2 ]
机构
[1] Korea Res Inst Stand & Sci, Div Ind Metrol, Taejon 305340, South Korea
[2] Chungnam Natl Univ, Dept Mat Engn, Taejon 305340, South Korea
关键词
1Cr-0.5Mo steel; coercivity; hysteresis loss; Rockwell hardness; carbide; isothermal aging; 1CR-1MO-0.25V STEEL;
D O I
10.4283/JMAG.2011.16.3.225
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Magnetic properties and Rockwell hardness of 1Cr-0.5Mo steel have been investigated as a function of isothermal aging time. Our results showed that coercivity, hysteresis loss and Rockwell hardness in the aged samples decreased as aging time increased. This phenomenon was analyzed using optical microscopy and scanning electron microscopy. A significant diffusion of Cr and Mo atoms formed M(2)C and M(7)C carbides, lowering the matrix strength. M(2)C and M(7)C carbides partially segregated inside grains, diffused into grain boundaries, and finally resulted in a soft ferrite matrix and a hard grain boundary. The magnetic and mechanical softening of the matrix is likely to govern the properties of the sample more than the hardening of the grain boundary by carbide precipitations.
引用
收藏
页码:225 / 228
页数:4
相关论文
共 50 条
  • [1] MICROSTRUCTURAL EXAMINATION OF 1CR-0.5MO STEEL DURING CREEP
    AFROUZ, A
    COLLINS, MJ
    PILKINGTON, R
    METALS TECHNOLOGY, 1983, 10 (DEC): : 461 - 463
  • [2] Extrapolation of creep life data for 1Cr-0.5Mo steel
    Wilshire, B.
    Scharning, P. J.
    INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2008, 85 (10) : 739 - 743
  • [3] CORRELATION BETWEEN THE MICROSTRUCTURE AND THE MECHANICAL STRENGTH OF STEEL 1Cr-0.5Mo
    Ramos, Emanuel
    Bottarini, Francisco
    Gutierrez, Nicolas
    Gonzalez, Gabriel
    Moro, Lilian
    AVANCES EN CIENCIAS E INGENIERIA, 2016, 7 (04): : 9 - 15
  • [4] Degradation Evaluation of 1Cr-0.5Mo Steel using Barkhausen Noise
    Kim, Min-Gi
    Park, Jong-Seo
    Lee, Yun-Hee
    Kim, CheolGi
    Ryu, Kwon-Sang
    JOURNAL OF THE KOREAN MAGNETICS SOCIETY, 2011, 21 (04): : 136 - 140
  • [5] CAVITATION IN NEW AND SERVICE-EXPOSED 1CR-0.5MO STEEL
    BOLLERUP, J
    HERTZMAN, S
    LUDVIGSEN, PB
    SANDSTROM, R
    VONWALDEN, E
    HIGH TEMPERATURE TECHNOLOGY, 1986, 4 (01): : 3 - 11
  • [6] A study on fretting fatigue behavior of degraded 1Cr-0.5Mo steel
    Kwon, JD
    Choi, S
    Bae, Y
    ADVANCES IN FRACTURE AND FAILURE PREVENTION, PTS 1 AND 2, 2004, 261-263 : 1221 - 1226
  • [7] Effect of cyclic heat treatment on carbide evolution and impact toughness of 1Cr-0.5Mo steel
    Chen Guang-xing
    Zhang Yong-wei
    Xu Xiao-chang
    Xu Chen
    Li Hong-ying
    Zhao Ming-chun
    CAILIAO GONGCHENG-JOURNAL OF MATERIALS ENGINEERING, 2020, 48 (12): : 135 - 140
  • [8] Effect of isothermal aging on magnetic properties in 12Cr steel
    Kim, C. S.
    Kim, I. H.
    Park, I. K.
    Hyun, C. Y.
    EXPERIMENTAL MECHANICS IN NANO AND BIOTECHNOLOGY, PTS 1 AND 2, 2006, 326-328 : 1201 - +
  • [9] Nondestructive Evaluation for Remanent Life of 1Cr-0.5Mo Steel by Reversible Permeability
    Ryu, Kwon-sang
    Lee, Yun Hee
    Park, Jong Seo
    Baek, Un Bong
    JOURNAL OF MAGNETICS, 2012, 17 (03) : 206 - 209
  • [10] MICROSTRUCTURAL CHANGES IN 1CR-0.5MO STEEL AFTER 20 YEARS OF SERVICE
    BISS, VA
    WADA, T
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1985, 16 (01): : 109 - 114