Brazing of 6061 aluminum alloy/Ti-6Al-4V using Al-Si-Cu-Ge filler metals

被引:68
|
作者
Chang, S. Y. [1 ]
Tsao, L. C. [2 ]
Lei, Y. H. [1 ]
Mao, S. M. [1 ]
Huang, C. H. [3 ]
机构
[1] Natl Yunlin Univ Sci & Technol, Dept Mech Engn, Touliu 64002, Yunlin, Taiwan
[2] Natl Pingtung Univ Sci & Technol, Dept Mat Engn, Neipu 91201, Pingtung, Taiwan
[3] Met Ind Res & Dev Ctr, Kaohsiung 81160, Taiwan
关键词
Brazing; Aluminum alloys; Ti-6Al-4V; Al-Si-Cu-Ge alloys; Rare-earth elements; MICROSTRUCTURE;
D O I
10.1016/j.jmatprotec.2011.07.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-8.4Si-20Cu-10Ge and mixed rare-earth elements (Re) containing Al-8.4Si-20Cu-10Ge-0.1Re filler metals were used for brazing of 6061 aluminum alloy/Ti-6Al-4V. The addition of 20 wt.% copper and 10 wt.% germanium into the Al-12Si filler metal lowered the solidus temperature from 586 degrees C to 489 degrees C and the liquidus temperature from 592 degrees C to 513 degrees C. The addition of 0.1 wt.% rare-earth elements into Al-8.4Si-20Cu-10Ge alloy caused remarkable Al-rich phase refinement and transformed the needle-like Al2Cu intermetallic compounds into block-like shapes. Shear strengths of the 6061 aluminum alloy/Ti-6AI-4V joints with the two brazing filler metals. Al-8.4Si-20Cu-10Ge and Al-8.4S-20Cu-10Ge-0.1Re, varied insignificantly with brazing periods of 10-60 min. The average shear strength of the 6061 aluminum alloy/Ti-6Al-4V joints brazed with Al-8.4Si-20Cu-10Ge at 530 degrees C was about 20 MPa. Rare-earth elements appeared to improve the reaction of the Al-8.45i-20Cu-10Ge filler metal with Ti-6Al-4V. The joint shear strength of the 6061 aluminum alloy/TI-6Al-4V with Al-8.4Si-20Cu-10Ge-0.1 Re reached about 51 MPa. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:8 / 14
页数:7
相关论文
共 50 条
  • [41] Nucleation Effect of Ti-6Al-4V Powder on Al-Si Eutectic Alloy
    Sarajan, Zohair
    MATERIALS AND MANUFACTURING PROCESSES, 2009, 24 (12) : 1354 - 1358
  • [42] Development of Zn-15Al-xZr filler metals for Brazing 6061 aluminum alloy to stainless steel
    Yang, Jinlong
    Xue, Songbai
    Xue, Peng
    Lv, Zhaoping
    Long, Weimin
    Zhang, Guanxing
    Zhang, Qingke
    He, Peng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 651 : 425 - 434
  • [43] Novel Ti-Zr-Co-Cu-M (M = Sn, V, Al) amorphous/nanocrystalline brazing fillers for joining Ti-6Al-4V alloy
    Bai, Xueyin
    Liu, Minqian
    Pang, Shujie
    Xiong, Huaping
    Ren, Xinyu
    Ren, Haishui
    Zhang, Tao
    MATERIALS CHARACTERIZATION, 2023, 196
  • [44] Strong and Ductile Ti-6Al-4V Alloy Produced by Hot Pressing of Ti-6Al-4V Swarf
    Yang, F.
    Pi, Z. Q.
    Zhao, Q. Y.
    Raynova, S.
    Liu, Q.
    Sharp, K.
    Brandt, M.
    Bolzoni, L.
    Qian, M.
    JOM, 2019, 71 (03) : 1056 - 1061
  • [45] Brazing of 5A01 aluminum alloy using Al-Cu-Si-Ni filler metal
    元琳琳
    史秀梅
    柳旭
    齐岳峰
    黄晓猛
    China Welding, 2018, 27 (04) : 41 - 45
  • [46] Strong and Ductile Ti-6Al-4V Alloy Produced by Hot Pressing of Ti-6Al-4V Swarf
    F. Yang
    Z. Q. Pi
    Q. Y. Zhao
    S. Raynova
    Q. Liu
    K. Sharp
    M. Brandt
    L. Bolzoni
    M. Qian
    JOM, 2019, 71 : 1056 - 1061
  • [47] DIFFUSION BRAZING OF TI-6AL-4V AND STAINLESS STEEL 316L USING AGCUZN FILLER METAL
    Tashi, R. Soltani
    Mousavi, S. A. A. Akbari
    Atabaki, M. Mazar
    METALLURGICAL & MATERIALS ENGINEERING, 2013, 19 (03) : 189 - 199
  • [48] Microstructural and mechanical properties of jointed ZrO2/Ti-6Al-4V alloy using Ti33Zr17Cu50 amorphous brazing filler
    Liu, Y. H.
    Hu, J. D.
    Shen, P.
    Han, X. H.
    Li, J. C.
    MATERIALS & DESIGN, 2013, 47 : 281 - 286
  • [49] Thermomechanical behavior of Ti-6Al-4V alloy
    Farmanesh, K
    Najafi-Zadeh, A
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2003, 19 (03) : 217 - 220
  • [50] Dry drilling of alloy Ti-6Al-4V
    Cantero, JL
    Tardío, MM
    Canteli, JA
    Marcos, M
    Miguélez, MH
    INTERNATIONAL JOURNAL OF MACHINE TOOLS & MANUFACTURE, 2005, 45 (11): : 1246 - 1255