Laser welding of Ti-6.8Mo-4.5Fe-1.5Al (Timetal® LCB) alloy

被引:0
|
作者
Weiss, I [1 ]
Stefansson, N [1 ]
Baeslack, WA [1 ]
Hurley, J [1 ]
Allen, PG [1 ]
Bania, PJ [1 ]
机构
[1] Wright State Univ, Dept Mech & Mat Engn, Dayton, OH 45435 USA
关键词
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Laser welding was utilized to obtain high-integrity welds in 1.5 mm thick LCB sheet. Welds were characterized by narrow fusion and heat-affected zones and a relatively fine beta grain size of about 100 mu m. Postweld heat treatment at 593 degrees C (1100 degrees F) for 4 hours resulted in fine alpha precipitation in the base and weld metals thus producing material with high strength above 1275 MPa (187 KSI) and a tow ductility of about 2%. Heat treatment at 649 degrees C (1200 degrees F) for 8 hours resulted in coarse alpha precipitation both along beta grain boundaries and in beta grain interiors. This material exhibited a lower tensile strength of about 1080 MPa (160 KSI) with higher ductility about 4%. An intermediate level of strength of about 1150 MPa (170 KSI) and significantly improved ductility exceeding 8% was achieved using a duplex heat treatment of 482 degrees C (900 degrees F) for 2 hours + 649 degrees C (1200 degrees F) for 3 hours. Fractography of the welded samples showed the fracture appearance of the fusion zone is mainly transgranular in nature for the as-welded material and intergranular in nature for the aged material. However, a mixture of dimpled type fracture and intergranular fracture mode was observed at the heat-affected zone and base metal for the aged samples.
引用
收藏
页码:561 / 583
页数:23
相关论文
共 50 条
  • [21] EFFECT OF MICROSTRUCTURE, DEFORMATION MODE AND RATE ON MECHANICAL BEHAVIOUR OF ELECTRON-BEAM MELTED Ti-6Al-4V AND Ti-1.5Al-6.8Mo-4.5Fe ALLOYS
    Ivasishin, O. M.
    Akhonin, S., V
    Savvakin, D. G.
    Berezos, V. A.
    Bondarchuk, V., I
    Stasyuk, O. O.
    Markovsky, P. E.
    [J]. USPEKHI FIZIKI METALLOV-PROGRESS IN PHYSICS OF METALS, 2018, 19 (03): : 309 - 336
  • [22] 烧结温度对10TiB/Ti-4.5Al-6.8Mo-1.5Fe复合材料组织与性能的影响
    郑玉凯
    蔡一湘
    陈峰
    闫志巧
    罗兵辉
    [J]. 粉末冶金材料科学与工程, 2013, 18 (04) : 546 - 551
  • [23] Superplastic Deformation Microstructure and Property of Laser Welded Ti-4.5Al-3V-2Fe-2Mo Alloy
    Fu Mingjie
    Chen Li
    Zeng Yuansong
    [J]. RARE METAL MATERIALS AND ENGINEERING, 2018, 47 (08) : 2555 - 2560
  • [24] Ultrasonic Characterization of Microstructural Changes in Ti-10V-4.5Fe-1.5Al β-Titanium Alloy
    Viswanath, A.
    Kumar, Anish
    Jayakumar, T.
    Rao, B. Purnachandra
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2015, 46A (08): : 3393 - 3405
  • [25] Ultrasonic Characterization of Microstructural Changes in Ti-10V-4.5Fe-1.5Al β-Titanium Alloy
    A. Viswanath
    Anish Kumar
    T. Jayakumar
    B. Purnachandra Rao
    [J]. Metallurgical and Materials Transactions A, 2015, 46 : 3393 - 3405
  • [26] Microstructure and texture of rolled and annealed β titanium alloy Ti-10V-4.5Fe-1.5Al
    Singh, AK
    Bhattacharjee, A
    Gogia, AK
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1999, 270 (02): : 225 - 230
  • [27] Microstructure and texture of rolled and annealed β titanium alloy Ti-10V-4.5Fe-1.5Al
    Singh, A.K.
    Bhattacharjee, Amit
    Gogia, A.K.
    [J]. Materials Science and Engineering A, 1999, 270 (02): : 225 - 230
  • [28] Study on the toughening mechanism of Ti-4.5Al-5Mo-1.5Cr alloy with the valence electron theory
    Liu, WD
    Liu, ZL
    Qu, H
    [J]. ACTA METALLURGICA SINICA, 2002, 38 (12) : 1246 - 1250
  • [29] Study on the toughening mechanism of Ti-4.5Al-5Mo-1.5Cr alloy with the valence electron theory
    Liu, Weidong
    Liu, Zhilin
    Qu, Hua
    [J]. Jinshu Xuebao/Acta Metallurgica Sinica, 2002, 38 (12):
  • [30] NEW TITANIUM-ALLOY WITH IMPROVED FRACTURE TOUGHNESS - TI-4.5AL-5MO-1.5CR
    BERRYMAN, RG
    CHESNUTT, JC
    FROES, FH
    WILLIAMS, JC
    [J]. JOURNAL OF AIRCRAFT, 1977, 14 (12): : 1182 - 1185