Workpiece surface integrity when milling Udimet 720 superalloy

被引:4
|
作者
Hood, R. [1 ]
Morris, J. [1 ]
Soo, S. L. [1 ]
机构
[1] Univ Birmingham, Sch Mech Engn, Machining Res Grp, Birmingham B15 2TT, W Midlands, England
关键词
Milling; nickel alloy; cutting environment; MACHINABILITY; PERFORMANCE; DRY;
D O I
10.1016/j.procir.2016.02.344
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The paper details a comprehensive investigation into the surface integrity of Udimet 720 following end milling under different environment conditions (dry, flood, higher pressure and MQL) and cutting speed (25 and 50m/min). Surface roughness (Ra) was < 0.25 mu m regardlss of tool condition with no white layers detected on any of the samples analysed. Residual stress measurements indicated surface compressive stress of 120 MPa on workpieces milled using new cutters under MQL environment. In contrast, worn tools produced surface tensile stresses of similar to 80 MPa, with subsurface compressive residual stress of up to similar to 400 MPa at a depth of 80 mu m. (C) 2016 The Authors. Published by Elsevier B.V.
引用
收藏
页码:283 / 286
页数:4
相关论文
共 50 条
  • [41] Characterization of hot deformation behavior of Udimet720Li superalloy using processing map
    Wang, Jianguo
    Liu, Dong
    Wang, Tao
    Yang, Yanhui
    ADVANCES IN MATERIALS AND MATERIALS PROCESSING IV, PTS 1 AND 2, 2014, 887-888 : 1161 - +
  • [42] Tool wear and workpiece surface integrity when high speed ball nose end milling hardened AISI H13
    Axinte, DA
    Dewes, RC
    METAL CUTTING AND HIGH SPEED MACHINING, 2002, : 171 - 179
  • [43] The impact of grain boundary serration treatments on the creep deformation of Udimet-720Li superalloy
    Chen, Tso-Wei
    Wu, Bo-Chen
    Kang, Yung-Chang
    Murakami, Hideyuki
    Toda, Yoshiaki
    Chung, Tsai-Fu
    Misra, R. Devesh Kumar
    Yeh, An-Chou
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2025, 924
  • [44] Workpiece surface integrity considerations when finish turning gamma titanium aluminide
    Sharman, ARC
    Aspinwall, DK
    Dewes, RC
    Bowen, P
    WEAR, 2001, 249 (5-6) : 473 - 481
  • [45] High temperature low cycle fatigue behaviour of hot isostatically pressed superalloy Udimet 720 LI
    Prasad, Kartik
    Sarkar, Rajdeep
    Ghosal, P.
    Rao, G. Appa
    Kumar, Vikas
    MATERIALS AT HIGH TEMPERATURES, 2011, 27 (04) : 295 - 300
  • [46] Small and long fatigue crack growth behaviour of a PM Ni-based superalloy, Udimet 720
    Luo, J
    Bowen, P
    INTERNATIONAL JOURNAL OF FATIGUE, 2004, 26 (02) : 113 - 124
  • [47] An investigation on quench cracking behavior of superalloy udimet 720LI using a fracture mechanics approach
    J. Mao
    K. -M. Chang
    V. L. Keefer
    D. Furrer
    Journal of Materials Engineering and Performance, 2000, 9 : 204 - 214
  • [48] EXPERIMENTAL STUDY ON SURFACE INTEGRITY IN END MILLING OF HASTELLOY C-2000 SUPERALLOY
    Razak, N. H.
    Rahman, M. M.
    Kadirgama, K.
    INTERNATIONAL JOURNAL OF AUTOMOTIVE AND MECHANICAL ENGINEERING, 2014, 9 : 1578 - 1587
  • [49] Influence of Tool Flank Wear on Surface Integrity in Orthogonal Milling of Powder Metallurgy Superalloy
    Du, Jin
    Liu, Zhanqiang
    HIGH SPEED MACHINING V, 2012, 723 : 182 - 187
  • [50] Evaluation of Nano Fluids with Minimum Quantity Lubrication in Turning of Ni-Base Superalloy UDIMET 720
    Ozbek, Onur
    LUBRICANTS, 2023, 11 (04)