Characteristics of glass sealants for intermediate-temperature solid oxide fuel cell applications

被引:22
|
作者
Wang, Sea-Fue [1 ]
Lu, His-Chuan [1 ]
Liu, Yi-Xin [1 ]
Hsu, Yung-Fu [1 ]
Liu, Zu-You [1 ]
机构
[1] Natl Taipei Univ Technol, Dept Mat & Mineral Resources Engn, 1 Sec 3,Chung Hsiao E Rd, Taipei 106, Taiwan
关键词
Solid oxide fuel cell; Sealing materials; Thermal properties; Glass; THERMAL-PROPERTIES; CERAMIC SEALANT; SEALING GLASS; SOFCS;
D O I
10.1016/j.ceramint.2017.05.211
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, seven glass sealants were explored for use in intermediate-temperature solid-oxide fuel cells (ITSOFCs): one with boron oxide and an alkaline earth metal (AEM) oxide (GS01), one with boron oxide and free of AEM oxides (GS02), two with AEM oxides but free of boron oxide (GS03 and GS06), and three free of both boron oxide and AEM oxides (GS04, GS05, and GS07). The thermal stability, adhesion, and sealing properties of the glass systems were examined with respect to SUS 430 stainless steel (SUS430). All the glass sealants had electrical resistivities greater than 10(6) Omega-cm. The glass transition points ranged from 632 degrees C to 800 degrees C, while the glass softening points ranged from 708 degrees C to 852 degrees C. The GS01 and GS06 glasses, which contained AEM oxides, had lower glass crystal temperatures (< 785 degrees C) and high coefficients of thermal expansion (CTE; > 11.6 ppm/ degrees C), comparable to those of SUS430. The glasses without AEM oxides had lower CTEs but possessed good thermal stability at 700 degrees C. The glasses exhibited different levels of crystallization after being held at a sealing temperature of 850 degrees C for 1 h. With further soaking at 700 degrees C for 200 h, no new phases were formed. Scanning electron microscopy (SEM) was used to examine cross-sections of the interfaces of the glasses with SUS430 after heat treatment at 850 degrees C. The SEM results indicate that chromate was formed at the interfaces of the glasses containing AEM oxides (GS01, GS03, and GS06) and SUS430, while the glasses that were free of AEM oxides had smooth interfaces with SUS430 but cracks along the interfaces caused by the large differences in the CTEs. No significant inter-diffusion of species across any of the glass SUS430 interfaces was observed. The leak rates of the glass seals were measured at 700 degrees C for 500 h after joining at 850 degrees C. The GS02 glass had the lowest leak rate of 0.017 sccm/cm. The glasses containing AEM oxides (GS01, GS03, and GS06) had high leak rates but good bond strength with SUS430. The GS06 glass had the highest bond strength, greater than 11 MPa.
引用
收藏
页码:S613 / S620
页数:8
相关论文
共 50 条
  • [41] Preparation and evaluation of new composites as anodes for intermediate-temperature solid oxide fuel cells
    Bao, Weitao
    Cheng, Jihai
    Hu, Zhanyong
    Jin, Sijia
    SOLID STATE IONICS, 2010, 181 (29-30) : 1366 - 1371
  • [42] Interface engineering to improve electrochemical performance of intermediate-temperature solid oxide fuel cells
    Yoo, Hyun Sik
    Kim, Seo Ju
    Megra, Yonas Tsegaye
    Lee, Jongseo
    Suk, Ji Won
    Lee, Wonyoung
    APPLIED SURFACE SCIENCE, 2023, 639
  • [43] Double Perovskite Material as An Electrode for Intermediate-Temperature Solid Oxide Fuel Cells Application
    Zhang Wenrui
    Zhang Zhihui
    Gao Liguo
    Ma Tingli
    PROGRESS IN CHEMISTRY, 2016, 28 (06) : 961 - 974
  • [44] Gradual internal methane reforming in intermediate-temperature solid-oxide fuel cells
    Vernoux, P
    Guindet, J
    Kleitz, M
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1998, 145 (10) : 3487 - 3492
  • [45] Fe-based perovskites as electrodes for intermediate-temperature solid oxide fuel cells
    Hou, Shu-en
    Aguadero, Ainara
    Antonio Alonso, Jose
    Goodenough, John B.
    JOURNAL OF POWER SOURCES, 2011, 196 (13) : 5478 - 5484
  • [46] Nanoengineered BSCF Cathode Materials for Intermediate-Temperature Solid-Oxide Fuel Cells
    Darab, Mahdi
    Toprak, Muhammet S.
    Syvertsen, Guttorm Ernst
    Muhammed, Mamoun
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2009, 156 (08) : K139 - K143
  • [47] Development of intermediate-temperature solid oxide fuel cells for direct utilization of hydrocarbon fuels
    Lu, C
    An, S
    Worrell, WL
    Vohs, JM
    Gorte, RJ
    SOLID STATE IONICS, 2004, 175 (1-4) : 47 - 50
  • [48] Influence of Thermal Conductivity on the Thermal Behavior of Intermediate-Temperature Solid Oxide Fuel Cells
    Aman, Nurul Ashikin Mohd Nazrul
    Muchtar, Andanastuti
    Rosli, Masli Irwan
    Baharuddin, Nurul Akidah
    Somalu, Mahendra Rao
    Kalib, Noor Shieela
    JOURNAL OF ELECTROCHEMICAL SCIENCE AND TECHNOLOGY, 2020, 11 (02) : 132 - 139
  • [49] A low-Cr metallic interconnect for intermediate-temperature solid oxide fuel cells
    Geng, Shujiang
    Zhu, Jiahong
    Brady, Michael P.
    Anderson, Harlan U.
    Zhou, Xiao-Dong
    Yang, Zhenguo
    JOURNAL OF POWER SOURCES, 2007, 172 (02) : 775 - 781
  • [50] A Layered Perovskite EuBaCo2O5+δ for Intermediate-Temperature Solid Oxide Fuel Cell Cathode
    Shi, Z.
    Xia, T.
    Meng, F.
    Wang, J.
    Lian, J.
    Zhao, H.
    Bassat, J. -M.
    Grenier, J. -C.
    Meng, J.
    FUEL CELLS, 2014, 14 (06) : 979 - 990