Application of X-ray microtomography to analysis of cavitation in AZ61 magnesium alloy during hot deformation

被引:11
|
作者
Rashed, H. M. M. A. [1 ]
Robson, J. D. [1 ]
Bate, P. S. [1 ]
Davis, B. [2 ]
机构
[1] Univ Manchester, Ctr Mat Sci, Manchester M1 7HS, Lancs, England
[2] Magnesium Elektron N Amer, Madison, IL 62060 USA
基金
英国工程与自然科学研究理事会;
关键词
Magnesium alloys; Tomography; Superplasticity; Failure; TEXTURE; EVOLUTION; BEHAVIOR; STRAIN; SIZE;
D O I
10.1016/j.msea.2010.11.083
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The efficiency of particles in acting as cavity formation sites during hot deformation was investigated for a fine-grained wrought magnesium-aluminium-zinc (AZ series) alloy using X-ray micro tomography. Two methodologies were developed to determine the particle/cavity association from 3-dimensional data, each clearly demonstrating that particles act as a major formation site for cavitation. The particles forming cavities were identified and characterised. It is shown that progressively smaller particles nucleate cavities as strain increases. This is due to concurrent grain growth which reduces the critical particle diameter for cavity nucleation during testing, leading to a continuous cavity nucleation. Particle agglomerates are shown to be particularly potent sites for cavity formation, leading to large and complex shaped cavities even if the individual particles within the agglomerate are below the critical particle diameter for cavity nucleation. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:2610 / 2619
页数:10
相关论文
共 50 条
  • [31] Application of Artificial Neural Network (ANN) to Hot Extrusion of AZ61 Magnesium Alloy Structural Parts
    Hsiang, Su-Hai
    Lin, Yi-Wei
    Lee, Tsang-Cheng
    JOURNAL OF THE CHINESE SOCIETY OF MECHANICAL ENGINEERS, 2010, 31 (01): : 67 - 73
  • [32] Thixotropic deformation behavior of semi-solid AZ61 magnesium alloy during compression process
    Yan, Hong
    Zhou, Bingfen
    MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY, 2006, 132 (1-2): : 179 - 182
  • [33] Deformation behavior of AZ61 magnesium alloy systematically rolled and annealed at 450 °C
    Sulkowski, B.
    Palka, P.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2016, 54 (03): : 147 - 151
  • [34] Effect of Zinc and Severe Plastic Deformation on Mechanical Properties of AZ61 Magnesium Alloy
    Huang, Song-Jeng
    Wu, Sheng-Yu
    Subramani, Murugan
    MATERIALS, 2024, 17 (07)
  • [35] Continuous characterization by X-ray microtomography of damage during high-temperature deformation of magnesium alloy
    Lhuissier, P.
    Scheel, M.
    Salvo, L.
    Di Michiel, M.
    Blandin, J. J.
    SCRIPTA MATERIALIA, 2013, 69 (01) : 85 - 88
  • [36] The solidification behavior of the AZ61 magnesium alloy during electromagnetic vibration processing
    Li, Mingjun
    Tamura, Takuya
    Omura, Naoki
    Miwa, Kenji
    JOURNAL OF ALLOYS AND COMPOUNDS, 2010, 494 (1-2) : 116 - 122
  • [37] Dislocation multiplication behavior of AZ61 magnesium alloy during cyclic bending
    Tian Tie
    Yuan Zhao-cheng
    Mi Lin
    Mao Xing-zi
    PROCEEDINGS OF THE 3RD INTERNATIONAL CONFERENCE ON MATERIAL, MECHANICAL AND MANUFACTURING ENGINEERING, 2015, 27 : 2147 - 2150
  • [38] Effect of Ca precipitation on texture development of AZ61 magnesium alloy during high-temperature deformation
    K. B. Kim
    S. M. Cho
    K. H. Kim
    MRS Advances, 2022, 7 : 829 - 834
  • [39] Dynamic behavior of extruded AZ61 Mg alloy during hot compression
    Wu, Horng-yu
    Yang, Jie-chen
    Liao, Jing-hao
    Zhu, Feng-jun
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 535 : 68 - 75
  • [40] Grain Refinement in AZ61 Mg Alloy during Hot Cyclic Bending
    Jiang, Yupei
    Yang, Xuyue
    Zhang, Lei
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION: NANOSPD5, PTS 1 AND 2, 2011, 667-669 : 623 - 627