Application of X-ray microtomography to analysis of cavitation in AZ61 magnesium alloy during hot deformation

被引:11
|
作者
Rashed, H. M. M. A. [1 ]
Robson, J. D. [1 ]
Bate, P. S. [1 ]
Davis, B. [2 ]
机构
[1] Univ Manchester, Ctr Mat Sci, Manchester M1 7HS, Lancs, England
[2] Magnesium Elektron N Amer, Madison, IL 62060 USA
基金
英国工程与自然科学研究理事会;
关键词
Magnesium alloys; Tomography; Superplasticity; Failure; TEXTURE; EVOLUTION; BEHAVIOR; STRAIN; SIZE;
D O I
10.1016/j.msea.2010.11.083
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The efficiency of particles in acting as cavity formation sites during hot deformation was investigated for a fine-grained wrought magnesium-aluminium-zinc (AZ series) alloy using X-ray micro tomography. Two methodologies were developed to determine the particle/cavity association from 3-dimensional data, each clearly demonstrating that particles act as a major formation site for cavitation. The particles forming cavities were identified and characterised. It is shown that progressively smaller particles nucleate cavities as strain increases. This is due to concurrent grain growth which reduces the critical particle diameter for cavity nucleation during testing, leading to a continuous cavity nucleation. Particle agglomerates are shown to be particularly potent sites for cavity formation, leading to large and complex shaped cavities even if the individual particles within the agglomerate are below the critical particle diameter for cavity nucleation. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:2610 / 2619
页数:10
相关论文
共 50 条
  • [1] Microstructural evolution of AZ61 magnesium alloy during hot deformation
    Zhou, HT
    Zeng, XQ
    Liu, LL
    Dong, J
    Wang, QD
    Ding, WJ
    Zhu, YP
    MATERIALS SCIENCE AND TECHNOLOGY, 2004, 20 (11) : 1397 - 1402
  • [2] Characteristics of cavitation behavior during superplastic deformation in AZ61 magnesium alloy
    Aguirre, JV
    Hosokawa, H
    Higashi, K
    PRICM 4: FORTH PACIFIC RIM INTERNATIONAL CONFERENCE ON ADVANCED MATERIALS AND PROCESSING, VOLS I AND II, 2001, : 2039 - 2042
  • [3] Cavitation during grain-boundary-sliding deformation in an AZ61 magnesium alloy
    Takigawa, Yorinobu
    Aguirre, Juan Velazquez
    Taleff, Eric M.
    Higashia, Kenji
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 497 (1-2): : 139 - 146
  • [4] Flow stress behavior of AZ61 magnesium alloy during hot compression deformation
    Tsao, L. C.
    Huang, Yen-Teng
    Fan, Kuo-Huan
    MATERIALS & DESIGN, 2014, 53 : 865 - 869
  • [5] Microstructure in as-cast AZ61 magnesium alloy during hot compression deformation
    Wang, Shao-Nan
    Tang, Guo-Yi
    Fu, Wan-Tang
    Lü, Zhi-Qing
    Guan, Lei
    Cailiao Rechuli Xuebao/Transactions of Materials and Heat Treatment, 2009, 30 (05): : 39 - 43
  • [6] Hot deformation behavior of as-cast AZ61 magnesium alloy
    Feng Zhongxue
    Shi Qingnan
    Pan Fusheng
    Tan Jun
    Chen Liangwei
    Chen Xiliang
    ADVANCED ENGINEERING MATERIALS III, PTS 1-3, 2013, 750-752 : 574 - +
  • [7] Experimental investigation of cavitation behavior in AZ61 magnesium alloy
    Aguirre, JV
    Takigawa, Y
    Higashi, K
    MATERIALS TRANSACTIONS, 2005, 46 (03) : 626 - 630
  • [8] Hot Cracking in AZ31 and AZ61 Magnesium Alloy
    Huang, C. J.
    Cheng, C. M.
    Chou, C. P.
    Chen, F. H.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (07) : 633 - 640
  • [9] Hot Cracking in AZ31 and AZ61 Magnesium Alloy
    C.J. Huang1)
    JournalofMaterialsScience&Technology, 2011, 27 (07) : 633 - 640
  • [10] Evaluation of the Effects of SiCp on Hot Deformation Behavior and Microstructure of AZ61 Magnesium Alloy
    Yu-Chih Tzeng
    Hsieh Yi-Chiuan
    Journal of Materials Engineering and Performance, 2024, 33 : 1919 - 1930