Growth of Al2O3/ZrO2(Y2O3) eutectic rods by the laser floating zone technique:: effect of the rotation

被引:30
|
作者
de Francisco, I [1 ]
Merino, RI [1 ]
Orera, VM [1 ]
Larrea, A [1 ]
Peña, JI [1 ]
机构
[1] Univ Zaragoza, CSIC, Inst Ciencia Mat Aragon, Zaragoza 50018, Spain
关键词
composites; microstructure; Al2O3-ZrO2; directionally solidified eutectics;
D O I
10.1016/j.jeurceramsoc.2005.01.017
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The laser floating zone technique has been applied to the growth of Al2O3/ZrO2(Y2O3) rods in the eutectic composition to reveal the effect of forced convection induced by rotation on the rod microstructure. A systematic experimental study of this effect has been carried out combining different source rod and/or eutectic rod rotation (0-200rpm) and travelling speeds (10-1500 mm/h) in an axial thermal gradient close to 6 x 10(5) C/m. The results indicate that the rotation is useful to achieve a more homogeneous temperature distribution, especially in thick rods but it has a limited effect in the change of the solidification front shape. The forced convection in the floating zone caused by rotation slightly flattens the solidification interface enhancing the homogeneity of the phase distribution across the sample. However, it introduces several new microstructural features like banding and phase coarsening that can deteriorate the mechanical behaviour of the rods. On the other hand, rods above 1.6 mm in diameter cannot be grown Without cracks, even with fast eutectic rod rotation. Rotation does not change the pulling rate threshold (50 mm/h) at which the transition from Coupled to dendritic and cellular growth morphology takes place. (c) 2004 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1341 / 1350
页数:10
相关论文
共 50 条
  • [31] Directional solidification and growth characteristics of Al2O3/Er3Al5O12/ZrO2 ternary eutectic ceramic by laser floating zone melting
    Qun Ren
    Haijun Su
    Jun Zhang
    Weidan Ma
    Yewei Cao
    Jun Chen
    Lin Liu
    Hengzhi Fu
    Journal of Materials Science, 2017, 52 : 5559 - 5568
  • [32] Directional solidification and growth characteristics of Al2O3/Er3Al5O12/ZrO2 ternary eutectic ceramic by laser floating zone melting
    Ren, Qun
    Su, Haijun
    Zhang, Jun
    Ma, Weidan
    Cao, Yewei
    Chen, Jun
    Liu, Lin
    Fu, Hengzhi
    JOURNAL OF MATERIALS SCIENCE, 2017, 52 (10) : 5559 - 5568
  • [33] Nano/Micro-Laminated (ZrO2–Y2O3)/(Al2O3–Y2O3) Composite Coatings and Their Oxidation Resistance
    Mingming Yao
    Yedong He
    Deren Wang
    Wei Gao
    Oxidation of Metals, 2007, 68 : 1 - 8
  • [34] Growth and characterization of Al2O3/Y3Al5O12/ZrO2 ternary eutectic fibers
    Lee, JH
    Yoshikawa, A
    Fukuda, T
    Waku, Y
    JOURNAL OF CRYSTAL GROWTH, 2001, 231 (1-2) : 115 - 120
  • [35] ZrO2 – Al2O3 ceramic with eutectic additives
    A. A. Evteev
    N. A. Makarov
    D. O. Lemeshev
    S. V. Zhitnyuk
    Glass and Ceramics, 2011, 68 : 258 - 262
  • [36] ZrO2 - Al2O3 CERAMIC WITH EUTECTIC ADDITIVES
    Evteev, A. A.
    Makarov, N. A.
    Lemeshev, D. O.
    Zhitnyuk, S. V.
    GLASS AND CERAMICS, 2011, 68 (7-8) : 258 - 262
  • [37] Phase Transformations of Electrochemically Prepared Precursors of the TiO2–ZrO2–Y2O3 and TiO2–Al2O3–ZrO2–Y2O3 Oxide Systems
    A. F. Dresvyannikov
    E. V. Petrova
    L. I. Kashfrazyeva
    A. I. Khairullina
    Inorganic Materials, 2023, 59 : 742 - 748
  • [38] GROWTH AND PROPERTIES OF EUTECTIC MICROCOMPOSITES IN SYSTEM AL2O3/ZRO2
    VIECHNIC.D
    SCHMID, F
    AMERICAN CERAMIC SOCIETY BULLETIN, 1970, 49 (04): : 390 - &
  • [39] Comparing the thermodynamic behaviour of Al(l)+ZrO2(4% Y2O3) and Al(l)+Al2O3
    Copland, Evan
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2006, 97 (08) : 1108 - 1114
  • [40] Interaction of SiC with Al2O3−(t + m)ZrO2(Y2O3) Oxide Composition
    M. G. Frolova
    A. S. Lysenkov
    S. N. Perevislov
    N. V. Petrakova
    K. A. Kim
    M. A. Sevost’yanov
    A. Yu. Ivannikov
    M. D. Mel’nikov
    Yu. F. Kargin
    Russian Journal of Inorganic Chemistry, 2023, 68 (8) : 1077 - 1083