Correlation of dynamic impact properties with adiabatic shear banding behaviour in Ti-15Mo-5Zr-3Al alloy

被引:22
|
作者
Lee, Woei-Shyan [1 ]
Lin, Chi-Feng [2 ]
Chen, Tao-Hsing [1 ]
Hwang, Hsin-Hwa [1 ]
机构
[1] Natl Cheng Kung Univ, Dept Mech Engn, Tainan 701, Taiwan
[2] Natl Ctr High Performance Comp, Hsin 744, Tainan Cty, Taiwan
关键词
Ti-15Mo-5Zr-3Al alloy; impact properties; adiabatic shear band; beta transus temperature; Splats and knobbles;
D O I
10.1016/j.msea.2007.05.027
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A compressive split-Hopkinson pressure bar is used to investigate the impact properties of Ti-15Mo-5Zr-3A1 alloy under strain rates ranging from 800 to 8000s(-1) at temperatures between 25 and 900 degrees C. The morphologies of the deformed microstructures and the fracture features of the adiabatic shear bands on the fracture surfaces are examined using optical and scanning electron microscopes. Based on the macroscopic and microscopic observations, the dynamic impact properties of the alloy are correlated with its adiabatic shear banding behaviour. The experimental results indicate that the strain rate and testing temperature both have a significant effect on the mechanical properties of Ti-15Mo-5Zr-3Al alloy. At a constant temperature, the flow stress increases with increasing strain rate. However, at a given strain rate, the flow stress reduces as the temperature increases. Furthermore, the fracture strain decreases with increasing temperature prior to phase transformation at 785 degrees C, but increases thereafter as the temperature is further increased. The temperature-dependent variation of the fracture strain is thought to be related to the amount of a phase in the deformed microstructure, which increases with increasing temperature prior to phase transformation, but dissolves entirely at higher temperatures and is replaced by a pure P phase. Fractographic analysis reveals that the specimens fracture as a consequence of adiabatic shear band formation. Specimens impacted at higher strain rates and lower temperatures are more likely to form adiabatic shear bands. The width of the shear band decreases with increasing temperature prior to phase transformation, but increases with increasing temperature thereafter. The microhardness within the adiabatic shear band is found to increase slightly in the specimens tested at higher strain rates and temperatures. The fracture surfaces of the impacted specimens exhibit both dimple-like and cleavage-like features. Finally, the splats and knobble-like features observed on the fracture surfaces of specimens deformed at the highest strain rate of 8 x 10(3) s(-1) and temperatures of 300 degrees C or higher, indicate that significant melting takes place during deformation under high strain rate and high temperature loading conditions prior to specimen fracture. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:172 / 184
页数:13
相关论文
共 50 条
  • [21] Effects of Microstructure on the Adiabatic Shear Banding Sensitivity of Ti-6Al-4V-4Zr-Mo Alloy
    Li Jianchong
    Li Shukui
    Fan Qunbo
    Huo Dongmei
    Liu Jie
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 (01) : 45 - 48
  • [22] 高强耐蚀合金Ti-15Mo-5Zr-3Al的发展和应用
    孟祥军
    钛工业进展, 1997, (05) : 25 - 26
  • [23] Fatigue behavior of bulk β-type titanium alloy Ti-15Mo-5Zr-3Al annealed in high temperature nitrogen gas
    Akita, Masayuki
    Uematsu, Yoshihiko
    Kakiuchi, Toshifumi
    Nakajima, Masaki
    Bai, Yu
    Tamada, Kazuhiro
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2015, 627 : 351 - 359
  • [24] βTi-15Mo-5Zr-3Al合金的疲劳裂纹扩展行为的研究
    周吉峰
    中国材料进展, 1999, (05) : 6 - 7
  • [25] The microstructure dependence of fatigue behaviour in Ti-15Mo-5Zr-2Al alloy
    Tokaji, K
    Bian, JC
    Ogawa, T
    Nakajima, M
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 1996, 213 (1-2): : 86 - 92
  • [26] THE EFFECT OF COLD DRAWING AND AGING ON THE STRENGTH OF TI-15MO-5ZR-3AL AND TI-13V-11CR-3AL
    MATSUMOTO, T
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (05): : S699 - S699
  • [27] Phase Transformation of a Ti-15Mo-5Zr-3Al Brazed Joint Using Clad Ti-15Cu-15Ni Filler
    Yue, Gui-Lin
    Chen, Tai-Cheng
    Shiue, Ren-Kae
    Tsay, Leu-Wen
    METALS, 2020, 10 (01)
  • [28] Stability of vacancies in 6-type Ti-15Mo-5Zr-3Al alloy fabricated via laser powder bed fusion
    Mizuno, Masataka
    Sugita, Kazuki
    Do, Kousuke
    Ishimoto, Takuya
    Nakano, Takayoshi
    Araki, Hideki
    ADDITIVE MANUFACTURING LETTERS, 2023, 7
  • [29] Adiabatic shear band in a Ti-3Al-5Mo-4.5V titanium alloy
    Wang, B. F.
    JOURNAL OF MATERIALS SCIENCE, 2008, 43 (05) : 1576 - 1582
  • [30] Adiabatic shear band in a Ti-3Al-5Mo-4.5V Titanium alloy
    B. F. Wang
    Journal of Materials Science, 2008, 43 : 1576 - 1582