Magnetic properties of Sm-Fe-N thick film magnets prepared by the aerosol deposition method

被引:42
|
作者
Sugimoto, S [1 ]
Maeda, T
Kobayashi, R
Akedo, J
Lebedev, M
Inomata, K
机构
[1] Tohoku Univ, Grad Sch Engn, Dept Mat Sci, Sendai, Miyagi 9808579, Japan
[2] Natl Inst Adv Ind Sci & Technol, Ibaraki 3058564, Japan
关键词
aerosol deposition method (ADM); coercivity; high deposition rate; Sm-Fe-N film;
D O I
10.1109/TMAG.2003.816715
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
This paper describes magnetic properties of Sm-Fe-N films prepared by an aerosol deposition method. The films with thickness of 3-45 mum were obtained by the deposition within 10 min and the deposition rate was estimated as approximately 2-10 mum/min. The Sm-Fe-N films showed relatively high micro Vickers hardness in the range from 500 to 700. The remanence of the Sm-Fe-N films was approximately 0.4 T, which was lower than that of initial host powders. However, almost of all samples showed higher coercivities around 1.8 T.
引用
收藏
页码:2986 / 2988
页数:3
相关论文
共 50 条
  • [21] Structures and magnetic properties of Sm-Fe-N bulk magnets produced by the spark plasma sintering method
    Tetsuji Saito
    Journal of Materials Research, 2007, 22 : 3130 - 3136
  • [22] Structures and magnetic properties of Sm-Fe-N bulk magnets produced by the spark plasma sintering method
    Saito, Tetsuji
    JOURNAL OF MATERIALS RESEARCH, 2007, 22 (11) : 3130 - 3136
  • [23] Magnetic properties of anisotropic Sm-Fe-N bulk magnets produced by spark plasma sintering method
    Saito, Tetsuji
    JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, 2008, 320 (13) : 1893 - 1897
  • [24] Influence of Swaging on the Magnetic Properties of Zn-Bonded Sm-Fe-N Magnets
    Kataoka, Kohei
    Matsuura, Masashi
    Tezuka, Nobuki
    Sugimoto, Satoshi
    MATERIALS TRANSACTIONS, 2015, 56 (10) : 88 - 92
  • [25] Magnetic properties of Sm-Fe-N bulk magnets prepared from Sm2Fe17N3 melt-spun ribbons
    Saito, Tetsuji
    Nishio-Hamane, Daisuke
    JOURNAL OF APPLIED PHYSICS, 2015, 117 (17)
  • [26] Extraction of Sm from Sm-Fe-N magnets by the glass slag method
    Saito, T
    Sato, H
    Motegi, T
    Kobayashi, K
    JOURNAL OF ALLOYS AND COMPOUNDS, 2005, 403 (1-2) : 341 - 344
  • [27] Extraction of Sm from Sm-Fe-N magnets by the glass slag method
    Saito, Tetsuji
    Sato, Hironori
    Motegi, Tetsuichi
    Kobayashi, Kurima
    Journal of Alloys and Compounds, 2005, 403 (1-2): : 341 - 344
  • [28] Progress of Sm-Fe-N anisotropic magnets
    Ohmori, Kenji
    Ishikawa, Takashi
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2006, 13 : 221 - 230
  • [29] Magnetic properties of Nd-Fe-B thick film magnets prepared by using arc deposition
    Nakano, M.
    Sahara, M.
    Yamawaki, K.
    Yanai, T.
    Fukunaga, H.
    JOURNAL OF APPLIED PHYSICS, 2010, 107 (09) : 3607
  • [30] Additive manufacturing of Sm-Fe-N magnets
    J.A.B.Engerroff
    A.B.Baldissera
    M.D.Magalh?es
    P.H.Lamar?o
    P.A.P.Wendhausen
    C.H.Ahrens
    J.M.Mascheroni
    JournalofRareEarths, 2019, 37 (10) : 1078 - 1082