The effect of surface modifications on titanium to enable titanium-porcelain bonding

被引:52
|
作者
Troia, Manoel G., Jr. [1 ]
Henriques, Guilherme E. P. [2 ]
Mesquita, Marcelo F. [2 ]
Fragoso, Wagner S. [2 ]
机构
[1] Herminio Ometto Univ, Araras Dent Sch, Dept Prosthodont, BR-13400480 Piracicaba, SP, Brazil
[2] Univ Estadual Campinas, Piracicaba Dent Sch, Dept Prosthodont, Unicamp, Brazil
关键词
cast titanium; ceramics; bond strength;
D O I
10.1016/j.dental.2007.01.009
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives. Titanium-ceramic restorations are currently used, despite the pending problem of titanium-ceramic bonding, which has only been partially solved. The surface treatment of the metal proposed by the manufacturer promotes lower bond strength between titanium and porcelain when compared to the conventional metal-ceramic systems. The objective of this study was to evaluate the influence of acid and caustic baths on the bonding characteristics of specific titanium porcelain bonded to cast commercially pure titanium (CP Ti). Methods. Eighty strips of cast CP Ti were obtained in dimensions of 25 mm x 3 mm x 0.5 mm, and divided into eight groups (n=10) which were subjected to surface treatment by immersion in one of the follow solutions-group HF: HF 10%; group NaOH+HF: NaOH 50%-CuSO4 center dot 5H(2)O 10% followed by HF 10%; group HCl: HCl 35%; group NaOH+HCl: NaOH 50%-CuSO4 5H(2)O 10% followed by HCl 35%; group HNO3: HNO3 35%-HF 5%; group NaOH+HNO3: NaOH 50%-CuSO4 center dot 5H(2)O 10% followed by HNO3 35%-HF 5%; control group: treated according to the manufacturer's instructions; NaOH + control group: treated according to the manufacturer's instructions followed by immersion in NaOH 50%-CuSO4 center dot 5H(2)O 10%. Low fusion porcelain (Vita Titankeramik) was applied to the center of one of the sides of each CP Ti sample with dimensions of 8 mm x 3 mm x 1 mm. All groups were submitted to a three-point flexure test. Scanning electron microscopy (SEM) photomicrographs were taken to characterize the failed surfaces at the titanium-porcelain interface. Anova and Tukey's multiple comparison tests were used to analyze the data at a 5% probability level. Results. All groups treated with NaOH 50%-CuSO4 center dot 5H(2)O 10% solution showed significant superior values when compared to groups treated exclusively with acid solution. There were no significant differences between HF (21.2 MPa) and HCl (23.4 MPa) groups; control (25.2 MPa), HCl (23.4 MPa) and HNO3 (26.6 MPa) groups; NaOH + HF (29.9 MPa) and NaOH + HCl (30.8 MPa) groups; NaOH + HNO3 (34.8 MPa) and NaOH + control (32.1 MPa) groups. SEM analysis indicated a combination of cohesive and adhesive fractures in NaOH + HNO3 and NaOH + control groups, while mainly adhesive fractures were found in the other groups. Significance. Bond strength between porcelain and cast CP Ti can be increased by use of a caustic bath prior to porcelain firing. (c) 2007 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:28 / 33
页数:6
相关论文
共 50 条
  • [21] ON THE BONDING OF PORCELAIN ON TITANIUM
    HAUTANIEMI, JA
    HERO, H
    JUHANOJA, JT
    JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1992, 3 (03) : 186 - 191
  • [22] Effect of Titanium Surface Oxidation on the Bonding Strength of Ti-Porcelain
    Guo Li-Tong
    Liu Xiao-Chen
    Gao Ji-Qiang
    Yang Jian-Feng
    Guo Tian-Wen
    JOURNAL OF INORGANIC MATERIALS, 2009, 24 (05) : 915 - 918
  • [23] EFFECT OF CRYSTALLINE LEUCITE ON PORCELAIN BONDING ON TITANIUM
    HAUTANIEMI, JA
    HERO, H
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1991, 74 (06) : 1449 - 1459
  • [24] Effect of SnOx film on the bonding of titanium–porcelain
    Litong Guo
    Xiaochen Liu
    Zengying He
    Jiqiang Gao
    Jianfeng Yang
    Tianwen Guo
    Journal of Sol-Gel Science and Technology, 2008, 47 : 239 - 242
  • [25] Gold and titanium nitride coatings on cast and machined commercially pure titanium to improve titanium-porcelain adhesion
    Park, Sangwon
    Kim, Yeonmi
    Lim, Hyunpil
    Oh, Gyejeong
    Kim, Hyunseung
    Ong, Joo L.
    Lee, Kwangmin
    SURFACE & COATINGS TECHNOLOGY, 2009, 203 (20-21): : 3243 - 3249
  • [26] Titanium-porcelain system. Part III: Effects of surface modification on bond strengths
    Reyes, MJD
    Oshida, Y
    Andres, CJ
    Barco, T
    Hovijitra, S
    Brown, D
    BIO-MEDICAL MATERIALS AND ENGINEERING, 2001, 11 (02) : 117 - 136
  • [27] Effect of TiO2-SiO2-SnOx sol-gel coating on the bonding strength of titanium-porcelain
    Zhang, Zichuan
    Li, Xiaoyan
    MATERIALS LETTERS, 2016, 180 : 288 - 290
  • [28] Effect of zirconium coating on bonding strength of porcelain to titanium
    School of Materials Science and Engineering, Jilin University, Changchun 130025, China
    不详
    China Weld Eng Ed, 2008, 3 (10-14):
  • [29] The effect of zirconium coating on bonding strength of porcelain to titanium
    段珍珍
    孙大千
    邱小明
    谷晓燕
    孙德新
    China Welding, 2008, (03) : 10 - 14
  • [30] Effects of sandblasting media and steam cleaning on bond strength of titanium-porcelain
    Wang, Che-Shun
    Chen, Ker-Kong
    Tajima, Kiyoshi
    Nagamatsu, Yuki
    Kakigawa, Hiroshi
    Kozono, Yoshio
    DENTAL MATERIALS JOURNAL, 2010, 29 (04) : 381 - 391