20 kW laser welding applied on the international thermonuclear experimental reactor correction coil case welding

被引:3
|
作者
Fang, Chao [1 ,2 ]
Xin, Jijun [1 ,2 ,3 ]
Dai, Wenhua [1 ,2 ,3 ]
Yang, Wuxiong [4 ]
Wei, Jing [1 ,2 ]
Song, Yuntao [1 ,2 ,3 ]
机构
[1] Chinese Acad Sci, Inst Plasma Phys, Hefei, Anhui, Peoples R China
[2] Anhui Key Lab Special Welding Technol, Huainan 232000, Anhui, Peoples R China
[3] Univ Sci & Technol China, Grad Sch, Sci Isl Branch, Hefei 230026, Anhui, Peoples R China
[4] Beijing Univ Technol, Inst Laser Engn, Beijing 100124, Peoples R China
基金
安徽省自然科学基金;
关键词
ITER; austenitic stainless steel; 20kW laser welding; cracking; welding deformation; STEEL;
D O I
10.2351/7.0000057
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
International thermonuclear experimental reactor correction coil cases are made of heavy, thick, high strength, and high toughness austenitic stainless steel 316LN. The BTCC (bottom and top correction coils) case has the dimension of 2.5 x 7 m(2) and cross section of 239.8 x 146.7 mm(2), side correction coil case has the dimension of 7.2 x 7.6 m(2) and cross section of 147.8 x 168 mm(2), and they will be closure welded after winding pack insertion. The 20 mm welding depth, dozens of meter of welding length, strict welding requirements, large size, and complex configuration bring a big challenge to this closure welding work. 20 kW high power laser welding is selected as the main welding method because of the advantage of potential welding deformation control and its penetrating ability and cracking resistance. The welding parameter is developed that can cover the assembly gap from 0 to 0.5 mm with a good welding quality. A special test coupon is designed for the welding procedure qualification, and related tests are carried out to qualify the joint properties of bend, tensile, and impact. Finally, a full-scale BTCC case is welded. After welding, ultrasonic testing confirms that almost all welds satisfy the weld seam quality requirement. The recorded temperatures less than 250 degrees indicate that the temperature induced by welding will not harm the internal winding pack. The dimensional deviation of the inner face is less than 4 mm and also satisfies the tolerance requirement of +/- 2 mm for the BTCC case.