Influence of the styrene content of thermoplastic styrene-butadiene rubbers in the effectiveness of the treatment with sulfuric acid

被引:32
|
作者
Cepeda-Jiménez, CM [1 ]
Pastor-Blas, MM [1 ]
Ferrándiz-Gómez, TP [1 ]
Martín-Martínez, JM [1 ]
机构
[1] Univ Alicante, Dept Inorgan Chem, Adhes & Adhes Lab, E-03080 Alicante, Spain
关键词
polyurethane; surface treatment; rubbers; infrared spectra;
D O I
10.1016/S0143-7496(00)00048-8
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Three thermoplastic block styrene-butadiene-styrene (TR) rubbers were treated with sulfuric acid to improve their adhesion to polyurethane adhesives. T-peel test, scanning electron microscopy (SEM), contact-angle measurements (water, ethane diol), infra red spectroscopy (ATR-IR) and stress-strain experiments were used to analyze the nature of surface modifications produced in the rubber. The length of the treatment and the neutralization procedure (with and without ammonium hydroxide) were considered in this study. The treatment produced the sulfonation of the butadiene units of the rubber and the creation of highly conjugated C=C bonds, which produced a change in the color of the TR rubbers. The treatment also produced a decrease in the tensile strength and the elongation at break of the TR rubbers. This suggests that the treatment with sulfuric acid was not restricted to the rubber surface but also produced a bulk modification. The lower the styrene content in the TR rubber, the more significant modifications were produced on the surface. The styrene content (33-55 wt%) in three thermoplastic styrene-butadiene (TR) rubbers affected the extent, but not the nature of the surface modifications produced by treatment with sulfuric acid. The H2SO4 treatment increased the T-peel strength of S1 and S2 rubber/polyurethane adhesive joints and produced a mixed failure mode (adhesion + cohesive failure in the rubber). Sulfonation of the TR rubbers is fast and needs only a 30s immersion in sulfuric acid to produce high adhesion. Furthermore, the neutralization of the acidic surface with ammonium hydroxide is critical to assure an adequate durability of the adhesive joints. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:161 / 172
页数:12
相关论文
共 50 条
  • [21] Characteristics of the pyrolysis patterns of styrene-butadiene rubbers with differing microstructures
    Choi, SS
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2002, 62 (02) : 319 - 330
  • [22] Slip of styrene-butadiene rubbers: The effects of pressure and viscous heating
    Georgantopoulos, Christos K.
    Zhang, Ziyue
    Pollard, Michael A.
    Causa, Andrea
    Kadar, Roland
    Wilhelm, Manfred
    van Ruymbeke, Evelyne
    Hatzikiriakos, Savvas G.
    PHYSICS OF FLUIDS, 2024, 36 (01)
  • [23] Polybutadiene and Styrene-Butadiene rubbers for high-dose dosimetry
    de Oliveira, Lucas N.
    Vieira, Silvio L.
    Schimidt, Fernando
    Antonio, Patricia L.
    Caldas, Linda V. E.
    2015 4TH INTERNATIONAL CONFERENCE ON ADVANCEMENTS IN NUCLEAR INSTRUMENTATION MEASUREMENT METHODS AND THEIR APPLICATIONS (ANIMMA), 2015,
  • [24] MEASUREMENT AND PREDICTION OF SOLUBILITIES OF ETHYLBENZENE VAPOR IN STYRENE-BUTADIENE RUBBERS
    IWAI, Y
    MIYAMOTO, S
    NAKANO, K
    ARAI, Y
    JOURNAL OF CHEMICAL ENGINEERING OF JAPAN, 1990, 23 (04) : 508 - 510
  • [26] Weak boundary layers on vulcanized styrene-butadiene rubber treated with sulfuric acid
    Cepeda-Jiménez, CM
    Pastor-Blas, MM
    Martín-Martínez, JM
    JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2001, 15 (11) : 1323 - 1350
  • [27] STARCH IN RUBBER - INFLUENCE OF STARCH TYPE AND CONCOMITANT VARIABLES IN REINFORCEMENT OF STYRENE-BUTADIENE RUBBERS
    BUCHANAN, RA
    KWOLEK, WF
    KATZ, HC
    RUSSELL, CR
    STARKE, 1971, 23 (10): : 350 - &
  • [28] SOLUTION AND BULK FLOW PROPERTIES OF LINEAR AND BRANCHED STYRENE-BUTADIENE RUBBERS
    MIERAS, HJMA
    JOURNAL OF POLYMER SCIENCE PART C-POLYMER SYMPOSIUM, 1973, (42): : 987 - 1000
  • [29] STARCH XANTHIDE STYRENE-BUTADIENE RUBBERS - EFFECT OF HUMIDITY AND OUTDOOR WEATHERING
    BUCHANAN, RA
    MCBRIEN, J
    OTEY, FH
    RUSSELL, CR
    STARKE, 1978, 30 (03): : 91 - 96
  • [30] EFFECT OF STRUCTURE OF STYRENE-BUTADIENE COPOLYMERS ON PROPERTIES OF RESINS IN ADMIXTURE WITH RUBBERS
    DINZBURG, BN
    POPOVA, VP
    DYUNINA, VG
    CHALYKH, AE
    COLLOID JOURNAL OF THE USSR, 1976, 38 (02): : 305 - 307