Influence of nickel on secondary hardening of a modified AISI H13 hot work die steel

被引:9
|
作者
Xia, S. W. [1 ]
Zuo, P. [1 ]
Zeng, Y. [1 ]
Wu, X. [1 ]
机构
[1] Shanghai Univ, Sch Mat Sci & Engn, Shanghai 200072, Peoples R China
基金
国家重点研发计划;
关键词
Hot work die steel; nickel content; carbides; secondary hardening; internal friction; DEEP CRYOGENIC TREATMENT; INTERNAL-FRICTION; CARBIDE PRECIPITATION; TEMPERATURE; BEHAVIOR;
D O I
10.1002/mawe.201700205
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
This paper focuses on the effects of nickel on secondary hardening of a modified H13 hot work die steel. Both the non-nickel steel and the nickel-added steel get a secondary hardening peak at 520 degrees C, and the secondary hardening peak trends to increase in the nickel-added steel. On the basis of scanning electron microscope and transmission electron microscope observation, the rise of the secondary hardening peak is in connection with the precipitation of M3C type carbides. More strip-shaped and needle-shaped M3C type carbides precipitated from matrix. By means of internal friction, the result suggests that nickel does not affect the position of the Snoek-Ke-Koster peak, but the height of Snoek-Ke-Koster peak of the nickel-added steel is higher, which indicates nickel enhances the interaction between dislocations and interstitial atoms, promoting the precipitation of carbides.
引用
收藏
页码:197 / 203
页数:7
相关论文
共 50 条
  • [21] Prediction and optimization of cutting temperature on hard-turning of AISI H13 hot work steel
    Ahmed A. Elsadek
    Ahmed M. Gaafer
    S. S. Mohamed
    A. A. Mohamed
    [J]. SN Applied Sciences, 2020, 2
  • [22] Atomic diffusion in laser surface modified AISI H13 steel
    S. N. Aqida
    D. Brabazon
    S. Naher
    [J]. Applied Physics A, 2013, 112 : 139 - 142
  • [23] Atomic diffusion in laser surface modified AISI H13 steel
    Aqida, S. N.
    Brabazon, D.
    Naher, S.
    [J]. APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2013, 112 (01): : 139 - 142
  • [24] Wear Resistance of H13 and a New Hot-Work Die Steel at High temperature
    Shuang Li
    Xiaochun Wu
    Shihao Chen
    Junwan Li
    [J]. Journal of Materials Engineering and Performance, 2016, 25 : 2993 - 3006
  • [25] Wear Resistance of H13 and a New Hot-Work Die Steel at High temperature
    Li, Shuang
    Wu, Xiaochun
    Chen, Shihao
    Li, Junwan
    [J]. JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2016, 25 (07) : 2993 - 3006
  • [26] Effect of strain amplitude on the isothermal fatigue behavior of H13 hot work die steel
    Zhu, Zhen-Qiang
    Ning, Hui
    Zuo, Peng-Peng
    Wu, Xiao-Chun
    [J]. Gongcheng Kexue Xuebao/Chinese Journal of Engineering, 2021, 43 (05): : 656 - 662
  • [27] Characterization of Hot Deformation Behavior and Processing Map of As-Cast H13 Hot Work Die Steel
    Yahui Han
    Changsheng Li
    Jinyi Ren
    Chunlin Qiu
    En LI
    Shuaishuai Chen
    [J]. Metals and Materials International, 2021, 27 : 3574 - 3589
  • [28] Characterization of Hot Deformation Behavior and Processing Map of As-Cast H13 Hot Work Die Steel
    Han, Yahui
    Li, Changsheng
    Ren, Jinyi
    Qiu, Chunlin
    Li, En
    Chen, Shuaishuai
    [J]. METALS AND MATERIALS INTERNATIONAL, 2021, 27 (09) : 3574 - 3589
  • [30] Prediction and Analysis on Oxidation of H13 Hot Work Steel
    Yong-an Min
    Xiao-chun Wu
    Rong Wang
    Lin Li
    Luo-ping Xu
    [J]. Journal of Iron and Steel Research International, 2006, 13 : 44 - 49