Anodic Corrosion Behavior of NiFe2O4-Based Cermet in Na3AlF6-K3AlF6-AlF3 for Aluminum Electrolysis

被引:15
|
作者
Tian, Zhongliang [1 ]
Lai, Yanqing [1 ]
Yang, Shu [1 ]
Li, Jie [1 ]
Hwang, Jiann-Yang [2 ]
Liu, Yexiang [1 ]
机构
[1] Cent S Univ, Sch Met & Environm, Changsha 410083, Hunan, Peoples R China
[2] Michigan Technol Univ, Dept Mat Sci & Engn, Houghton, MI 49931 USA
关键词
INERT ANODES; NICKEL FERRITE; LOWER TEMPERATURE; SYSTEM; PERFORMANCE; SOLUBILITY;
D O I
10.1007/s11663-015-0328-8
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A (Cu,Ni)/(10NiO-NiFe2O4) cermet was tested as an inert anode for aluminum electrolysis in Na3AlF6-K3AlF6-AlF3 melt at 1173 K (900 A degrees C), and its corrosion behavior was studied. The results show that the low-temperature Na3AlF6-K3AlF6-AlF3 bath is beneficial, improving the service conditions. With the combined effects of the electrolyte composition and the nascent oxygen during electrolysis, the metal phase (Cu,Ni) at the surface of anode will not be leached preferentially, but be transferred into the aluminates including FeAl2O4, NiAl2O4 and CuAl2O4. This is helpful for the anode to improve its corrosion resistance.
引用
收藏
页码:1257 / 1261
页数:5
相关论文
共 50 条
  • [41] PHASE-EQUILIBRIA IN THE SYSTEM CAF2-ALF3-NA3ALF6 AND PART OF THE SYSTEM CAF2-ALF3-NA3ALF6-AL2O3
    CRAIG, DF
    BROWN, JJ
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1980, 63 (5-6) : 254 - 261
  • [42] Effect of LiF on liquidus temperature and solubility of Al2O3 in Na3AlF6-K3AlF6- AlF3 melts
    Huang, You-Guo
    Tian, Zhong-Liang
    Lai, Yan-Qing
    Li, Jie
    Liu, Ye-Xiang
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2010, 20 (05): : 903 - 907
  • [43] Na3AlF6-K3AlF6-AlF3熔盐体系的物理化学性质研究进展
    吕晓军
    陈世月
    田忠良
    赖延清
    李劼
    轻金属, 2013, (08) : 29 - 32
  • [44] Study on the corrosion behavior of alumina coating on the surface of aluminum electrolysis anode steel claw in Na3AlF6-AlF3 molten salt
    Zhang, Fengqi
    Shao, Yilin
    Dong, Hongrui
    Mao, Pengyan
    Zhang, Wu
    Tao, Shaohu
    MATERIALS TODAY COMMUNICATIONS, 2025, 44
  • [45] K3AlF6-Na3AlF6-AlF3铝电解体系密度的研究
    阚素荣
    孟庆勇
    袁敏娟
    卢世刚
    丁海洋
    张向军
    稀有金属, 2011, 35 (03) : 469 - 474
  • [46] ELECTROLYSIS EXPANSION PERFORMANCE OF MODIFIED PITCH BASED TiB2-C COMPOSITE CATHODE IN [K3AlF6/Na3AlF6]-AlF3-Al2O3 MELTS
    Fang Zhao
    Xu Jian
    Hou Jin-long
    LoLin-bo
    Zhu Jun
    LIGHT METALS 2012, 2012, : 1361 - 1365
  • [47] Liquidus temperature of electrolyte Na3AlF6-K3AlF6-AlF3-LiF-CaF2-MgF2-Al2O3 molten melts
    Fang Z.
    Dang Y.-Y.
    Xin P.-F.
    Tian Z.-L.
    Zhou L.
    Zhang W.-G.
    Shen B.
    Zhang Z.-Y.
    Zhao J.-X.
    Lai Y.-Q.
    Lai, Yan-Qing (laiyanqing@csu.edu.cn), 1928, Central South University of Technology (28): : 1928 - 1936
  • [48] REINVESTIGATION OF SYSTEM NA3ALF6-LI3ALF6
    GARTON, G
    WANKLYN, BM
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1967, 50 (08) : 395 - &
  • [49] ENTHALPY OF FUSION OF ALF3 AND ENTHALPIES OF MIXING OF ALF3 WITH LI3ALF6 AND NA3ALF6
    HONG, KC
    KLEPPA, OJ
    HIGH TEMPERATURE SCIENCE, 1976, 8 (04): : 299 - 307
  • [50] Electrical conductivity of (Na3AlF6-40 wt%K3AlF6) AlF3 wt% melts
    Huang Youguo
    Lai Yanqing
    Tian Zhonghang
    Li Jie
    Liu Yexiang
    Yi Qingyu
    LIGHT METALS 2008, 2008, : 519 - +