Initial microstructure effect on the mechanical properties of Ti-6Al-4V ELI alloy processed by high-pressure torsion

被引:8
|
作者
Cvijovic-Alagic, I. [1 ]
Cvijovic, Z. [2 ]
Maletaskic, J. [1 ]
Rakin, M. [2 ]
机构
[1] Univ Belgrade, Inst Nucl Sci Vinca, Mike Petrovica Alasa 12-14, Belgrade 11001, Serbia
[2] Univ Belgrade, Fac Technol & Met, Karnegijeva 4, Belgrade 11120, Serbia
关键词
Ti-based alloy; High-pressure torsion; Microstructure; Mechanical properties; Fracture; BIOMEDICAL APPLICATIONS; TITANIUM-ALLOYS; SUBMICROCRYSTALLINE STRUCTURE; TEXTURE EVOLUTION; FATIGUE BEHAVIOR; TI-6A1-4V ALLOY; AL-ALLOY; DEFORMATION; STRAIN; REDUCTION;
D O I
10.1016/j.msea.2018.08.094
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
effect of initial microstructure on the mechanical properties and fracture mode of the Ti-6Al-4V ELI alloy subjected to the high-pressure torsion (HPT) processing at room temperature and 500 degrees C was investigated. In this purpose, the four different microstructures (fully lamellar, martensitic, equiaxed and globular microstructures) were developed by the proper heat treatments. The results showed that the application of the HPT processing provided substantial microstructural refinement, independent on the alloy initial microstructure. As a consequence, the alloy hardness, tensile strength and ductility significantly increased. At the same time, the elastic modulus of the HPT-processed alloy is almost 2 times lower as compared to that of the alloy in the initial heat treated state. The obtained improvements strongly depend on the alloy initial microstructure and HPT processing temperature. It was found that the initial martensitic microstructure is beneficial to improve the hardness, tensile and fracture properties. The HPT processing at 500 degrees C enhanced them more effectively. After the warm HPT processing, alloy with the initial martensitic microstructure exhibited exceptional hardness (455 MPa), high ultimate tensile strength (1546 MPa), high elongation to failure (18.8%) and low elastic modulus (78.6 GPa). Although the alloy with initial fully lamellar microstructure displayed the lowest elastic modulus (68 GPa), the ultrafine and homogeneous (alpha + beta) two-phase microstructure produced by the HPT processing of the alloy with initial martensitic microstructure offered the best combination of the strength-ductility balance and strength-to-elastic modulus ratio (19.8 x 10(-3)). The complex fracture process, involving transgranular quasi-cleavage and ductile dimple fracture mode, corresponded to the changes in ductility.
引用
收藏
页码:175 / 192
页数:18
相关论文
共 50 条
  • [31] Microstructure and properties of the oxynitrided Ti-6Al-4V alloy
    Moskalewicz, T.
    Zimowski, S.
    Kitano, Y.
    Wierzchon, T.
    Czyrska-Filemonowicz, A.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2006, 44 (03): : 133 - 138
  • [32] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z.X.
    Qu, S.J.
    Feng, A.H.
    Shen, J.
    Chen, D.L.
    Journal of Alloys and Compounds, 2017, 718 : 170 - 181
  • [33] Hot deformation behavior of Ti-6Al-4V alloy: Effect of initial microstructure
    Zhang, Z. X.
    Qu, S. J.
    Feng, A. H.
    Shen, J.
    Chen, D. L.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 718 : 170 - 181
  • [34] Effect of Initial Microstructure on High-Temperature Dynamic Deformation of Ti-6Al-4V Alloy
    Gangireddy, Sindhura
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (10): : 4581 - 4594
  • [35] EFFECT OF CARBON CONTENT ON THE MICROSTRUCTURE AND PROPERTIES OF Ti-6Al-4V ALLOY
    Szkliniarz, A.
    Szkliniarz, W.
    ARCHIVES OF METALLURGY AND MATERIALS, 2020, 65 (03) : 1197 - 1204
  • [36] Microstructure of Ti-6Al-4V alloy
    Kim, Tae Wan
    Yoon, Yo Han
    Oh, Ho Ra
    Park, Jong Bum
    Lee, Jung-Il
    Ryu, Jeong Ho
    JOURNAL OF THE KOREAN CRYSTAL GROWTH AND CRYSTAL TECHNOLOGY, 2016, 26 (03): : 126 - 130
  • [37] An investigation of the effect of fatigue deformation on the residual mechanical properties of Ti-6Al-4V ELI
    Akahori, T
    Niinomi, M
    Fukunaga, KI
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (08): : 1937 - 1948
  • [38] An investigation of the effect of fatigue deformation on the residual mechanical properties of Ti-6Al-4V ELI
    Toshikazu Akahori
    Mitsuo Niinomi
    Kei-Ichi Fukunaga
    Metallurgical and Materials Transactions A, 2000, 31 : 1937 - 1948
  • [39] MECHANICAL-PROPERTIES OF CAST TI-6AL-4V ALLOY WITH IMPROVED MICROSTRUCTURE
    IBARAKI, Y
    SASAKI, T
    HONMA, H
    JOURNAL OF THE JAPAN INSTITUTE OF METALS, 1980, 44 (03) : 311 - 316
  • [40] Microstructure and mechanical properties of laser rapid formed Ti-6Al-4V alloy
    Chen Jing
    Xue Lei
    Yang Haiou
    Tan Hua
    Huang Weidong