Failure of stainless steel furnace parts has been observed following treatment of gallium-containing plutonium compounds at 800 degreesC to 1200 degreesC. Our previous work examined the corrosive effects of gallium suboxide (Ga2O) gas on 316 L SS in an effort to elucidate a failure mechanism. Elemental segregation, oxidation, and Ga uptake were found to occur following exposure. Qualitative mechanical tests using four-point bend specimens suggested that stainless steel was severely embrittled following exposure to Ga2O at 1150 degreesC. The objective of this work is to quantitatively detail the effects of Ga2O on crack initiation and propagation in 316 L SS using fracture mechanics specimens. Samples were exposed to Ga2O gas and tested in laboratory air. Results indicate that increasing Ga uptake is detrimental to the crack initiation and propagation resistance of 316 L SS. Increasing Ga absorption decreased the threshold stress intensity required for crack initiation. Increasing Ga uptake also promoted unstable crack propagation and intergranular fracture. A combination of micro X-ray fluorescence and SEM suggests that compound formation and intrinsic Ga embrittlement result in increased cracking susceptibility. Ga embrittlement was shown to parallel hydrogen embrittlement, with reduction of a monovalent oxide resulting in specimen corrosion, uptake, and intrinsic and extrinsic embrittlement, depending on concentration. The combination of results from specimens Ga loaded by exposure to Ga liquid and to Ga2O gas suggest that the corrosion reaction is detrimental to fracture resistance. That is, for the same Ga concentration, specimens exposed to liquid metal Ga were more failure resistant than those exposed to Ga2O gas.
引用
收藏
页码:635 / 648
页数:14
相关论文
共 50 条
  • [31] Stress corrosion cracking on irradiated 316 stainless steel
    Furutani, G
    Nakajima, N
    Konishi, T
    Kodama, M
    JOURNAL OF NUCLEAR MATERIALS, 2001, 288 (2-3) : 179 - 186
  • [32] Corrosion fatigue cracking of AISI 316L stainless steel screen mesh
    Kaewkumsai, S.
    Khonraeng, W.
    Chainpairote, A.
    ENGINEERING FAILURE ANALYSIS, 2010, 17 (04) : 857 - 863
  • [33] Cracking analysis of 316L stainless steel lining plates in alkaline environments
    You, Yiliang
    Zhang, Zheng
    Ma, Luoning
    ENGINEERING FAILURE ANALYSIS, 2014, 39 : 34 - 40
  • [34] Cracking Mechanism of Laser Cladding Rapid Manufacturing 316L Stainless Steel
    Song Jian-li
    Li Yong-tang
    Deng Qi-lin
    Cheng, Z. -Y.
    Chin, Bryan
    ADVANCED DESIGN AND MANUFACTURE II, 2010, 419-420 : 413 - +
  • [35] Strain incompatibilities and their role in intergranular cracking of irradiated 316L stainless steel
    West, E. A.
    Was, G. S.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 441 (1-3) : 623 - 632
  • [36] Nanometre to micrometre length-scale techniques for characterising environmentally-assisted cracking: An appraisal
    Clark, Ronald N.
    Burrows, Robert
    Patel, Rajesh
    Moore, Stacy
    Hallam, Keith R.
    Flewitt, Peter E. J.
    HELIYON, 2020, 6 (03)
  • [37] Effects of surface treatments on environmentally-assisted cracking susceptibility of Alloy 182 in BWR environment
    Que, Z.
    Volpe, L.
    Toivonen, A.
    Burke, M.G.
    Scenini, F.
    Ehrnstén, U.
    Corrosion Science, 2021, 188
  • [38] RESULTS FROM ENVIRONMENTALLY-ASSISTED SHORT CRACK FATIGUE TESTING ON AUSTENITIC STAINLESS STEELS
    Coult, Ben
    Griffiths, Adam
    Beswick, Jack
    Gill, Peter
    Platts, Norman
    Smith, Jean
    Stevens, Gary
    PROCEEDINGS OF THE ASME 2020 PRESSURE VESSELS & PIPING CONFERENCE (PVP2020), VOL 1, 2020,
  • [39] ENVIRONMENTALLY-ASSISTED FATIGUE BEHAVIOR OF 316 STAINLESS STEELS IN SIMULATED PWR PRIMARY ENVIRONMENT: STRAIN HOLDING, ZN-ADDITION, AND THEIR COMBINED EFFECT
    Lee, Hyeon Bae
    Kim, Ho-Sub
    Chen, Junjie
    Jang, Changheui
    Kim, Tae Soon
    Stevens, Gary L.
    Ahluwalia, Kawaljit
    PROCEEDINGS OF THE ASME PRESSURE VESSELS AND PIPING CONFERENCE, 2019, VOL 1, 2019,
  • [40] Environmentally-assisted microstructural integrity of commercial cold drawn pearlitic steel wires
    Toribio, Jesus
    Ayaso, Francisco-Javier
    Fernandez-Vina, Antonio
    4TH INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY (ICSI 2021), 2022, 37 : 1001 - 1006