Electromagnetic Interference Shielding Properties of SiC Ceramic Matrix Composite Reinforced by Three-dimensional Silicon Carbide Nanowire Network

被引:2
|
作者
Ruan Jing [1 ,2 ,3 ]
Yang Jinshan [1 ,2 ]
Yan Jingyi [1 ,2 ,4 ]
You Xiao [1 ,2 ,4 ]
Wang Mengmeng [1 ,2 ,4 ]
Hu Jianbao [1 ,2 ]
Zhang Xiangyu [1 ,2 ]
Ding Yusheng [1 ,2 ]
Dong Shaoming [1 ,2 ,5 ]
机构
[1] Chinese Acad Sci, Shanghai Inst Ceram, State Key Lab High Performance Ceram & Superfine, Shanghai 200050, Peoples R China
[2] Chinese Acad Sci, Struct Ceram & Composites Engn Res Ctr, Shanghai Inst Ceram, Shanghai 201899, Peoples R China
[3] ShanghaiTech Univ, Sch Phys Sci & Technol, Shanghai 201210, Peoples R China
[4] Univ Chinese Acad Sci, Beijing 100039, Peoples R China
[5] Univ Chinese Acad Sci, Ctr Mat Sci & Optoelect Engn, Beijing 100049, Peoples R China
基金
中国国家自然科学基金;
关键词
SiC nanowire; electromagnetic interference shielding; ceramic matrix composite; PyC deposition; SiC matrix; MICROWAVE ABSORBING PROPERTIES; ABSORPTION PROPERTIES; DIELECTRIC-PROPERTIES; LIGHTWEIGHT; NANOSHEETS; FOAM;
D O I
10.15541/jim20210224
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon carbide nanowires (SiCNWs) possess excellent electromagnetic absorption performance and a three-dimensional (3D) network structure is beneficial to the multiple reflection and absorption of electromagnetic waves (EMWs). The 3D staggered SiCNWs network preforms with a volume fraction of 20% was realized by vacuum filtration method. And then the PyC interphase and SiC matrix were prepared through chemical vapor infiltration (CVI) process, and the densified SiCNWs/SiC ceramic matrix composites were obtained through CVI and precursor impregnation pyrolysis (PIP) process. Methane (CH4) and trichloromethylsilane (MTS) were selected as gaseous precursor of the PyC and SiC, respectively. With increase of deposited PyC from 0 to 29.5%, the electromagnetic interference (EMI) shielding efficiency (SE) of the porous SiCNWs increases from 9.2 dB to 64.1 dB in 8-12 GHz (X-band). The densified SiCNWs/SiC ceramic matrix composites with a mass gain of about 13% of PyC interphase present an average EMI SE of 37.8 dB in X-band. The achieved EMI shielding properties suggested that the potential application of the SiCNWs/SiC ceramic matrix composites may be a promising new-generation EMI shielding material.
引用
收藏
页码:579 / 584
页数:6
相关论文
共 34 条
  • [31] Research and Development of Continuous SiC Fibers and SiCf/SiC Composities
    Yuan Qin
    Song Yong-Cai
    [J]. JOURNAL OF INORGANIC MATERIALS, 2016, 31 (11) : 1157 - 1165
  • [32] Porous carbon/graphite nanosheet/ferromagnetic nanoparticle composite absorbents with adjustable electromagnetic properties
    Zhang, Chongyang
    Liu, Zhi
    Xu, Pan
    Zhang, Ying
    Yue, Xigui
    [J]. NANOTECHNOLOGY, 2021, 32 (20)
  • [33] Morphology-control synthesis of polyaniline decorative porous carbon with remarkable electromagnetic wave absorption capabilities
    Zhang, Feng
    Cui, Wei
    Wang, Bingbing
    Xu, Binghui
    Liu, Xiaohan
    Liu, Xuehua
    Jia, Zirui
    Wu, Guanglei
    [J]. COMPOSITES PART B-ENGINEERING, 2021, 204
  • [34] Simple approach to β-SiC nanowires:: Synthesis, optical, and electrical properties
    Zhou, Weimin
    Liu, Xuan
    Zhang, Yafei
    [J]. APPLIED PHYSICS LETTERS, 2006, 89 (22)