Fracture toughness of SiC, Si3N4, and sialon ceramics using controlled surface flaws

被引:3
|
作者
Cook, SG [1 ]
King, JE [1 ]
Little, JA [1 ]
机构
[1] UNIV CAMBRIDGE,DEPT MAT SCI & MET,CAMBRIDGE CB2 1TN,ENGLAND
关键词
D O I
10.1179/mst.1996.12.4.366
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Knoop and Vickers indentation cracks have frequently been used as model 'precracks' in ceramic bend specimens for fracture toughness (K-1c) determination. Indentation residual stress reduces the measured K-1c but can be removed or accounted for by grinding, annealing, or modelling. Values of K-1c are obtained for four materials using Vickers indentations and an improved stress intensity factor. Methods for residual stress removal or incorporation are compared, and the most reliable stress removal alternative is identified for each material. (C) 1996 The Institute of Materials.
引用
收藏
页码:366 / 370
页数:5
相关论文
共 50 条
  • [31] Estimation of thermal shock fracture toughness of Si3N4
    Awaji, Hideo
    Takahashi, Toshifumi
    Yamamoto, Naoto
    Honda, Sawao
    Hirosaki, Naoto
    Nippon Seramikkusu Kyokai Gakujutsu Ronbunshi/Journal of the Ceramic Society of Japan, 1998, 106 (1237): : 877 - 882
  • [32] Estimation of thermal shock fracture toughness of Si3N4
    Awaji, H
    Takahashi, T
    Yamamoto, N
    Honda, S
    Hirosaki, N
    JOURNAL OF THE CERAMIC SOCIETY OF JAPAN, 1998, 106 (09) : 877 - 882
  • [33] Room-temperature strength and fracture toughness of β-sialon (z=1)-SiC composite fabricated from aluminum-iso-propoxide, α-Si3N4 and β-SiC
    Kyushu Natl Industrial Research Inst, Saga, Japan
    J Ceram Soc Jpn, 1212 (770-773):
  • [34] Comparison in microstructure and mechanical properties of porous Si3N4 ceramics with SiC and Si3N4 coatings
    Li, Xiangming
    Yin, Xiaowei
    Zhang, Litong
    Pan, Tianhao
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 527 (1-2): : 103 - 109
  • [35] FLEXURAL CREEP OF SELECTED SI3N4 AND SIC CERAMICS
    LARSEN, DC
    WALTHER, GC
    BORTZ, SA
    RUH, R
    AMERICAN CERAMIC SOCIETY BULLETIN, 1979, 58 (03): : 350 - 350
  • [36] Correlation between microstructure and toughness of hot pressed Si3N4 ceramics seeded with β-Si3N4 particles
    De Pablos, A
    Osendi, MI
    Miranzo, P
    CERAMICS INTERNATIONAL, 2003, 29 (07) : 757 - 764
  • [37] Development of α-β SiAlON ceramics from different Si3N4 starting powders
    Acikbas, Nurcan Calis
    Kara, Ferhat
    Mandal, Hasan
    SIAIONS AND NON-OXIDES, 2009, 403 : 107 - +
  • [38] The effect of Si content on the fracture toughness of CrAlN/Si3N4 coatings
    Liu, S.
    Wheeler, J. M.
    Davis, C. E.
    Clegg, W. J.
    Zeng, X. T.
    JOURNAL OF APPLIED PHYSICS, 2016, 119 (02)
  • [39] CHARACTERIZATION OF DYNAMIC FAILURE PROCESS OF Si3N4 CERAMICS, PART II: DYNAMIC FRACTURE TOUGHNESS
    Maros, Maria B.
    Kaulics, Nikoletta
    Dusza, Jan
    FRACTOGRAPHY OF GLASSES AND CERAMICS V, 2007, 199 : 435 - +
  • [40] Fracture toughness of Si3N4 based ceramics with rare-earth oxide sintering additives
    Tatarko, Peter
    Lojanova, Stefania
    Dusza, Jan
    Sajgalik, Pavol
    FRACTOGRAPHY OF ADVANCED CERAMICS III, 2009, 409 : 377 - +