In vitro durability of one-bottle resin adhesives bonded to dentin

被引:42
|
作者
Hashimoto, Masanori [1 ]
Fujita, Shinichi [1 ]
Kaga, Masayuki [1 ]
Yawaka, Yasutaka [1 ]
机构
[1] Hokkaido Univ, Grad Sch Dent Med, Dept Dent Children & Disabled Persons, Sapporo, Hokkaido, Japan
关键词
one-bottle resin adhesive; degradation; hydrolysis;
D O I
10.4012/dmj.26.677
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Recently, one-bottle resins adhesives have been developed to reduce the number of clinical steps of resin application. They are now widely used in clinical dental practice. However, little is known regarding the detailed mechanism of bond degradation. Therefore, this study evaluated the durability of one-bottle resin adhesives using long-term water storage testing. Resin-dentin bonded specimens were prepared using five commercially available one-bottle resin adhesives. The specimens were sectioned perpendicular to the adhesive interface to produce beams and stored in distilled water for 24 hours (control), 100, 200, and 300 days. After the water storage, each beam was subjected to a microtensile bond test and then SEM fractography was performed on the fractured surface. Compared to the bond strength at 24 hours after bonding (control), the bond strength of all tested adhesives were significantly decreased after 100 or more days in water. SEM fractography revealed a typical type of deterioration in the adhesive-composite interface that might cause a decline in bond strength after aging.
引用
收藏
页码:677 / 686
页数:10
相关论文
共 50 条
  • [21] Microtensile bond strength of thermally stressed composite-dentin bonds mediated by one-bottle adhesives
    Xie, BS
    Dickens, SH
    Giuseppetti, AA
    [J]. AMERICAN JOURNAL OF DENTISTRY, 2002, 15 (03): : 177 - 184
  • [22] One-year bonding performance of one-bottle etch-and-rinse adhesives to dentin at different moisture conditions
    Bossardi, Mayara
    Piva, Evandro
    Isolan, Cristina Pereira
    Munchow, Eliseu Aldrighi
    [J]. JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2020, 34 (06) : 686 - 694
  • [23] In vitro analysis of the antibacterial activity of twelve one-bottle adhesives on streptococcus mutans.
    Sander, HH
    Pimenta, FJGS
    Neves, AD
    Discacciati, JAC
    Souza, MCFMC
    Santos, VR
    [J]. JOURNAL OF DENTAL RESEARCH, 2003, 82 : 206 - 206
  • [24] NaOCl degradation of one-step one-bottle self-etch adhesives bonded to bovine dentine
    Yildirim, Tahsin
    Ayar, Muhammet Kerim
    Yesilyurt, Cemal
    [J]. JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 2016, 30 (02) : 210 - 217
  • [25] NaOCl degradation of one-step one-bottle self-etch adhesives bonded to bovine dentine
    [J]. Ayar, Muhammet Kerim (kerimayar@ktu.edu.tr), 1600, Taylor and Francis Ltd. (30):
  • [26] An FE-SEM evaluation of resin dentin interface with four one-bottle adhesive systems.
    Mori, G
    Bassi, MA
    Goracci, G
    [J]. JOURNAL OF DENTAL RESEARCH, 1998, 77 : 680 - 680
  • [27] Dentin permeability:: Self-etching and one-bottle dentin bonding systems
    Grégoire, G
    Joniot, S
    Guignes, P
    Millas, A
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 2003, 90 (01): : 42 - 49
  • [28] Shear bond strengths of one-bottle dentin adhesive systems
    Bae, JH
    Son, HH
    Heo, SJ
    Cho, BH
    [J]. JOURNAL OF DENTAL RESEARCH, 2000, 79 : 374 - 374
  • [29] Effects of repeated use on bond strengths of one-bottle adhesives
    Perdigao, J
    Swift, EJ
    Lopes, GC
    [J]. QUINTESSENCE INTERNATIONAL, 1999, 30 (12): : 819 - 823
  • [30] Shear bond strengths of saliva contaminated 'one-bottle' adhesives
    Taskonak, B
    Sertgöz, A
    [J]. JOURNAL OF ORAL REHABILITATION, 2002, 29 (06) : 559 - 564