Effect of processing on Density of Mg-6Zn-0.5Y Alloy

被引:0
|
作者
Jia Zheng [1 ]
Zhang Zhi-Qiang [1 ]
Le Qi-Chi [1 ]
Cui Jian-Zhong [1 ]
机构
[1] Northeastern Univ, Key Lab Electromagnet Proc Mat, Minist Educ, Shenyang 110004, Liaoning, Peoples R China
来源
关键词
Mg-6Zn-0.5Y alloy; hydrogen content; density; C2Cl6; degasser; ZN-AL ALLOYS; MG;
D O I
10.4028/www.scientific.net/MSF.686.57
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Effect of different melt temperatures, holding time, cooling rate and C2Cl6 degasser treatment on the density of Mg-6Zn-0.5Y alloy was studied. The experimental results indicated that the density of RPT samples decreased with increasing of melt temperature, which indicating that the hydrogen content increased with the increment of temperature. And the results also showed that the density of RPT samples rapidly decreased at first and then decreased slowly with increasing of holding time, suggesting that the hydrogen content rapidly increased at first and then reached a saturated state with increasing of holding time. When cooling rate increased, the density of ingots gradually increased at the same melt temperature. When the melt was treated by 1%, 3% and 5% C2Cl6 degasser at 720 degrees C, the density of ingots gradually increased compared with the ingot without treatment by C2Cl6 degasser. The density of ingot reached the maximum value when C2Cl6 degasser content was 3%, i.e, the ingot density value increased from 1.8649g.cm(-3) of the untreated sample to 1.8774g.cm(-3) of the sample treated by 3% C2Cl6 degasser, indicating that 3% C2Cl6 degasser treatment has an optimum degassing effect.
引用
收藏
页码:57 / 62
页数:6
相关论文
共 50 条
  • [31] Effect of Trace Y on Microstructure and Properties of Mg-5Al-0.8Zn-0.5Mn Magnesium Alloy
    Zhang Jianxin
    Gao Aihua
    Guo Xuefeng
    RARE METAL MATERIALS AND ENGINEERING, 2012, 41 : 459 - 462
  • [32] Effect of Zn addition on microstructure and mechanical properties of Mg-3Y-2Nd-0.5Zr alloy
    Feiyu He
    Wenxin Hu
    Lijuan Liu
    Shaobo Ma
    Wei He
    China Foundry, 2023, 20 (04) : 299 - 306
  • [33] Effect of Zn addition on microstructure and mechanical properties of Mg-3Y-2Nd-0.5Zr alloy
    Fei-yu He
    Wen-xin Hu
    Li-juan Liu
    Shao-bo Ma
    Wei He
    China Foundry, 2023, 20 : 299 - 306
  • [34] Effect of Heat Treatment on Corrosion and Mechanical Properties of Mg-10Y-1.5Zn-0.5Zr Alloy
    Mingming Liu
    Quanan Li
    Xiaoya Chen
    Xiangyu Li
    Peijun Chen
    Jinfeng Tan
    Journal of Materials Engineering and Performance, 2023, 32 : 1463 - 1473
  • [35] Effect of annealing on microstructure and tensile properties of as-extruded Mg-5Gd-4Y-0.5Zn-0.5Zr alloy
    Wu, Xuan
    Wang, Yong
    Chen, Yi
    Qiao, Liying
    She, Jia
    Journal of Materials Research and Technology, 2022, 21 : 929 - 942
  • [36] Effect of annealing on microstructure and tensile properties of as-extruded Mg-5Gd-4Y-0.5Zn-0.5Zr alloy
    Wu, Xuan
    Wang, Yong
    Chen, Yi
    Qiao, Liying
    She, Jia
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2022, 21 : 929 - 942
  • [37] Effect of Zn addition on microstructure and mechanical properties of Mg-9Gd-3Y-0.5Zr alloy
    Cui, Wendong
    Xiao, Lv
    Liu, Wencai
    Wu, Guohua
    Wang, Xianfei
    Li, Zhongquan
    JOURNAL OF MATERIALS RESEARCH, 2018, 33 (06) : 733 - 744
  • [38] Effect of erbium on microstructure and thermal compressing flow behavior of Mg-6Zn-0.5Zr alloy
    王忠军
    张彩碚
    邵晓宏
    崔建忠
    乐启炽
    TransactionsofNonferrousMetalsSocietyofChina, 2006, (S3) : 1774 - 1778
  • [39] Effect of Al on the microstructure and mechanical properties of Mg-6Zn-2Sn-0.5Mn alloy
    Wang, Cong
    Cui, Jie
    Luo, Tianjiao
    Liu, Yunteng
    Wang, Changzheng
    Hao, Xuehui
    Yang, Yuansheng
    MATERIALS SCIENCE AND TECHNOLOGY, 2019, 35 (12) : 1464 - 1470
  • [40] Effect of erbium on microstructure and thermal compressing flow behavior of Mg-6Zn-0.5Zr alloy
    Wang Zhong-jun
    Zhang Cai-bei
    Shao Xiao-hong
    Cui Jian-zhong
    Le Qi-chi
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1774 - S1778