Investigation on the thermal decomposition of the elastomer containing fluoroolefin segment by DSC-TG-MS-FTIR

被引:6
|
作者
Tang, Weiqiang [1 ]
Zeng, Tao [2 ]
Hu, Jinghui [2 ]
Li, Jianmin [2 ]
Yang, Rongjie [1 ,2 ]
机构
[1] Beijing Inst Technol, State Key Lab Explos Sci & Technol, Beijing 100081, Peoples R China
[2] Beijing Inst Technol, Natl Engn Res Ctr Flame Retardant Mat, Sch Mat Sci & Engn, Beijing, Peoples R China
关键词
HF; propellant; recross-linked fluoroelastomer; thermal decomposition; COMBUSTION CHARACTERISTICS; POLY(VINYLIDENE FLUORIDE); POLYVINYLIDENE FLUORIDE; DEGRADATION MECHANISMS; COMPATIBILITY; ACID;
D O I
10.1002/pat.5480
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Based on the cross-linking reaction of bisphenol A epoxy resin and liquid carboxy-terminated poly(tetrafluoroethylene-hexafluoropropylene-vinylidene fluoride) copolymer (CTTHV), the elastomer containing fluoroolefin segment was prepared. The bis(2,2-dinitropropyl)-acetal/formal (BDNPA/F) was used as an energetic plasticizer for this fluoroolefin segment-containing elastomer (FO elastomer). The compatibility of CTTHV and BDNPA/F was evaluated by the combination of differential scanning calorimetry (DSC) and derivative thermogravimetry (DTG) methods. Thermal decomposition of the FO elastomers was investigated by TG-DSC. The kinetic parameters of the FO elastomers were calculated by Kissinger-Akahira-Sunose method. DSC-TG-MS-Fourier transform infrared spectroscopy analysis was used to detect the thermal decomposition products. The thermal decomposition mechanisms of the FO and FO/BDNPA/F elastomers were discussed. The results show that CTTHV has a good compatibility with BDNPA/F, and the prepared FO/BDNPA/F elastomers have good thermal stability. BDNPA/F can promote the thermal decomposition of the FO elastomer and bring more heat for the binder system according to the thermal decomposition behaviors and kinetic calculation results of FO/BDNPA/F elastomers. The FO elastomer preferentially undergoes depolymerization, HF elimination with the formation of polyene sequences, and subsequent main-chain cleavage, polyaromatization. The H ion fragments of the decomposition of BDNPA/F can be an important factor in the improvement of HF concentration at the initial thermal decomposition of FO elastomer. An abundant HF released during all decomposition of FO/BDNPA/F elastomers may be beneficial to the ignition and combustion of aluminum particles in future applications.
引用
收藏
页码:4880 / 4890
页数:11
相关论文
共 50 条
  • [31] Research on the catalytic thermal decomposition of RDX-CMDB propellants by TG-DSC-IR-MS
    Xi'an Modern Chemistry Research Institute, Xi'an 710065, China
    Guti Houjian Jishu, 2009, 5 (539-542+553):
  • [32] Thermal decomposition of two synthetic glycosides by TG, DSC and simultaneous Py-GC-MS analysis
    W.-C. Xie
    X.-H. Gu
    Z.-C. Tan
    J. Tang
    G.-Y. Wang
    C.-R. Luo
    L.-X. Sun
    Journal of Thermal Analysis and Calorimetry, 2007, 87 : 505 - 510
  • [33] Thermal decomposition of two synthetic glycosides by TG, DSC and simultaneous Py-GC-MS analysis
    Xie, W-C.
    Tan, Z-C.
    Gu, X-H.
    Tang, J.
    Wang, G-Y.
    Luo, C-R.
    Sun, L-X.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2007, 87 (02) : 505 - 510
  • [34] Research on thermal decomposition of trinitrophloroglucinol salts by DSC, TG and DVST
    Liu, Rui
    Zhang, Tonglai
    Yang, Li
    Zhou, Zunning
    Hu, Xiaochun
    CENTRAL EUROPEAN JOURNAL OF CHEMISTRY, 2013, 11 (05): : 774 - 781
  • [35] TG AND DSC KINETICS OF THERMAL-DECOMPOSITION AND CRYSTALLIZATION PROCESSES
    PERRENOT, B
    WIDMANN, G
    JOURNAL OF THERMAL ANALYSIS, 1991, 37 (08): : 1785 - 1792
  • [36] Thermal analysis in oxidative and pyrolysis conditions of alkaline earth metals picolinates using the techniques: TG-DSC, DSC, MWTA, HSM and EGA (TG-DSC-FTIR and HSM-MS)
    Nascimento, A. L. C. S.
    Parkes, G. M. B.
    Ashton, G. P.
    Fernandes, R. P.
    Teixeira, J. A.
    Nunes, W. D. G.
    Ionashiro, M.
    Caires, F. J.
    JOURNAL OF ANALYTICAL AND APPLIED PYROLYSIS, 2018, 135 : 67 - 75
  • [37] Thermal decomposition of HNIW by TG-MS
    Dong, Lin-Mao
    Li, Xiao-Dong
    Yang, Rong-Jie
    Hanneng Cailiao/Chinese Journal of Energetic Materials, 2007, 15 (06): : 660 - 663
  • [38] Spectroscopic study and thermal behavior of trivalent lanthanides and yttrium(III) chelates of EDTA using TG-DSC, FTIR, and TG-DSC coupled to FTIR
    A. C. Gigante
    F. J. Caires
    D. J. C. Gomes
    L. S. Lima
    O. Treu-Filho
    M. Pivatto
    M. Ionashiro
    Journal of Thermal Analysis and Calorimetry, 2014, 115 : 127 - 135
  • [39] Using TG–FTIR and TG–MS to study thermal degradation of metal hypophosphites
    Weihong Wu
    Shufang Lv
    Xin Liu
    Hongqiang Qu
    Hongchao Zhang
    Jianzhong Xu
    Journal of Thermal Analysis and Calorimetry, 2014, 118 : 1569 - 1575
  • [40] Spectroscopic study and thermal behavior of trivalent lanthanides and yttrium(III) chelates of EDTA using TG-DSC, FTIR, and TG-DSC coupled to FTIR
    Gigante, A. C.
    Caires, F. J.
    Gomes, D. J. C.
    Lima, L. S.
    Treu-Filho, O.
    Pivatto, M.
    Ionashiro, M.
    JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2014, 115 (01) : 127 - 135