Microstructural evolution in adiabatic shear bands in Ta and Ta-W alloys

被引:179
|
作者
Pérez-Prado, MT
Hines, JA
Vecchio, KS [1 ]
机构
[1] Univ Calif San Diego, Mat Sci Grp, Dept Mech & Aerosp Engn, La Jolla, CA 92093 USA
[2] Ford Motor Co, Dept Mat Sci, Ford Res Lab, Dearborn, MI 48121 USA
基金
美国国家科学基金会;
关键词
adiabatic shear bands; recrystallization;
D O I
10.1016/S1359-6454(01)00215-4
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Microstructural evolution of adiabatic shear bands originated due to high strain, high strain rate deformation in Ta and Ta-W alloys has been examined. Tests were performed using a specially designed stepped specimen in a Hopkinson bar. Upon completion of the deformation, the region is cooled to below one half of the temperature achieved during adiabatic heating in less than one millisecond. Microstructural characterization of the shear bands was performed using optical microscopy as well as scanning and transmission electron microscopy. No evidence of recrystallization within the shear bands could be found. This is in contradiction with several recent reports, which claim that recrystallization may take place at these stringent time and temperature conditions. These studies, however, do not take into account the kinetics of boundary refinement processes, which are a distinctive characteristic of a recrystallized microstructure. It will be shown that the absence of recrystallization in Ta and Ta-W adiabatic shear bands can be predicted by a progressive subgrain misorientation (PriSM) recrystallization model, applied successfully in previous studies to predict the microstructure evolution in copper adiabatic shear bands. (C) 2001 Acta Materialia Inc. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2905 / 2917
页数:13
相关论文
共 50 条
  • [41] First Principles Calculations of Thermodynamic Quantities and Phase Diagrams of High Temperature BCC Ta-W and Mo-Ta Alloys
    Masuda-Jindo, K.
    Vu Van Hung
    Turchi, P. E. A.
    ADVANCED MATERIALS AND PROCESSING, 2007, 26-28 : 205 - +
  • [42] Structural, mechanical, and oxidation resistance properties of double glow plasma Ta-W alloys
    Zhang, Dongying
    Huang, Lei
    Yang, Kai
    Yuan, Juntang
    Ma, Zhimeng
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2024, 124
  • [43] First-principles study of stability and local order in substitutional Ta-W alloys
    Turchi, PEA
    Gonis, A
    Drchal, V
    Kudrnovsky, J
    PHYSICAL REVIEW B, 2001, 64 (08): : 851121 - 851128
  • [44] Ta-W合金的动态断裂方式
    张廷杰
    张德尧
    丁旭
    稀有金属材料与工程, 1998, (01) : 34 - 38
  • [45] Ta-W非晶合金膜生产
    胡初潜
    稀有金属, 1991, (03) : 237 - 237
  • [46] Electron beam welding of TC4/Ta-W alloys dissimilar metal
    Chen, Guoqing
    Zhang, Binggang
    Wu, Shuanghui
    Feng, Jicai
    Sun, Yi
    Hanjie Xuebao/Transactions of the China Welding Institution, 2011, 32 (08): : 21 - 24
  • [47] Direct measurement of isothermal flow stress of metals at elevated temperatures and high strain rates with application to Ta and Ta-W alloys
    Univ of California, San Diego, La Jolla, United States
    Acta Mater, 3 (907-919):
  • [48] STRESS AND RESISTIVITY OF TA-MO AND TA-W SPUTTERED THIN-FILMS
    OSHIO, S
    TAKEDA, M
    MATSUOKA, T
    JAPANESE JOURNAL OF APPLIED PHYSICS PART 1-REGULAR PAPERS SHORT NOTES & REVIEW PAPERS, 1994, 33 (7A): : 4086 - 4089
  • [49] Microstructural evolution and creep of Fe-Al-Ta alloys
    Prokopcakova, Petra
    Svec, Martin
    Palm, Martin
    INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2016, 107 (05) : 396 - 405
  • [50] High-temperature deformation in a Ta-W alloy
    Li, Y
    Lavernia, EJ
    Mohamed, FA
    TANTALUM, 1996, : 335 - 341