Effect of firing temperature on the interface between 3Y-TZP zirconia and porcelain

被引:0
|
作者
Seto, Munetsugu [1 ]
Ueda, Kazuhiko [1 ]
Katsuta, Yasuhiro [1 ]
Suzuki, Shohei [1 ]
Ozawa, Makoto [1 ]
Outaki, Rina [2 ]
Hiroyasu, Kazuhiko [2 ]
Watanabe, Fumihiko [1 ]
机构
[1] Nippon Dent Univ, Sch Life Dent Niigata, Dept Crown & Bridge Prosthodont, Niigata, Japan
[2] Nippon Dent Univ, Niigata Hosp, Oral Implant Care Unite, Niigata, Japan
基金
日本学术振兴会;
关键词
bending test; bonding interface; elemental analysis; porcelain; zirconia; BOND STRENGTH; VENEERING CERAMICS; SHEAR-STRENGTH; FRACTURE; RELIABILITY; MODE; IMPACT;
D O I
10.2334/josnusd.21-0431
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Purpose: The purpose of this study is to clarify the porcelain firing temperature conditions that give strongest bonding strength of porcelain to zirconia to manufacture all-ceramic fixed dental prostheses (FDPs) with excellent long-term stability. Methods: Opaque porcelain samples (8.0 x 3.0 x 1.2 mm) were placed in the center of zirconia plates (25.0 x 3.0 x 0.5 mm) and fired at temperatures of 950 degrees C. 1,050 degrees C, 1,100 degrees C, and 1,150 degrees C. Schwickerath crack initiation tests. elemental analyses, and morphological changes of the samples were compared. Results: There was no difference in the bonding strength among all the groups of porcelain fired at different temperatures. Elemental analysis of Si and O-2 at the interface between the zirconia and porcelain were observed in the 950 degrees C, 1,050 degrees C, and 1,100 degrees C groups. No silicon was found in the 1,150 degrees C group by elemental analysis, and the zirconia plate where the porcelain sample was placed had irregular shape changes. Conclusion: It is suggested that silicon is also involved in chemical bonds due to firing at high temperatures.
引用
收藏
页码:135 / 138
页数:4
相关论文
共 50 条
  • [31] Effect of crystalline phase assemblage on reliability of 3Y-TZP
    Denry, Isabelle
    Abdelaal, Maged
    Dawson, Deborah, V
    Holloway, Julie A.
    Kelly, John Robert
    JOURNAL OF PROSTHETIC DENTISTRY, 2021, 126 (02): : 238 - 247
  • [32] Analysis of the stability of 3Y-TZP zirconia abutments after thermocycling and mechanical loading
    Almeida, Paulo J.
    Silva, Cesar L.
    Alves, Jorge L.
    Silva, Filipe S.
    Martins, Ramiro C.
    Sampaio-Fernandes, Joao
    REVISTA PORTUGUESA DE ESTOMATOLOGIA MEDICINA DENTARIA E CIRURGIA MAXILOFACIAL, 2016, 57 (04): : 197 - 206
  • [33] Stability of 3Y-TZP nano zirconia powder after hydrothermal ageing treatment
    Ahmed, Shafique
    Zou, Lifong
    Yan, Haixue
    ADVANCES IN APPLIED CERAMICS, 2022, 121 (5-8) : 159 - 165
  • [34] Research on the Low Temperature Degradation Resistance of TiN/3Y-TZP
    Sun Jing
    Han Baokun
    Yang Xinghua
    Huang Chuanzhen
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 287 - +
  • [35] Effect of prestraining on cavity morphology in a superplastic 3 mol% yttria-stabilized tetragonal zirconia (3Y-TZP)
    Tekeli, S
    Davies, TJ
    SCRIPTA MATERIALIA, 1998, 39 (01) : 119 - 124
  • [36] The effect of an alumina counterface on friction reduction of CuO/3Y-TZP composite at room temperature
    Song, Jiupeng
    Valefi, Mandiar
    de Rooij, Matthijn
    Schipper, Dirk J.
    Winnubst, Louis
    WEAR, 2012, 274 : 75 - 83
  • [37] Effect of sintering temperature on aging resistance and mechanical properties of 3Y-TZP dental ceramic
    Jingchao Zhang
    Yongqi Zhao
    Yunmao Liao
    Li Jiang
    Xiaofei Yun
    Wei Li
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2012, 27 : 316 - 320
  • [38] SEM observations of porcelain Y-TZP interface
    Tholey, Michael J.
    Swain, Michael V.
    Thiel, Norbert
    DENTAL MATERIALS, 2009, 25 (07) : 857 - 862
  • [39] High temperature mechanical loss spectrum of 3Y-TZP zirconia reinforced with carbon nanotubes or silicon carbide whiskers
    Ionascu, C.
    Schaller, R.
    INTERACTION BETWEEN DEFECTS AND ANELASTIC PHENOMENA IN SOLIDS, 2008, 137 : 29 - 34
  • [40] Effect of low-temperature aging on friction and wear properties of 3Y-TZP ceramics
    Lu, Qing
    Liang, Xiao-Ping
    Wang, Guang-Hui
    Mocaxue Xuebao/Tribology, 2010, 30 (01): : 64 - 67