Effect of water exposure on the fracture toughness and flexure strength of a dental glass

被引:22
|
作者
Scherrer, SS [1 ]
Denry, IL
Wiskott, HWA
Belser, UC
机构
[1] Univ Geneva, Dept Prosthodont, Sch Dent Med, Geneva, Switzerland
[2] Ohio State Univ, Dept Restorat & Prosthet Dent, Columbus, OH 43210 USA
关键词
water exposure; fracture toughness; flexure strength; dental glass;
D O I
10.1016/S0109-5641(01)00002-1
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: The low fusing dental glass (Duceram LFC) has been advertised as presenting a superior chemical resistance and augmented strength after 16 h exposure to water or 4% acetic acid. The purpose of this study was to evaluate the effect of prolonged exposure to water on two mechanical properties (fracture toughness and flexure strength) of LFC. Methods: Disks and bars were mirror polished and annealed prior to aging in: (1) air (control), (2) water for 24 h at 80 degreesC and (3) water for 8 weeks at 80 degreesC. Fracture toughness (K-Ic) was determined by indentation fracture (IF) and indentation strength (IS) using a 19.6 N Vickers indentation load. Flexure strength values were obtained from three-point bending at 0.1 mm/min. Statistical analysis was performed using the Weibull distribution, Tukey and Bartlett tests (P < 0.05). Results: Both techniques (IS and IF) showed a significant improvement in the K of Duceram LFC after 8 weeks in water (0.88 and 1.14 MPa m(0.5)) as opposed to the 24-h values both in water and air (0.77-0.78 MPa m(0.5)). However, for flexure strength the Weibull characteristic (S-0) and the m parameter did not change significantly with water storage (S-0 = 90-100 MPa, Weibull m = 7-8). Significance: The increase in toughness of Duceram LFC after aging in water is an interesting and favorable observation for a restorative material exposed to the oral environment. Nevertheless, in comparison with other contemporary ceramics, the toughness of this LFC remains in the range of soda-lime-glass or classic feldspar porcelains. (C) 2001 Academy of Dental Materials. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:367 / 371
页数:5
相关论文
共 50 条
  • [21] Effect of light exposure on fracture toughness and flexural strength of light-cured composites
    Miyazaki, M
    Oshida, Y
    Moore, BK
    Onose, H
    DENTAL MATERIALS, 1996, 12 (5-6) : 328 - 332
  • [22] High-temperature flexure strength, fracture toughness and fatigue of zirconia/alumina composites
    Choi, SR
    Bansal, NP
    27TH INTERNATIONAL COCOA BEACH CONFERENCE ON ADVANCED CERAMICS AND COMPOSITES: A, 2003, 24 (03): : 273 - 279
  • [23] Change in flexural strength and fracture toughness of glass ionomers.
    Miyazaki, M
    Moore, BK
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 424 - 424
  • [24] Improvement of flexure strength and fracture toughness in alumina matrix composites reinforced with carbon nanotubes
    Kim, Sung Wan
    Chung, Won Sub
    Sohn, Kee-Sun
    Son, Chang-Young
    Lee, Sunghak
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 517 (1-2): : 293 - 299
  • [25] Effect of early water exposure on the strength of glass ionomer restoratives
    Wang, X. Y.
    Yap, A. U. J.
    Ngo, H. C.
    OPERATIVE DENTISTRY, 2006, 31 (05) : 584 - 589
  • [26] Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic
    Department of Prosthodontics, School of Dentistry, University of Geneva, Geneva, Switzerland
    不详
    不详
    Dent. Mater., 4 (246-255):
  • [27] Comparison of three fracture toughness testing techniques using a dental glass and a dental ceramic
    Scherrer, SS
    Denry, IL
    Wiskott, HWA
    DENTAL MATERIALS, 1998, 14 (04) : 246 - 255
  • [28] Flexure strength of resin-modified glass ionomer cements and their bond strength to dental composites
    Li, JG
    Liu, YJ
    Liu, Y
    Soremark, R
    Sundstrom, F
    ACTA ODONTOLOGICA SCANDINAVICA, 1996, 54 (01) : 55 - 58
  • [29] EFFECT OF CRYSTALLINITY ON STRENGTH AND FRACTURE-TOUGHNESS OF LITHIA-BASED GLASS-CERAMIC
    ANUSAVICE, KJ
    ZHANG, NZ
    JOURNAL OF DENTAL RESEARCH, 1995, 74 : 218 - 218
  • [30] Probabilistic strength of glass cylinders subjected to flexure: total and local probabilities of fracture
    G. Díaz
    P. Kittl
    V. H. Martínez
    R. Henríquez
    Journal of Materials Science, 2002, 37 : 1437 - 1441