Effect of water exposure on the fracture toughness and flexure strength of a dental glass

被引:22
|
作者
Scherrer, SS [1 ]
Denry, IL
Wiskott, HWA
Belser, UC
机构
[1] Univ Geneva, Dept Prosthodont, Sch Dent Med, Geneva, Switzerland
[2] Ohio State Univ, Dept Restorat & Prosthet Dent, Columbus, OH 43210 USA
关键词
water exposure; fracture toughness; flexure strength; dental glass;
D O I
10.1016/S0109-5641(01)00002-1
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objectives: The low fusing dental glass (Duceram LFC) has been advertised as presenting a superior chemical resistance and augmented strength after 16 h exposure to water or 4% acetic acid. The purpose of this study was to evaluate the effect of prolonged exposure to water on two mechanical properties (fracture toughness and flexure strength) of LFC. Methods: Disks and bars were mirror polished and annealed prior to aging in: (1) air (control), (2) water for 24 h at 80 degreesC and (3) water for 8 weeks at 80 degreesC. Fracture toughness (K-Ic) was determined by indentation fracture (IF) and indentation strength (IS) using a 19.6 N Vickers indentation load. Flexure strength values were obtained from three-point bending at 0.1 mm/min. Statistical analysis was performed using the Weibull distribution, Tukey and Bartlett tests (P < 0.05). Results: Both techniques (IS and IF) showed a significant improvement in the K of Duceram LFC after 8 weeks in water (0.88 and 1.14 MPa m(0.5)) as opposed to the 24-h values both in water and air (0.77-0.78 MPa m(0.5)). However, for flexure strength the Weibull characteristic (S-0) and the m parameter did not change significantly with water storage (S-0 = 90-100 MPa, Weibull m = 7-8). Significance: The increase in toughness of Duceram LFC after aging in water is an interesting and favorable observation for a restorative material exposed to the oral environment. Nevertheless, in comparison with other contemporary ceramics, the toughness of this LFC remains in the range of soda-lime-glass or classic feldspar porcelains. (C) 2001 Academy of Dental Materials. Published by Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:367 / 371
页数:5
相关论文
共 50 条
  • [1] The effect of different types of fiber on flexure strength and fracture toughness in SIFCON
    Ipek, Metin
    Aksu, Mecbure
    CONSTRUCTION AND BUILDING MATERIALS, 2019, 214 : 207 - 218
  • [2] Effect of nucleation temperature on toughness and flexure strength of canasite glass-ceramic.
    Anusavice, KJ
    Zhang, NZ
    JOURNAL OF DENTAL RESEARCH, 1996, 75 : 395 - 395
  • [3] Effect of Water Penetration on the Strength and Toughness of Silica Glass
    Wiederhorn, Sheldon M.
    Fett, Theo
    Rizzi, Gabriele
    Fuenfschilling, Stefan
    Hoffmann, Michael J.
    Guin, Jean-Pierre
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2011, 94 : S196 - S203
  • [4] Biaxial flexure strength and fracture toughness of flowable composites.
    Wilkerson, MD
    Thompson, JY
    Bayne, SC
    Stamatiades, PJ
    JOURNAL OF DENTAL RESEARCH, 1998, 77 : 203 - 203
  • [5] Strength and fracture toughness of zirconia dental ceramics
    Turon-Vinas, Miquel
    Anglada, Marc
    DENTAL MATERIALS, 2018, 34 (03) : 365 - 375
  • [6] Effect of moulding temperature on flexure, impact strength and interlaminar fracture toughness of CF/PEI composite
    Hou, M
    Ye, L
    Mai, YW
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1996, 15 (11) : 1117 - 1130
  • [7] Water Penetration—Its Effect on the Strength and Toughness of Silica Glass
    Sheldon M. Wiederhorn
    Theo Fett
    Gabriele Rizzi
    Michael J. Hoffmann
    Jean-Pierre Guin
    Metallurgical and Materials Transactions A, 2013, 44 : 1164 - 1174
  • [8] Fracture toughness and flexural strength of dental porcelains.
    Mitchell, C. A.
    Mansour, Y. F.
    O'Reilly, C. P.
    Geary, J. L.
    JOURNAL OF DENTAL RESEARCH, 2003, 82 : B121 - B121
  • [9] Fracture toughness and flexural strength of dental porcelains.
    Mitchell, CA
    Mansour, YF
    O'Reilly, CP
    Geary, JL
    JOURNAL OF DENTAL RESEARCH, 2002, 81 : A166 - A166
  • [10] Flexural strength and fracture toughness of dental core ceramics
    Yilmaz, Handan
    Aydin, Cemall
    Gul, Basak E.
    JOURNAL OF PROSTHETIC DENTISTRY, 2007, 98 (02): : 120 - 128