共 50 条
- [46] EFFECT OF CE ADDITIONS ON THE MICROSTRUCTURE AND HIGH-TEMPERATURE CORROSION BEHAVIOR OF FE-30CR-5AL ALLOYS TRANSACTIONS OF THE JAPAN INSTITUTE OF METALS, 1986, 27 (09): : 680 - 692
- [48] INFLUENCE OF THERMAL-DEGRADATION ON THE DEFORMATION-BEHAVIOR OF RAPIDLY SOLIDIFIED AL-FE-CE ALLOYS SCRIPTA METALLURGICA ET MATERIALIA, 1991, 25 (11): : 2571 - 2576
- [49] Fe-Al-Si-X ALLOYS FOR HIGH TEMPERATURE APPLICATIONS METAL 2011: 20TH ANNIVERSARY INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2011, : 957 - 961
- [50] Mechanical properties of rapidly solidified Al-Ti-Fe, Al-Cu-Fe and Al-Fe-Cu-Ti based alloys extruded from their atomized powders Materials Science and Engineering A, 1997, A232 (1-2): : 177 - 182