CVD diamond coating on WC cutting tool using electrophoresis

被引:0
|
作者
Tsubota, T
Nagata, M
Okada, N
Ida, S
Matsumoto, Y
Yatsushiro, N
机构
[1] Kumamoto Ind Res Inst, Mat Dev Dept, Kumamoto 8620901, Japan
[2] Kumamoto Univ, Fac Engn, Dept Appl Chem & Biochem, Kumamoto 8608555, Japan
[3] Kumabou Met Co, Kumamoto 8620937, Japan
关键词
diamond; CVD; WC; electrophoresis; ECR; adhesion; heat treatment; pretreatment;
D O I
10.2109/jcersj.109.1273_782
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
CVD diamond films were deposited on commercial WC cutting tools. An electron cyclotron resonance microwave plasma chemical vapor deposition (ECR-MPCVD) apparatus was used to deposit diamond films. Methane and hydrogen were used as gaseous source for CVD, and WC-Co (JIS standard: K-10) was used as a substrate for CVD. Cobalt on the surface of the WC cutting tool prevented CVD diamond from depositing on the WC cutting tool. Scratching with diamond particles on the surface of the WC cutting tool, which is one of the most popular pretreatments for enhancing the nuclei density of CVD diamond, was ineffective on the WC cutting tool without removing surface cobalt. On the other hand, Electrophoresis treatment was effective for increasing diamond nuclei density on the WC cutting tool without removing surface cobalt. However, CVD diamond films synthesized on the WC cutting tool (from which surface cobalt was removed) using electrophoresis pretreatment separated from the surface of the WC cutting tool. To improve the adhesion between CVD diamond film and WC cutting tool, heat treatment was performed after electrophoresis pretreatment. The heat treatment condition was 500 degreesC for I h in Ar flow. The heat treatment after electrophoresis treatment was effective for improving adhesion between WC surface and CVD diamond film. Vickers hardness test was carried out for estimating the adhesion. The Vickers hardness of the CVD diamond film obtained by the electrophore sis -heat pretreatment, was as hard as that of a CVD diamond film obtained with conventional scratching pretreatment. From the results of Vickers hardness test, it was found that heat treatment after electrophoresis process is effective for improving the strength of the adhesion layer.
引用
收藏
页码:782 / 788
页数:7
相关论文
共 50 条
  • [31] Laser cutting of CVD diamond wafers
    Chmelícková, H
    Vanecek, M
    Rosa, J
    Stranyánek, M
    XV International Symposium on Gas Flow, Chemical Lasers, and High-Power Lasers Pt 1 and 2, 2005, 5777 : 913 - 916
  • [32] CVD diamond insert in stone cutting
    Turchetta, S
    Carrino, L
    Polini, W
    DIAMOND AND RELATED MATERIALS, 2005, 14 (3-7) : 641 - 645
  • [33] TECHNOLOGY-ASSESSMENT FOR CVD-DIAMOND-COATED CUTTING-TOOL INSERTS
    WALTON, KR
    DISMUKES, JP
    KRUEGER, RA
    FIELD, FR
    CLARK, JP
    MATERIALS AND SOCIETY, 1989, 13 (03): : 319 - 350
  • [34] Effect of micro-cracks in coating on performance of CVD coated carbide cutting tool
    Katayama, S
    Hashimura, M
    ADVANCED CERAMIC TOOLS FOR MACHINING APPLICATION - III, 1998, 138-1 : 245 - 261
  • [35] The improvement of cutting performance in semi-dry condition by the combination of DLC coating and CVD smooth surface diamond coating
    Hanyu, H
    Kamiya, S
    Murakami, Y
    Kondoh, Y
    SURFACE & COATINGS TECHNOLOGY, 2005, 200 (1-4): : 1137 - 1141
  • [36] Case Studies of Diamond-coated Tool Cutting Simulations: Coating Thickness and Cutting Speed Effects
    Qin, Feng
    Chou, Y. Kevin
    PROCEEDINGS OF THE ASME INTERNATIONAL MANUFACTURING SCIENCE AND ENGINEERING CONFERENCE 2010, VOL 2, 2011, : 179 - 185
  • [37] CVD diamond coating of steel on a CVD-TiBN interlayer
    Bareiss, J. C.
    Hackl, G.
    Popovska, N.
    Rosiwal, S. M.
    Singer, R. F.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (3-4): : 718 - 723
  • [38] Research on precise cutting performance of CVD diamond
    Zhang, HZ
    Yao, YX
    Yuan, ZJ
    INITIATIVES OF PRECISION ENGINEERING AT THE BEGINNING OF A MILLENNIUM, 2001, : 284 - 288
  • [39] Evaluation of CVD diamond coating layer using leaky Rayleigh wave
    Song, Sung-Jin
    Kim, Hak-Joon
    Wang, Wen-Wu
    Yang, Dong-Ju
    Kim, Young H.
    Kwon, Sung D.
    Takagi, T.
    Uchimoto, T.
    Abe, T.
    ULTRASONICS, 2006, 44 (SUPPL.) : E1365 - E1369
  • [40] Fabrication and performance of CVD diamond cutting tool in micro milling of oxygen-free copper
    Zhao, Guolong
    Li, Ziyi
    Hu, Maoshun
    Li, Liang
    He, Ning
    Jamil, Muhammad
    DIAMOND AND RELATED MATERIALS, 2019, 100