摘要
C0(33)Zr(67) ribbons with increasing oxygen contents were produced by melt-spinning. Crystallizing phases were compared with the stable phases in the relevant part of the ternary system Co-Zr-O. Our results indicate that even minor oxygen contents lead to drastic changes in the crystallization mode and kinetics, i.e. the formation of nanocrystalline microstructures instead of large grained CoZr2. It is assumed that the dramatic change in the nucleation behaviour results from phase separation in the Co-Zr-O glasses. The nanocrystalline phase formed is always the so-called ''big-cube phase'' (E9(3), fcc: a approximate to 1.22 nm). Zr65Cu17.5N10Al7.5 ribbons without and with 1.5 at.% oxygen were produced by melt-spinning. Whereas in oxygen-free samples primary crystallization of a quasicrystalline phase was observed, crystallization of oxygenated glasses leads to additional formation of a nanocrystalline fee phase with the same structure as known from the binary Zr-based glasses.
引用
收藏
页码:311 / 316
页数:6
相关论文
共 50 条
  • [21] 非晶态Zr65Cu17.5Ni10Al7.5合金氧化和晶化过程研究
    王焕荣
    石志强
    张均燕
    滕新营
    闵光辉
    叶以富
    金属功能材料, 2002, (02) : 16 - 20
  • [22] Enhanced thermal stability of Zr65Cu17.5Ni10Al7.5 metallic glass at temperature range near glass transition by oxygen impurity
    He, L.
    Wu, Z. G.
    Jiang, F.
    Sun, J.
    JOURNAL OF ALLOYS AND COMPOUNDS, 2008, 456 (1-2) : 181 - 186
  • [23] Nanocrystallization of Zr61Al7.5Cu17.5Ni10Si4 metallic glass
    Jang, J. S. C.
    Tsao, S. F.
    Chang, Lj.
    Huang, J. C.
    Liu, C. T.
    INTERMETALLICS, 2009, 17 (1-2) : 56 - 64
  • [24] Study of air oxidation of amorphous Zr65Cu17.5Ni10Al7.5 by X-ray photoelectron spectroscopy (XPS)
    Dhawan, A.
    Zaporojtchenko, V.
    Faupel, F.
    Sharma, S. K.
    JOURNAL OF MATERIALS SCIENCE, 2007, 42 (21) : 9037 - 9044
  • [25] Bending deformation behavior of Zr65Cu17.5Ni10Al7.5 bulk metallic glass with different solidification cooling rate
    Hu, Y.
    Yan, H. H.
    Yan, Z. J.
    Wang, X. G.
    AIP ADVANCES, 2018, 8 (10)
  • [26] Study of air oxidation of amorphous Zr65Cu17.5Ni10Al7.5 by X-ray photoelectron spectroscopy (XPS)
    A. Dhawan
    V. Zaporojtchenko
    F. Faupel
    S. K. Sharma
    Journal of Materials Science, 2007, 42 : 9037 - 9044
  • [27] Mechanism of internal friction in bulk Zr65Cu17.5Ni10Al7.5 metallic glass -: art. no. 184208
    Cai, B
    Shang, LY
    Cui, P
    Eckert, J
    PHYSICAL REVIEW B, 2004, 70 (18): : 1 - 5
  • [28] Influence of iron additions on structure and properties of amorphous Zr65Al7.5CU17.5Ni10
    Mattern, N
    Roth, S
    Bauer, HD
    Henninger, G
    Eckert, J
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 304 (1-2): : 311 - 314
  • [29] Effect of hydrogen on Zr65Cu17.5Al7.5Ni10 metallic glass
    Ismail, N
    Gebert, A
    Uhlemann, M
    Eckert, J
    Schultz, L
    JOURNAL OF ALLOYS AND COMPOUNDS, 2001, 314 (1-2) : 170 - 176
  • [30] Air oxidation of Zr65Cu17.5Ni10Al7.5 its amorphous and supercooled liquid states, studied by thermogravimetric analysis
    Dhawan, A
    Raetzke, K
    Faupel, F
    Sharma, SK
    PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 2003, 199 (03): : 431 - 438