Effect of thickness and loading mode on the fracture properties of V-4Cr-4Ti at room temperature

被引:11
|
作者
Li, H [1 ]
Kurtz, RJ [1 ]
Jones, RH [1 ]
机构
[1] Pacific NW Lab, Richland, WA 99352 USA
关键词
D O I
10.1016/S0022-3115(98)00160-3
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of thickness on the room temperature (RT) mode I fracture behavior of V-4Cr-4Ti has been investigated. Mode I fracture properties were measured from J-integral tests of compact tension (CT) specimens ranging in thickness from 6.4 to 25.4 mm. Al specimens were machined in the T-L orientation and vacuum annealed following final machining. Two heats of V-4Cr-4Ti were tested. Specimens 6.4 and 12.7 mm thick were taken from Wah Chang Heat No. 832665. The 25.4 mm thick specimens were obtained from Wah Chang Heat No. 832864. The effect of loading mode on fracture of V-4Cr-4Ti at RT was also studied using material from Heat No. 832665. Mode I fracture behavior was compared to mixed-mode (I/III) fracture properties obtained from modified CT specimens. Crack angles of 0 degrees and 25 degrees were used to vary the ratio of mode III to mode I loading. J-R curves were generated as the basis for determining the affect of loading mode. The specimen loaded in mixed-mode exhibited lower resistance to crack initiation and propagation than pure mode I specimens. (C) 1998 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:1386 / 1391
页数:6
相关论文
共 50 条
  • [41] Reference vanadium alloy V-4Cr-4Ti for fusion application
    Smith, DL
    Chung, HM
    Loomis, BA
    Tsai, HC
    JOURNAL OF NUCLEAR MATERIALS, 1996, 233 : 356 - 363
  • [42] Mechanical properties of V-4Cr-4Ti after exposure in static lithium at 650°C
    The Graduate University for Advanced Studies , Toki 509-5292, Japan
    不详
    不详
    Plasma Fusion Res., 1 SPECIAL ISSUE
  • [43] Metallurgical and mechanical properties of laser weldment for low activation V-4Cr-4Ti alloy
    Heo, NJ
    Nagasaka, T
    Muroga, T
    Nishimura, A
    Shinozaki, K
    Takeshita, N
    FUSION ENGINEERING AND DESIGN, 2002, 61-62 : 749 - 755
  • [44] Microstructure of V-4Cr-4Ti alloy after low-temperature irradiation by ions and neutrons
    Gazda, J.
    Meshii, M.
    Chung, H.M.
    Journal of Nuclear Materials, 1998, 258-263 (pt B): : 1437 - 1441
  • [45] Effect of small additional elements on DBTT of V-4Cr-4Ti irradiated at low temperatures
    Shibayama, T
    Yamagata, I
    Kayano, H
    Namba, C
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1361 - 1368
  • [46] Temperature dependence of the radiation damage microstructure in V-4Cr-4Ti neutron irradiated to low dose
    Rice, PM
    Zinkle, SJ
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1414 - 1419
  • [47] Temperature dependence of the radiation damage microstructure in V-4Cr-4Ti neutron irradiated to low dose
    Rice, P.M.
    Zinkle, S.J.
    Journal of Nuclear Materials, 1998, 258-263 (pt B): : 1414 - 1419
  • [48] Pulse current electrodeposition of tungsten coatings on V-4Cr-4Ti alloy
    Jiang, Fan
    Zhang, Yingchun
    Li, Xuliang
    FUSION ENGINEERING AND DESIGN, 2015, 93 : 30 - 35
  • [49] Helium-vacancy clustering in V-4Cr-4Ti at elevated temperatures
    Fedorov, AV
    van Veen, A
    Ryazanov, AI
    JOURNAL OF NUCLEAR MATERIALS, 1998, 258 : 1396 - 1399
  • [50] Influence of heat treatment on hydrogen ingress into V-4Cr-4Ti alloy
    Hayakawa, R
    Hatano, Y
    Fukumoto, K
    Matsui, H
    Watanabe, K
    JOURNAL OF NUCLEAR MATERIALS, 2004, 329 : 411 - 415