Characterization of Hydrogen-Induced Contact Fracture in High-Strength Steel

被引:2
|
作者
Yonezu, Akio [1 ]
Niwa, Michihiro [1 ]
Chen, Xi [2 ,3 ]
机构
[1] Chuo Univ, Dept Precis Mech, Bunkyo Ku, Tokyo 1128551, Japan
[2] Columbia Univ, Dept Earth & Environm Engn, New York, NY 10027 USA
[3] Xi An Jiao Tong Univ, Sch Aerosp, Int Ctr Appl Mech, SV Lab, Xian 710049, Peoples R China
来源
JOURNAL OF ENGINEERING MATERIALS AND TECHNOLOGY-TRANSACTIONS OF THE ASME | 2015年 / 137卷 / 02期
基金
美国国家科学基金会; 中国国家自然科学基金; 日本学术振兴会;
关键词
contact loading; spherical indentation test; hydrogen embrittlement cracking; high-strength steel; STRESS INTENSITY FACTOR; ASSISTED CRACK-GROWTH; INDENTATION CRACKING; EMBRITTLEMENT; TOUGHNESS; FATIGUE; DAMAGE;
D O I
10.1115/1.4029530
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
This study investigated the hydrogen embrittlement (HE) cracking behavior produced by local contact loading of high-strength steel. When a spherical impression was applied to a hydrogen-absorbed high-strength steel, HE induces contact fracture, where radial cracks are initiated and propagated from the indentation impression. The length of the radial crack was found to be dependent on the hydrogen content in the steel as well as the applied contact force. A combined experimental/computational investigation was conducted in order to clarify the mechanism of hydrogen-induced contact fracture. In the computation, crack propagation was simulated using a cohesive zone model (CZM) in finite element method (FEM), in order to elucidate stress criterion of the present HE crack. It was found that the normal tensile stress was developed around impression, and it initiated and propagated the HE crack. It was also revealed that the hydrogen content enhanced contact fracture damage, especially the resistance of crack propagation (i.e., threshold stress intensity factor, Kth). The findings may be useful for countermeasure of contact fracture coupled with hydrogen in high-strength steel. Such phenomenon is potentially experienced in various contact components in hydrogen environment.
引用
收藏
页数:7
相关论文
共 50 条
  • [21] Effect of Nb on the hydrogen-induced cracking of high-strength low-alloy steel
    Zhang Shiqi
    Fan Endian
    Wan Jifang
    Liu Jing
    Huang Yunhua
    Li Xiaogang
    CORROSION SCIENCE, 2018, 139 : 83 - 96
  • [22] Hydrogen-induced delayed fracture behaviour of V plus Nb-microalloyed high-strength bolt steel with internal and environmental hydrogen
    Zhang, Chengxiang
    Hui, Weijun
    Zhao, Xiaoli
    Zhang, Yongjian
    Zhao, Xiuming
    CORROSION SCIENCE, 2022, 209
  • [24] Effects of Niobium and Vanadium on Hydrogen-Induced Delayed Fracture in High Strength Spring Steel
    Chao-lei Zhang
    Ya-zheng Liu
    Chao Jiang
    Jin-fu Xiao
    Journal of Iron and Steel Research International, 2011, 18 : 49 - 53
  • [25] Effects of Niobium and Vanadium on Hydrogen-Induced Delayed Fracture in High Strength Spring Steel
    Zhang Chao-lei
    Liu Ya-zheng
    Jiang Chao
    Xiao Jin-fu
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2011, 18 (06) : 49 - 53
  • [26] Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment
    Zhang, Peng
    Laleh, Majid
    Hughes, Anthony E.
    Marceau, Ross K. W.
    Hilditch, Tim
    Tan, Mike Yongjun
    CORROSION SCIENCE, 2024, 227
  • [27] RECENT OBSERVATION OF HYDROGEN-INDUCED CRACKING OF HIGH-STRENGTH STEELS
    McMahon, C. J., Jr.
    Liu, Xinyu
    Kameda, Jun
    Morgan, Michael J.
    EFFECTS OF HYDROGEN ON MATERIALS, 2009, : 46 - +
  • [28] Hydrogen-induced delayed fracture of a 1180 MPa martensitic advanced high-strength steel under U-bend loading
    Li, Huixing
    Venezuela, Jeffrey
    Zhou, Qingjun
    Luzin, Vladimir
    Yan, Ming
    Shi, Zhiming
    Knibbe, Ruth
    Zhang, Mingxing
    Dong, Futao
    Dargusch, Matthew S.
    Atrens, Andrej
    Materials Today Communications, 2021, 26
  • [29] HYDROGEN-INDUCED CRACKING SUSCEPTIBILITY IN HIGH-STRENGTH WELD METAL
    OKUDA, N
    OGATA, Y
    NISHIKAWA, Y
    AOKI, T
    GOTO, A
    ABE, T
    WELDING JOURNAL, 1987, 66 (05) : S141 - S146
  • [30] Hydrogen-induced delayed fracture of a 1180 MPa martensitic advanced high-strength steel under U-bend loading
    Li, Huixing
    Venezuela, Jeffrey
    Zhou, Qingjun
    Luzin, Vladimir
    Yan, Ming
    Shi, Zhiming
    Knibbe, Ruth
    Zhang, Mingxing
    Dong, Futao
    Dargusch, Matthew S.
    Atrens, Andrej
    MATERIALS TODAY COMMUNICATIONS, 2021, 26