EIS evaluation of the filiform corrosion of aluminium coated by a cataphoretic paint

被引:35
|
作者
Olivier, MG
Poelman, M
Demuynck, M
Petitjean, JP
机构
[1] Materia Nova ASBL, B-7000 Mons, Belgium
[2] Fac Polytech Mons, B-7000 Mons, Belgium
关键词
filiform corrosion; electrochemical impedance spectroscopy; aluminium alloy; cataphoretic primer; conversion treatment;
D O I
10.1016/j.porgcoat.2004.05.008
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
Filiform. corrosion is mainly considered as a cosmetic attack and is undesirable in most applications. The initiation and propagation of the filaments are related to different parameters such as the presence of defects, the permeability of the coating to water and oxygen, the adherence of the paint system and the presence of salts. The aim of this work is to study the behaviour of painted aluminium samples towards filiform corrosion or delamination. The 6082 Aluminium alloy was selected and the samples were covered with a cataphoretic epoxy primer without lead (PPG Industries France). Prior to the application of the electrocoat, the samples were pre-treated by a commercial Zr/Ti or chromate conversion treatment or simply etched with a commercial acid etching product. Filiform corrosion was studied by the normalized test (ISO/DIS 4623): painted and scratched samples were inoculated in HCl and exposed in a constant humidity chamber at 40 degrees C and 82% RH for 3 weeks. After exposure the samples were subjected to a visual and optical microscopic examination. Electrochemical impedance spectroscopy was used to study the sensitivity to filiform corrosion. The operating mode of this test is similar to the normalized one. The samples were scratched before inoculation for 1 h in HCl and then exposed to the humidity chamber for a maximum of 4 days. The samples were tested by EIS in an acidified 0.1 M Na2SO4 electrolyte solution. The resulting impedance spectra were analyzed with an appropriate equivalent electrical circuit which allows the evaluation of the exposed metallic surface area, directly related to the extent of filiform corrosion or delamination. Different parameters were varied: the exposure time in the humidity chamber; the immersion time in the electrolyte sulphate solution as well as its pH and the coating thickness. (c) 2004 Elsevier B.V. All rights reserved.
引用
收藏
页码:263 / 270
页数:8
相关论文
共 50 条
  • [31] On the evaluation of filiform corrosion test results
    Bockmair, G.
    von Czarnecki, J.
    Strob, G.
    Farbe und Lack, 105 (01): : 74 - 76
  • [32] Filiform corrosion of electrocoated aluminium alloy: Role of surface pretreatment
    Nazarov, A.
    Romano, A. -P.
    Fedel, M.
    Deflorian, F.
    Thierry, D.
    Olivier, M. -G.
    CORROSION SCIENCE, 2012, 65 : 187 - 198
  • [33] Filiform corrosion on 6000 series aluminium: Kinetics and inhibition strategies
    Coleman, A. J.
    McMurray, H. N.
    Williams, G.
    Afseth, A.
    Scamans, G.
    ALUMINIUM ALLOYS 2006, PTS 1 AND 2: RESEARCH THROUGH INNOVATION AND TECHNOLOGY, 2006, 519-521 : 629 - 633
  • [34] A filiform corrosion and potentiodynamic polarisation study of some aluminium alloys
    J. M. C. Mol
    B. R. W. Hinton
    D. H. Van Der Weijde
    J. H. W. De Wit
    S. Van Der Zwaag
    Journal of Materials Science, 2000, 35 : 1629 - 1639
  • [35] Cerium pretreatments to prevent filiform corrosion of painted aluminium alloys
    Poulain, V
    Petitjean, JP
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 1641 - 1647
  • [36] A filiform corrosion and potentiodynamic polarisation study of some aluminium alloys
    Mol, JMC
    Hinton, BRW
    Van der Weijde, DH
    De Wit, JHW
    Van der Zwaag, S
    JOURNAL OF MATERIALS SCIENCE, 2000, 35 (07) : 1629 - 1639
  • [37] Effect of powder painting procedures on the filiform corrosion of aluminium profiles
    Fedrizzi, L.
    Stenico, M.
    Deflorian, F.
    Maschio, S.
    Bonora, P. L.
    PROGRESS IN ORGANIC COATINGS, 2007, 59 (03) : 230 - 238
  • [38] Filiform corrosion of aluminium sheet. I. Corrosion behaviour of painted material
    Leth-Olsen, H
    Nisancioglu, K
    CORROSION SCIENCE, 1998, 40 (07) : 1179 - 1194
  • [39] INVESTIGATION FOR FILIFORM CORROSION ON LOW TIN COATED STEEL SHEETS
    KANEDA, Y
    TETSU TO HAGANE-JOURNAL OF THE IRON AND STEEL INSTITUTE OF JAPAN, 1987, 73 (05): : S408 - S408
  • [40] Effect of climatic parameters on filiform corrosion of coated aluminum alloys
    LeBozec, N
    Persson, D
    Thierry, D
    Axelsen, SB
    CORROSION, 2004, 60 (06) : 584 - 593