Boroaluminide coatings on ferritic-martensitic steel deposited by low-temperature pack cementation

被引:34
|
作者
Tsipas, S. A. [1 ]
Omar, H. [2 ]
Perez, F. H. [1 ]
Tsipas, D. N. [2 ]
机构
[1] Univ Complutense Madrid, Dpto Ciencia Mat, Grp Invest Ingn Superficies, Fac Ciencias Quim, E-28040 Madrid, Spain
[2] Aristotle Univ Thessaloniki, Met Phys Lab, Dept Mech Engn, Thessaloniki 54124, Greece
来源
SURFACE & COATINGS TECHNOLOGY | 2008年 / 202卷 / 14期
关键词
thermodynamic calculations; protective coatings; boron; steels; pack cementation; thermochemical processes; diffusion barrier;
D O I
10.1016/j.surfcoat.2007.11.034
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, new boroaluminide protective coatings were deposited on ferritic-martensitic steel substrates (P91) using the pack cementation technique, at moderate temperatures in order not to influence the substrates' mechanical properties. Extensive thermodynamic calculations were performed initially, using the Thermocalc Computer program, so as to optimize the process parameters. The most important gas-precursors for successful deposition of the coatings were identified. The effect of pack composition on the formation and growth of boroaluminides at 715 degrees C, using pack powders containing Al and B as element depositing sources, two halide salts as activators, and Al2O3 as inert filler, was investigated. Three distinct regions were found in the coatings consisting of an outer Al-rich layer, a transition region containing Al, B and Fe and an inner layer containing mostly B, Cr and Fe. The layers were characterized by means of optical and Scanning Electron Microscopy (SEM) in terms of coating morphology and thickness. X-ray diffraction (XRD) was used in order to detect the phases formed and the presence of iron aluminide and boride phases in the coatings due to the boroaluminizing process. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:3263 / 3271
页数:9
相关论文
共 50 条
  • [31] Creep and corrosion testing of aluminide coatings on ferritic-martensitic substrates
    Dryepondt, S.
    Zhang, Y.
    Pint, B. A.
    SURFACE & COATINGS TECHNOLOGY, 2006, 201 (07): : 3880 - 3884
  • [32] Low temperature embrittlement behaviour of different ferritic-martensitic alloys for fusion applications
    Rieth, M
    Dafferner, B
    JOURNAL OF NUCLEAR MATERIALS, 1996, 233 (233-237) : 229 - 232
  • [33] Low cycle fatigue properties of ODS ferritic-martensitic steels at high temperature
    Ukai, S.
    Ohtsuka, S.
    JOURNAL OF NUCLEAR MATERIALS, 2007, 367 (SPEC. ISS.) : 234 - 238
  • [34] Prediction of wall temperature and oxide scale thickness of ferritic-martensitic steel superheater tubes
    Sun, Li
    Yan, Weiping
    APPLIED THERMAL ENGINEERING, 2018, 134 : 171 - 181
  • [35] The bipolar plate of AISI 1045 steel with chromized coatings prepared by low-temperature pack cementation for proton exchange membrane fuel cell
    Bai, Ching-Yuan
    Wen, Tse-Min
    Hou, Kung-Hsu
    Ger, Ming-Der
    JOURNAL OF POWER SOURCES, 2010, 195 (03) : 779 - 786
  • [36] Deposition of Manganese and Cobalt on Ferritic–Martensitic Steels via Pack Cementation Process
    Diana Schmidt
    Mathias Galetz
    Michael Schütze
    Oxidation of Metals, 2013, 79 : 589 - 599
  • [37] Effects of substrate surface roughness and aluminizing agent composition on the aluminide coatings by low-temperature pack cementation
    Dong, Jian
    Sun, Yanhui
    He, Feiyu
    Huang, Hongtao
    Zhen, Jianping
    MATERIALS RESEARCH EXPRESS, 2019, 6 (03)
  • [38] Oxidation behavior of aluminide coatings on carbon steel with and without electrodeposited Ni-CeO2 film by low-temperature pack cementation
    Zhou, Y. B.
    Hu, H. T.
    Zhang, H. J.
    VACUUM, 2011, 86 (02) : 210 - 217
  • [39] New insights into the oxidation mechanisms of a Ferritic-Martensitic steel in high-temperature steam
    Shen, Zhao
    Chen, Kai
    Yu, Hongbing
    Jenkins, Benjamin
    Ren, Yanru
    Saravanan, Naganand
    He, Guanze
    Luo, Xiaonan
    Bagot, Paul A. J.
    Moody, Michael P.
    Zhang, Lefu
    Lozano-Perez, Sergio
    ACTA MATERIALIA, 2020, 194 : 522 - 539
  • [40] Hydrogen interaction with the low activation ferritic-martensitic steel EK-181 (Rusfer)
    Golubeva, A. V.
    Bobyr, N. P.
    Cherkez, D. I.
    Spitsyn, A. V.
    Mayer, M.
    Gasparyan, Yu. M.
    Efimov, V. S.
    Chernov, V. M.
    Leontieva-Smirnova, M. V.
    JOURNAL OF NUCLEAR MATERIALS, 2013, 438 : S983 - S987