Microstructural Evolution in Various Regions of Stir Zone during Friction Stir Processing of Al-7Si-0.3Mg Cast Alloy

被引:3
|
作者
Chen, Zhan W. [1 ]
Cui, Song [1 ]
Gao, Wei [2 ]
Zhu, Tianping [2 ]
机构
[1] AUT Univ, Dept Mech & Mfg Engn, Auckland, New Zealand
[2] Univ Auckland, Dept Chem & Mat Engn, Auckland, New Zealand
来源
PRICM 7, PTS 1-3 | 2010年 / 654-656卷
关键词
Friction stir; materials flow; cast and wrought microstructures;
D O I
10.4028/www.scientific.net/MSF.654-656.962
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Castings may be used more as structural components if friction stir (FS) processing could refine the microstructures satisfactorily. For this, material flow and the formation of various microstructural regions during FS were studied. It was found that alpha-Al dendrites and eutectic Al-Si were sheared into the thread spaces and the microstructures were significantly modified and refined. Material merely dragged into the FS zone remains microstructurally segregated. The volume of each flow was affected by rotation speed and forward speed and the reason for this is explained. Finally, textures determined together with the strain values estimated are presented to discuss further the microstructual development in various stir zones.
引用
收藏
页码:962 / +
页数:2
相关论文
共 50 条
  • [21] Properties Augmentation of Cast Hypereutectic Al–Si Alloy Through Friction Stir Processing
    William P. Bates
    Vivek Patel
    Harikrishna Rana
    Joel Andersson
    Jeroen De Backer
    Mattias Igestrand
    Livan Fratini
    [J]. Metals and Materials International, 2023, 29 : 215 - 228
  • [22] Ductilizing of cast hypereutectic Al-17%Si alloy by friction stir processing
    Saini, Nitin
    Pandey, Chandan
    Dwivedi, Dheerendra Kumar
    [J]. PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART E-JOURNAL OF PROCESS MECHANICAL ENGINEERING, 2018, 232 (06) : 696 - 701
  • [23] Inhibition of delayed ageing by trace additions in Al-7Si-0.3Mg Cast alloy
    Murali, S.
    Kashyap, K.T.
    Raman, K.S.
    Murthy, K.S.S.
    [J]. Scripta Metallurgica et Materialia, 1993, 29 (11): : 1421 - 1426
  • [24] Continuous cooling precipitation diagram of cast aluminium alloy Al-7Si-0.3Mg
    Milkereit, Benjamin
    Froeck, Hannes
    Schick, Christoph
    Kessler, Olaf
    [J]. TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2014, 24 (07) : 2025 - 2033
  • [25] Microstructural evolution and mechanical properties of Al-7Si-0.3Mg alloys with erbium additions
    Pandee, P.
    Patakham, U.
    Limmaneevichitr, C.
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 728 : 844 - 853
  • [26] Characteristics of Microstructure and Texture in the Stir Zone of Friction Stir Welded Al-12.7Si-0.7Mg Alloy
    He, Changshu
    Wang, Dong
    Tong, Weiping
    Zhao, Gang
    Zhao, Xiang
    Zuo, Liang
    [J]. TEXTURES OF MATERIALS, PTS 1 AND 2, 2012, 702-703 : 56 - +
  • [27] Friction Stir Processing of Cast Mg-Y-Zn Alloy
    Morishige, T.
    Tsujikawa, M.
    Oki, S.
    Kamita, M.
    Chung, S. W.
    Higashi, K.
    [J]. THERMEC 2006 SUPPLEMENT: 5TH INTERNATIONAL CONFERENCE ON PROCESSING AND MANUFACTURING OF ADVANCED MATERIALS, 2007, 15-17 : 369 - 374
  • [28] Friction stir processing of a cast WE43 mg alloy
    Freeney, T. A.
    Mishra, R. S.
    Grant, G. J.
    Verma, R.
    [J]. FRICTION STIR WELDING AND PROCESSING IV, 2007, : 429 - +
  • [29] Microstructural evolution and mechanical properties of Mg-Zn-Y-Zr alloy during friction stir processing
    Wang, Yaobin
    Huang, Yongxian
    Meng, Xiangchen
    Wan, Long
    Feng, Jicai
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 696 : 875 - 883
  • [30] Effect of friction stir processing on aging properties of die-cast Al-Si-Cu-Mg alloy
    Ando T.
    Enomoto R.
    Yoshida Y.
    Ito K.
    [J]. Keikinzoku Yosetsu/Journal of Light Metal Welding, 2020, 58 : 19 - 23