Capillary absorption of water and n-decane by autoclaved aerated concrete

被引:65
|
作者
Ioannou, Ioannis [1 ]
Hamilton, Andrea [2 ,3 ]
Hall, Christopher [2 ,3 ]
机构
[1] Univ Cyprus, Sch Engn, CY-1678 Nicosia, Cyprus
[2] Univ Edinburgh, Sch Elect & Engn, Edinburgh EH9 3JL, Midlothian, Scotland
[3] Univ Edinburgh, Ctr Mat Sci & Engn, Edinburgh EH9 3JL, Midlothian, Scotland
基金
英国工程与自然科学研究理事会;
关键词
autoclaved aerated concrete; transport properties; microstructure; pore size distribution;
D O I
10.1016/j.cemconres.2008.01.013
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
An autoclaved aerated concrete was one of three construction materials used in the round-robin study of hygral properties carried out in the European Commission funded Heat, Air and Moisture Standards Development [HAMSTAD] project (Roels S et al., Journal of Thermal Envelope and Building Science 2004 27 307-325). The material has fine micron-scale matrix porosity generated by the packing of thin tobermorite 11 angstrom plates; and coarse mm-scale aeration pores arising from the foaming of the wet mix. We treat the material as having a strongly bimodal pore size distribution. Capillary absorption does not obey simple t(1/2) kinetics. We report here the results of liquid uptake tests using both water and n-decane to investigate the cause of the inhibition behaviour. The transport properties are modelled in a Sharp Front analysis as a parallel combination of absorption into the coarse aeration pores and into the fine matrix pores. The aeration pores have weak capillary suction and absorption into these pores reaches capillary rise equilibrium during the test. The Sharp Front model is applied here for the first time separately to subsets of the total porosity. The matrix sorptivity of the autoclaved aerated concrete studied (density 450 kg m(-3), porosity 0.82) is about 0.23 mm min(-1/2). (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:766 / 771
页数:6
相关论文
共 50 条
  • [21] Autoclaved aerated concrete as an obstacle for burglars
    Flassenberg, Georg
    Jürgen, M.A.
    Küenzlen, H.R.
    Betonwerk und Fertigteil-Technik/Concrete Plant and Precast Technology, 2011, 77 (04): : 16 - 20
  • [22] Reinforced Autoclaved Aerated Concrete in the UK
    Atkins, Chris
    Corrosion Management, 2024, (177): : 30 - 33
  • [23] ANOMALOUS TOBERMORITE IN AUTOCLAVED AERATED CONCRETE
    MITSUDA, T
    CHAN, CF
    CEMENT AND CONCRETE RESEARCH, 1977, 7 (02) : 191 - 194
  • [24] Drying shrinkage of autoclaved aerated concrete
    Jerman, Milos
    Vyborny, Jaroslav
    Cerny, Robert
    THEROPHYSICS 2011 - CONFERENCE PROCEEDINGS, 2011, : 72 - 76
  • [25] Effect of Dry-Wet Circulation on Moisture Absorption of Autoclaved Aerated Concrete
    He, Xiao
    Yin, Jian
    Yang, Jiewen
    Liang, Qiao
    Wu, Songyun
    ADVANCES IN MATERIALS SCIENCE AND ENGINEERING, 2019, 2019
  • [26] CHEMICAL PROTECTION OF AERATED AUTOCLAVED CONCRETE MASONRY AGAINST WATER AND MOISTURE
    Struharova, Alena
    Dubik, Marian
    14TH CONFERENCE ON ENVIRONMENT AND MINERAL PROCESSING, PT II, 2010, : 133 - 135
  • [27] Measurement and modeling of water sorption isotherm of autoclaved aerated concrete with salt
    Abuku, Masaru
    Ogura, Daisuke
    Hokoi, Shuichi
    Journal of Environmental Engineering (Japan), 2014, 79 (700): : 499 - 506
  • [28] Experimental and Modeling Investigations on the Water Sorption Behaviors of Autoclaved Aerated Concrete
    Garbalinska, Halina
    Bochenek, Magdalena
    Stasiak, Marcin
    MATERIALS, 2021, 14 (21)
  • [29] Photocatalytic degradation of n-decane and n-decene in water system
    Zhong, Ping
    Kong, Ling-Ren
    Feng, Jian-Fang
    Liu, Guang-Ming
    Zhongguo Huanjing Kexue/China Environmental Science, 2003, 23 (02):
  • [30] VISCOSITY OF HYDROCARBONS - N-DECANE
    CARMICHAEL, LT
    BERRY, VM
    SAGE, BH
    JOURNAL OF CHEMICAL AND ENGINEERING DATA, 1969, 14 (01): : 27 - +