Titanium-Enriched Slag Prepared by Atmospheric Hydrochloric Acid Leaching of Mechanically Activated Vanadium Titanomagnetite Concentrates

被引:3
|
作者
Wu, En-Hui [1 ]
Lin, Yin-He [2 ]
Liu, Jun [3 ]
Wang, Zhe [4 ]
Liu, Jin-Chuan [2 ]
Yin, Guo-Liang [2 ]
Li, Jing-Wei [5 ,6 ]
Cheng, Xiang-Kui [1 ]
Jia, Yu-Long [2 ]
机构
[1] Panzhihua Univ, Panzhihua Int Res Inst Vanadium & Titanium, Panzhihua 617000, Peoples R China
[2] Yinbin Univ, Sch Mat & Chem Engn, Yibin 644007, Peoples R China
[3] Sichuan Lomon Min & Met Co Ltd, Titanium Chloride Slag Plant, Panzhihua 617000, Peoples R China
[4] Univ Sci & Technol Beijing, State Key Lab Adv Met, Beijing 100083, Peoples R China
[5] Hefei Univ Technol, Sch Mat Sci & Engn, Hefei 230009, Peoples R China
[6] Hefei Univ Technol, Natl Local Joint Engn Res Ctr Nonferrous Met & Pr, Hefei 230009, Peoples R China
基金
中国国家自然科学基金;
关键词
vanadium titanomagnetite concentrates; mechanical activation; hydrochloric acid Leaching; titanium-enriched slag; TiO2; extraction; BEARING TITANOMAGNETITE; DIRECT-REDUCTION; CARBOTHERMIC REDUCTION; BEHAVIOR; RECOVERY; IRON; SEPARATION; CHROMIUM; PELLETS;
D O I
10.3390/ma14226736
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The titanium-enriched slag was obtained via atmospheric hydrochloric acid leaching of mechanically activated vanadium titanomagnetite concentrates (VTMCs). Under the influence of mechanical activation, specific physicochemical changes were observed via X-ray diffractometry, scanning electron microscopy, and granulometric laser diffraction analysis. Experimental findings revealed that the mechanical activation of VTMCs resulted in a decrease in the median volume particle diameter (d50) and an increase in the specific surface area (SA) with an increased milling time. The results of the leaching experiment revealed that the mechanical activation treatment favors the extraction of iron (Fe) and titanium dioxide (TiO2) from the VTMCs. The Fe and TiO2 extractions from the mechanically activated sample after 10 h compared with the unactivated sample were increased by 12.82% and 4.73%, respectively. The presence of the ilmenite phase in the titanium-enriched slag was confirmed by X-ray diffractometry and EDS patterns, and the content of the TiO2 in the enriched slag can get as high as 43.75%.
引用
收藏
页数:11
相关论文
共 34 条
  • [31] Efficient separation of vanadium, titanium, and iron from vanadium-bearing titanomagnetite by pressurized pyrolysis of ammonium chloride-acid leaching-solvent extraction process
    Bian, Zhenzhong
    Feng, Yali
    Li, Haoran
    Wu, Hao
    SEPARATION AND PURIFICATION TECHNOLOGY, 2021, 255
  • [32] Recovery of TiO2-enriched material from vanadium titano-magnetite concentrates by partial carbon reduction and mild acid leaching
    Safdar, Faiza
    Zhang, Ying
    Zheng, Shili
    Chen, Xing
    Sun, Pei
    Zhang, Yang
    Li, Ping
    HYDROMETALLURGY, 2020, 193
  • [33] φ-pH diagram of V-Ti-H2O system during pressure acid leaching of converter slag containing vanadium and titanium
    Mu Wang-zhong
    Zhang Ting-an
    Dou Zhi-he
    Lu Guo-zhi
    Liu Yan
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2011, 21 (09) : 2078 - 2086
  • [34] Recovery of titanium compounds from Ti-enriched product of alkali melting Ti-bearing blast furnace slag by dilute sulfuric acid leaching
    He, Siqi
    Sun, Hongjuan
    Tan, Daoyong
    Peng, Tongjiang
    SELECTED PROCEEDINGS OF THE TENTH INTERNATIONAL CONFERENCE ON WASTE MANAGEMENT AND TECHNOLOGY, 2016, 31 : 977 - 984