Effects of Zr on microstructural evolution and mechanical property of Cu-15Ni-8Sn alloy

被引:37
|
作者
Zhang, Junjia [1 ]
Liu, Zhaoyu [1 ]
Guo, Zhongkai [3 ]
Liu, Shichao [4 ]
Dong, Yong [5 ]
Fu, Ying [6 ]
Jie, Jinchuan [3 ]
Zhang, Deliang [2 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Lightweight Struct Mat Liaoning Prov, Shenyang 110819, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
[3] Dalian Univ Technol, Sch Mat Sci & Engn, Dalian 116024, Peoples R China
[4] Soochow Univ, Sch Iron & Steel, Suzhou 215021, Jiangsu, Peoples R China
[5] Guangdong Univ Technol, Sch Mat & Energy, Guangzhou 510006, Peoples R China
[6] Bohai Univ, Sch Engn, Jinzhou 121007, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Cu-15Ni-8Sn alloy; Microstructural evolution; Discontinuous precipitation; Mechanical property; CELLULAR PRECIPITATION; SPINODAL DECOMPOSITION; CU-CR; BEHAVIOR; ELEMENTS;
D O I
10.1016/j.msea.2021.142287
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Cu-15Ni-8Sn-XZr (wt.%, X=0-0.7) alloys were prepared by vacuum melting, and their microstructural evolutions during the solidification and heat-treatment processes were systematically investigated as well as the corresponding mechanical properties. Zr addition could offer a significant effect on the dendritic morphology by controlling the constitutional supercooling in solidification front, and it also made the gamma-phase more likely to form in the needlelike-shape rather than the lamellar-like shape in subsequent cooling process. After solution treatment, the Zr atoms with a low content of 0.1 wt% were completely solidly dissolved in the alpha-matrix. With its content increasing to 0.3 and 0.5 wt%, the existence form was changed into the nano-scale precipitation phase (Ni5Zr) and then to micron-scale segregation phase (Ni4SnZr). The presence of Zr could significantly extend the aging window of alloy and improve its mechanical properties by inhibiting the nucleation and growth of discontinuous precipitation (DP), and there was few DP even after 16 h aging. The optimal combination of properties was obtained for Cu-15Ni-8Sn-0.5Zr alloy aged at 673 K for 4-16 h, including a hardness of 330HB, ultimate tensile strength (UTS) of 980 MPa and electrical conductivity of 9%IACS.
引用
收藏
页数:10
相关论文
共 50 条
  • [41] Spinodal decomposition, ordering transformation, and discontinuous precipitation in a Cu-15Ni-8Sn alloy
    Zhao, JC
    Notis, MR
    ACTA MATERIALIA, 1998, 46 (12) : 4203 - 4218
  • [42] Hot isostatic pressing of Cu-15Ni-8Sn alloy with suppressed Sn macro-segregation and enhanced mechanical properties
    Li, Jikang
    Zhang, Zhenwu
    Xu, Wenhe
    Yang, Yuanqi
    Xue, Pengju
    Teng, Qing
    Cai, Chao
    Li, Wei
    Wei, Qingsong
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 855
  • [43] Electrochemical corrosion behavior of Cu-15Ni-8Sn alloy in marine microbial medium
    Lei, Yanhua
    Yin, Yansheng
    Liu, Chaohong
    Chang, Xueting
    Chen, Yan
    Cheng, Sha
    MULTI-FUNCTIONAL MATERIALS AND STRUCTURES II, PTS 1 AND 2, 2009, 79-82 : 1099 - 1102
  • [44] Microstructure evolution and mechanical property of Cu-15Ni-8Sn-0.2Nb alloy during aging treatment
    Wang, Nan
    Shen, Yidi
    An, Qi
    Reddy, Kolan Madhav
    Jin, Mingjiang
    Karre, Rajamallu
    Wang, Xiaodong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2021, 86 : 227 - 236
  • [45] Microstructure evolution and mechanical property of Cu-15Ni-8Sn-0.2Nb alloy during aging treatment
    Nan Wang
    Yidi Shen
    Qi An
    Kolan Madhav Reddy
    Mingjiang Jin
    Rajamallu Karre
    Xiaodong Wang
    Journal of Materials Science & Technology, 2021, 86 (27) : 227 - 236
  • [46] The Mechanical Mixed Layer and Its Role in Cu-15Ni-8Sn/Graphite Composites
    Feng, Chunfang
    Wang, Yan
    Chen, Wu
    Zhang, Lei
    Zhou, Kechao
    TRIBOLOGY TRANSACTIONS, 2017, 60 (01) : 135 - 145
  • [47] Evolution of microstructure and mechanical properties during hot forging and heat treatments of Cu-15Ni-8Sn alloy fabricated by hot isostatic pressing
    Hu, Meichen
    Zhang, Xianwei
    Liu, Chaoqiang
    Gan, Xueping
    JOURNAL OF ALLOYS AND COMPOUNDS, 2025, 1010
  • [49] Effects of Initial States on the Spinodal Decomposition of Quenched and Melt-Spun Cu-15Ni-8Sn Alloy
    Kondo, Shin-ichiro
    Masusaki, Akinori
    Ogawa, Kento
    Morimura, Takao
    Nakashima, Hiromichi
    MATERIALS TRANSACTIONS, 2015, 56 (01) : 23 - 29
  • [50] Recrystallization behavior and mechanical properties of a Cu-15Ni-8Sn(P) alloy during prior deformation and aging treatment
    Shi, Yufan
    Guo, Chengjun
    Chen, Jinshui
    Xiao, Xiangpeng
    Huang, Hao
    Yang, Bin
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 826