Effects of Zr on microstructural evolution and mechanical property of Cu-15Ni-8Sn alloy

被引:37
|
作者
Zhang, Junjia [1 ]
Liu, Zhaoyu [1 ]
Guo, Zhongkai [3 ]
Liu, Shichao [4 ]
Dong, Yong [5 ]
Fu, Ying [6 ]
Jie, Jinchuan [3 ]
Zhang, Deliang [2 ]
机构
[1] Northeastern Univ, Sch Mat Sci & Engn, Key Lab Lightweight Struct Mat Liaoning Prov, Shenyang 110819, Peoples R China
[2] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110819, Peoples R China
[3] Dalian Univ Technol, Sch Mat Sci & Engn, Dalian 116024, Peoples R China
[4] Soochow Univ, Sch Iron & Steel, Suzhou 215021, Jiangsu, Peoples R China
[5] Guangdong Univ Technol, Sch Mat & Energy, Guangzhou 510006, Peoples R China
[6] Bohai Univ, Sch Engn, Jinzhou 121007, Peoples R China
基金
中国博士后科学基金; 中国国家自然科学基金;
关键词
Cu-15Ni-8Sn alloy; Microstructural evolution; Discontinuous precipitation; Mechanical property; CELLULAR PRECIPITATION; SPINODAL DECOMPOSITION; CU-CR; BEHAVIOR; ELEMENTS;
D O I
10.1016/j.msea.2021.142287
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The Cu-15Ni-8Sn-XZr (wt.%, X=0-0.7) alloys were prepared by vacuum melting, and their microstructural evolutions during the solidification and heat-treatment processes were systematically investigated as well as the corresponding mechanical properties. Zr addition could offer a significant effect on the dendritic morphology by controlling the constitutional supercooling in solidification front, and it also made the gamma-phase more likely to form in the needlelike-shape rather than the lamellar-like shape in subsequent cooling process. After solution treatment, the Zr atoms with a low content of 0.1 wt% were completely solidly dissolved in the alpha-matrix. With its content increasing to 0.3 and 0.5 wt%, the existence form was changed into the nano-scale precipitation phase (Ni5Zr) and then to micron-scale segregation phase (Ni4SnZr). The presence of Zr could significantly extend the aging window of alloy and improve its mechanical properties by inhibiting the nucleation and growth of discontinuous precipitation (DP), and there was few DP even after 16 h aging. The optimal combination of properties was obtained for Cu-15Ni-8Sn-0.5Zr alloy aged at 673 K for 4-16 h, including a hardness of 330HB, ultimate tensile strength (UTS) of 980 MPa and electrical conductivity of 9%IACS.
引用
收藏
页数:10
相关论文
共 50 条
  • [1] Effects of Zr on microstructural evolution and mechanical property of Cu-15Ni-8Sn alloy
    Zhang, Junjia
    Liu, Zhaoyu
    Guo, Zhongkai
    Liu, Shichao
    Dong, Yong
    Fu, Ying
    Jie, Jinchuan
    Zhang, Deliang
    Materials Science and Engineering: A, 2022, 831
  • [2] The Strengthening of Cu-15Ni-8Sn Alloy
    WANG Yan-hui
    材料热处理学报, 2004, (05) : 97 - 100
  • [3] Evolution behavior of γ-D03 phase in Cu-15Ni-8Sn alloy and the corresponding effects on alloy property
    Zhang, Junjia
    Guo, Zhongkai
    Jie, Jinchuan
    Cheng, Jun
    Zhang, Deliang
    JOURNAL OF ALLOYS AND COMPOUNDS, 2022, 897
  • [4] The strengthening of Cu-15Ni-8Sn alloy
    Wang, YH
    Wang, MP
    Hong, B
    14TH CONGRESS OF INTERNATIONAL FEDERATION FOR HEAT TREATMENT AND SURFACE ENGINEERING, VOLS 1 and 2, PROCEEDINGS, 2004, : 97 - 100
  • [5] Microstructural effects on tension behavior of Cu-15Ni-8Sn sheet
    Caris, Joshua
    Li, Dingqiang
    Stephens, John J., Jr.
    Lewandowski, John J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2010, 527 (03): : 769 - 781
  • [6] Wear of Cu-15Ni-8Sn spinodal alloy
    Zhang, Shao-Zong
    Jiang, Bo-Hong
    Ding, Wen-Jiang
    WEAR, 2008, 264 (3-4) : 199 - 203
  • [7] AGE HARDENING IN CU-15NI-8SN ALLOY
    LEFEVRE, BG
    DANNESSA, AT
    KALISH, D
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1978, 9 (04): : 577 - 586
  • [8] Microstructural effects on tension and fatigue behavior of Cu-15Ni-8Sn sheet
    Caris, Joshua
    Varadarajan, Ravikumar
    Stephens, John J., Jr.
    Lewandowski, John J.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 491 (1-2): : 137 - 146
  • [9] Aging behavior of Cu-15Ni-8Sn alloy prepared by mechanical alloying
    Department of Materials Science and Engineering, Zhejiang University, Hangzhou 310027, China
    Trans Nonferrous Met Soc China, 4 (707-711):
  • [10] Ageing behavior of Cu-15Ni-8Sn alloy prepared by mechanical alloying
    郑史烈
    吴进明
    曾跃武
    李志章
    Transactions of Nonferrous Metals Society of China, 1999, (04) : 707 - 711