In-situ SEM investigation on the fatigue behavior of Ti-6Al-4V ELI fabricated by the powder-blown underwater directed energy deposition technique

被引:17
|
作者
Wang, Zhandong
Wang, Shibin
Yang, Kun
Chen, Mingzhi
Bi, Kedong
Ni, Zhonghua
Sun, Guifang [1 ]
机构
[1] Southeast Univ, Sch Mech Engn, Nanjing 211189, Jiangsu, Peoples R China
关键词
Underwater directed energy deposition; Titanium alloys; In-situ SEM; Microstructure; Fatigue crack growth; CRACK-GROWTH-BEHAVIOR; TITANIUM-ALLOY; MECHANICAL-PROPERTIES; PROPAGATION BEHAVIOR; MELTED TI-6AL-4V; MICROSTRUCTURE; STRESS; SLIP; INITIATION; TEXTURE;
D O I
10.1016/j.msea.2022.142783
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Underwater directed energy deposition (UDED) is a promising technology for on-site maintenance and repair of Ti-6Al-4V alloy. The microstructurally short fatigue crack initiation and growth behaviors of Ti-6Al-4V repaired by UDED were investigated through in-situ SEM fatigue testing. The results were compared with those of the Ti-6Al-4V repaired by in-air directed energy deposition (DED) and a substrate. The experimental results show that the microstructure of the Ti-6Al-4V repaired by UDED was dominated by alpha' martensite. The alpha' martensite in the Ti-6Al-4V repaired by in-air DED decomposed into alpha+beta due to the intrinsic heat treatment. Both the strength and microhardness of the Ti-6Al-4V repaired by UDED were higher than those of the Ti-6Al-4V repaired by in air DED. Compared with the Ti-6Al-4V repaired by in-air DED, the Ti-6Al-4V repaired by UDED presented a short micro crack initiation time and a poor fatigue crack propagation resistance. The short fatigue crack initiation and propagation behaviors of the as-deposited Ti-6Al-4V were primarily controlled by the structures and morphologies of the microstructures rather than the residual stresses. In addition, the prior-beta boundaries in the Ti-6Al-4V repaired by UDED had a resistance effect on the fatigue crack growth rate. However, the resistant effect of prior-beta boundaries in the Ti-6Al-4V repaired by in-air DED was not obvious and the local colony alpha+beta played a dominant role in the resistance of short fatigue crack propagation.
引用
收藏
页数:15
相关论文
共 50 条
  • [21] In-situ grain structure control in directed energy deposition of Ti6Al4V
    Zhang, Guohao
    Lu, Xufei
    Li, Jiaqiang
    Chen, Jing
    Lin, Xin
    Wang, Meng
    Tan, Hua
    Huang, Weidong
    ADDITIVE MANUFACTURING, 2022, 55
  • [22] Fatigue Performance of Ti-6Al-4V Processed by Wire-Arc Directed Energy Deposition
    Neves, Jose L.
    Papenberg, Nikolaus
    Kiener, Daniel
    Klein, Thomas
    JOM, 2024,
  • [23] An investigation of the effect of fatigue deformation on the residual mechanical properties of Ti-6Al-4V ELI
    Akahori, T
    Niinomi, M
    Fukunaga, KI
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2000, 31 (08): : 1937 - 1948
  • [24] An investigation of the effect of fatigue deformation on the residual mechanical properties of Ti-6Al-4V ELI
    Toshikazu Akahori
    Mitsuo Niinomi
    Kei-Ichi Fukunaga
    Metallurgical and Materials Transactions A, 2000, 31 : 1937 - 1948
  • [25] In-situ SEM study of the effect of Β grain boundary on the fracture behavior of laser direct melting deposition Ti-6Al-4V alloy
    You, Xiao-Xiao
    Chang, Ling
    Lyu, Jun-Xia
    Surface Technology, 2019, 48 (05): : 97 - 101
  • [26] Role of changes in heat input on additively manufactured Ti-6Al-4V fabricated by directed energy deposition
    Nayir, S.
    Keist, J. S.
    Palmer, T. A.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 822
  • [27] Fatigue crack initiation and fatigue life prediction of Ti-6Al-4V ELI
    Niinomi, M
    Akahori, T
    Fukunaga, K
    Eylon, D
    FATIGUE BEHAVIOR OF TITANIUM ALLOYS, 1999, : 307 - 314
  • [28] Influence of deposition strategy on the microstructure and fatigue properties of laser metal deposited Ti-6Al-4V powder on Ti-6Al-4V substrate
    Choi, Yi Rye
    Sun, Shi D.
    Liu, Qianchu
    Brandt, Milan
    Qian, Ma
    INTERNATIONAL JOURNAL OF FATIGUE, 2020, 130
  • [29] The fretting fatigue behavior of Ti-6Al-4V
    Neu, R.W.
    Key Engineering Materials, 2008, 378-379 : 147 - 162
  • [30] Fatigue behavior of ultrafine-grained Ti-6Al-4V 'ELI' alloy for medical applications
    Saitova, L. R.
    Hoeppela, H. W.
    Goeken, M.
    Semenova, I. P.
    Raab, G. I.
    Valiev, R. Z.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2009, 503 (1-2): : 145 - 147